TG-DTG-DSC, FTIR, DRIFT, and Py-GC-MS studies have been conducted to determine the effect of the thermal decomposition conditions and structure of foundry binder BioCo3 in the form of a composition poly(sodium acrylate)/dextrin (PAANa/D) on the progress of degradation in terms of processes occurring in foundry sands in contact with liquid metal. TG-DTG-DSC curves of the composition allowed us to determine the temperature range in which they do not undergo degradation, by which they do not lose their binding properties. With temperature increasing, physical and chemical changes occur that are related to the evaporation of solvent water (20–110°C), followed by the release of constitution water, and finally intermolecular dehydration (110–230°C). In this temperature range, processes that are mainly reversible take place. Within a temperature range of 450–826°C, polymer chains are decomposed, including the decomposition of side chains. Within a temperature range of 399–663°C, polymer composition decomposition can be observed (FTIR, DRIFT), and gas products are generated from this destruction (Py-GC-MS).
W artykule przedstawiono badania nad przebiegiem procesu biodegradacji nowych spoiw polimerowych w środowisku wodnym i w glebie. Przeprowadzone badania biodegradacji w środowisku wodnym wykazały, że nowe spoiwa polimerowe są w pełni biodegradowalne w środowisku wodnym. Podczas procesu biodegradacji próbki usieciowanych spoiw polimerowych w glebie ogrodowej trwającego 6 miesięcy przeprowadzono analizy zmian powierzchniowych i strukturalnych wynikających z rozkładu próbki.
EN
The investigations on the biodegradation process pathway of the new polymer binders in water environment and in a soil are presented in the hereby paper. These investigations indicated that the new polymer binders constitutes the fully biodegradable material in water environment. During the 6 months biodegradation process of the crosslinked sample of the polymer binders in a garden soil several analysis of surface and structural changes, resulting from the sample decomposition, were performed.
W artykule przedstawiono analizę lotnych produktów rozkładu nowych odlewniczych spoiw polimerowych BioCo przy zastosowaniu metody termograwimetrycznej (TG) sprzężonej on-line ze spektrometrią masową (MS). W zakresie temperatury 40-600°C stwierdzono sygnały dla małych mas cząsteczkowych, co świadczy o zachodzeniu procesu degradacji, fragmentaryzacji łańcuchów polimerowych i tworzeniu się małocząsteczkowych związków, w tym przede wszystkim H2O i CO2. Podczas degradacji prawdopodobnie powstają również rodniki alkilowe, na co wskazują sygnały MS. Przedstawiono wyniki badań emisji BTEX mas wiązanych spoiwami BioCo podczas procesu zalewania ciekłym żeliwem.
EN
In this paper presented the analysis of the volatile decomposition products was carried out by means of the thermogravimetric (TG) method coupled ”on-line” with the mass spectrometry (MS) method. At the temperature range 40–600°C the signals for small molecular masses were found, which indicates that the degradation process and the fragmentation of polymer chains occurred as well as the small particles were formed including, first of all, H2O and CO2. Probably during the degradation radicals are also formed, which is indicated by the MS signals. The basic the results of research of BTEX emission from tested moulded sands with binders BioCo on during liquid iron pouring were presented.
Podstawowe znaczenie dla charakterystyki polimeru ma określenie takich jego parametrów, jak: temperatura destrukcji, zeszklenia, topnienia, określonych ubytków masy czy przemian polimorfi cznych, które to decydują często o jakości produktu i jego zastosowaniu. Badaniom analizy termicznej (TG-DSC) poddano próbkę spoiwa polimerowego. Badania te miały na celu określenie zmian, jakie mogą zachodzić w masie odlewniczej w warunkach kontaktu z ciekłym metalem.
EN
To characterise a polymer, it is of fundamental importance to determine its parameters, like the temperatures of destruction, vitrification, melting point, specific mass losses or polymorphic transformations, which frequently determine the quality of the product and its applications. Thermal analyses (TG-DSC) of the sample of a polymer binder were conducted. These examinations were also aimed at identifying the changes that can take place in the casting paste when it comes into contact with liquid metal.
In this study, the results of biodegradability of a new polymeric binder consisting of modified starch – Polvitex Z (by Xenon) in a water solution are presented. Biodegradation tests were conducted in accordance with the Zahn–Wellens method, which is intended to denote the susceptibility to biodegradation by microorganisms (in high concentrations during the static test) of the non-volatile, watersoluble organic compounds. Observations of the decomposition process were carried out through regular, daily or at certain time intervals by measurement the Chemical Oxygen Demand (COD) and level of biodegradability (RT) in the prepared samples during the test. The study showed that the starch binder is fully biodegradable material in an aqueous medium.
PL
W niniejszej pracy zostały omówione wyniki badań stopnia biodegradacji roztworu wodnego modyfikatu skrobiowego Polvitex Z firmy Xenon – materiału polimerowego użytego jako spoiwo do mas formierskich. Testy biodegradacji przeprowadzono zgodnie z metodą Zahna–Wellensa, która ma na celu oznaczenie podatności nielotnych, rozpuszczalnych w wodzie związków organicznych na biodegradacje przez mikroorganizmy występujące w dużym stężeniu podczas badania statycznego. Obserwacje procesu rozkładu prowadzono przez regularne, codzienne lub w określonych przedziałach czasowych pomiary chemicznego zapotrzebowania na tlen (ChZT) i stopnia biodegradacji (R T), mierzonych w przygotowanych próbkach w trakcie trwania testu. Przeprowadzone badania wykazały, że spoiwo skrobiowe jest materiałem w pełni biodegradowalnym w środowisku wodnym.