Protecting Melted Zinc-Aluminium based Foundry Alloys Against Hydrogen Pick-Up

Treść / Zawartość
Identyfikatory
Warianty tytułu
PL
Ochrona przetapianych odlewniczych stopów cynk-aluminium przed pochłanianiem wodoru
Języki publikacji
EN
Abstrakty
EN
The paper is devoted to examinations of the refining efficiency of fluxes and refiners applied during melting of zinc and zinc-aluminium alloys. The content of gases, mainly hydrogen, in the alloys not protected during the charge melting and in the ones protected with the fluxes and/or refined is discussed. The performed examinations show that using the protecting fluxes and melt-refining before pouring leads to significant improvement of ductility in Zn and binary Zn-Al alloys as well as significant increase of the material clearness confirmed by increased density. Furthermore, the metallurgical yields are also increased.
PL
Praca poświęcona jest badaniom rafinacyjnej skuteczności żużli ochronnych i rafinatorów stosowanych w technologii przetapiania cynku oraz stopów cynk-aluminium. Wykonane badania wykazały, iż Zn i stopy podwójne Zn-Al przetapiane pod żużlami ochronnymi oraz przerafinowane przed odlaniem do formy wykazują zwiększoną plastyczność i zwiększoną czystość, potwierdzoną podwyższoną gęstością masy. Dodatkowo, wzrastają uzyski metalurgiczne.
Twórcy
  • AGH University of Science and Technology, Faculty of Foundry Engineering, 23 Reymonta Str., 30-059 Kraków, Poland
  • AGH University of Science and Technology, Faculty of Foundry Engineering, 23 Reymonta Str., 30-059 Kraków, Poland
  • AGH University of Science and Technology, Faculty of Foundry Engineering, 23 Reymonta Str., 30-059 Kraków, Poland
Bibliografia
  • [1] W. Krajewski, The Effect of Ti Addition on Properties of Selected Zn-Al Alloys, Physica Status Solidi A - Applied Research 147, 389-399 (1995).
  • [2] W. Krajewski, Phases of Heterogeneous Nucleation in the Zn Al25 Alloy Modified by Zn-Ti and Al-Ti Master Alloys, Zeitschrift fur Metallkunde 87, 645-651 (1996).
  • [3] W. K. Krajewski, Determination of Al Site Preference in L12 Ti Zn3 - base Trialuminides, Materials Science Forum 508, 615-620 (2006).
  • [4] W. K. Krajewski, A. L. Greer, EBSD Study of Zn Al25 Alloy Inoculated with Zn Ti4 Master Alloy, Materials Science Forum 508, 281-286 (2006).
  • [5] K. Haberl, W. K. Krajewski, P. Schumacher, Microstructural Features of the Grain-refined Sand Cast Al Zn20 Alloy, Archives of Metallurgy and Materials 55, 837-841 (2010).
  • [6] T. Wróbel, J. Szajnar, Modification of Pure Al and Al Si2 Alloy Primary Structure with use of Electromagnetic Stirring Method, Archives of Metallurgy and Materials 58, 955-958 (2013).
  • [7] J. Campbell, Castings, Butterworth-Heinemann, 1997.
  • [8] W. K. Krajewski, Efficacy of New Agents for Melt-refining and Grain-refining of Zn and Zn Al-base Alloys, Metallurgy and Foundry Engineering 21, 233-237 (1995).
  • [9] W. K. Krajewski, The Alloys of Zinc with Aluminium. Types, properties, usage, AKAPIT, Krakow 2013, (in Polish).
  • [10] W. A. Keczin, E. J. Lublinskij, Zinc Alloys, Mietallurgija, Moskwa 1986 (in Russian).
  • [11] S. Rzadkosz, C. Adamski, Synthetic Fluxes for Zinc Alloys, Foundry Review - Przegląd Odlewnictwa, 12, 341-343 (1996) (in Polish).
  • [12] J. Campbell, R. A. Harding, IRCin Materials, EAA - European Aluminium Association, 1994.
  • [13] K. M. Mac Kay, Hydrogen Compounds of Metallic Elements, John Wiley & Sons, Incorporated, 1973.
  • [14] S. Rzadkosz, W. Krok, Technological and Ecological Problems of Melting and Refining Zinc Alloys, Proceedings of the II International Conference Modern Foundry Technologies - Environmental Protection, Krakow, 55-59, (1997) (in Polish).
  • [15] R. J. Barnhurst, Zinc and Zinc Alloys, ASM Handbook, Volume 2, Properties and Selection, Nonferrous Alloys and Special-Purpose Materials, ASM International, 527-542 (1990).
Typ dokumentu
Bibliografia
Identyfikator YADDA
bwmeta1.element.baztech-b9d93a2f-a0d9-4f01-9824-32415c893ab9
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.