Results of investigation of silicon additions and processing parameters on mechanical properties and microstructure of the iron-base sintered materials are presented. Green density as well as as-sintered density, hardness, tensile strength, transverse rupture strength and impact toughness were measured. As-sintered microstructures were also examined. The results indicate marked effect of silicon additions, cold compacting pressure and sintering temperature on evaluated properties.