Ten serwis zostanie wyłączony 2025-02-11.
Nowa wersja platformy, zawierająca wyłącznie zasoby pełnotekstowe, jest już dostępna.
Przejdź na https://bibliotekanauki.pl
Preferencje help
Widoczny [Schowaj] Abstrakt
Liczba wyników

Znaleziono wyników: 4

Liczba wyników na stronie
first rewind previous Strona / 1 next fast forward last
Wyniki wyszukiwania
help Sortuj według:

help Ogranicz wyniki do:
first rewind previous Strona / 1 next fast forward last
1
Content available remote A new accelerated test for the evaluation of the protective properties of coatings
100%
EN
Weathering of coatings by natural conditions at climatically different locations provides reliable data on the protective properties of coatings, it is however very time and cost consuming and non-practical for a quick evaluation of coatings. A number of diverse short time tests are therefore in usage by the development and optimization of new protective coatings. The most important requirements on such tests are the appropriate loading conditions, a sensitive quantitative detection of the coating deterioration, a short test duration as well as a good correlation with a natural weathering and a long term performance of coatings. By the development of a new short time test, we tried to fulfil these requirements as good as possible. For the accelerated aging of coatings we used the concept of the forced internal stress, induced by a thermal cycling, combined with an electrolytic, chemical or UV loading. By this kind of aging/loading both the natural weathering conditions and the standard laboratory tests can be simulated and performed at a shorter time. For the detection of the protection loss the impedance spectroscopy and the scanning Kelvin probe were chosen. Specific parameters from this kind of detection provide quantitative criteria for the quantitative evaluation of the protective properties of coatings in the early stages of their testing.
PL
Badania odporności powłok na czynniki atmosferyczne na stacjach terenowych w różnych warunkach klimatycznych dostarczają wiarygodnych danych na temat ochronnych właściwości powłok, jest to jednak metoda czasochłonna i kosztowna, w związku z tym niepraktyczna do szybkiej oceny powłok. W przypadku optymalizacji i opracowywania nowych wyrobów lakierowych używa się więc wielu różnorodnych metod badań przyspieszonych. Najważniejsze w takich metodach badań jest zapewnienie odpowiednich warunków narażenia, czuła ilościowa metoda wykrywania zmian, krótki czas trwania, jak również dobra korelacja z metodami badań w warunkach naturalnych i z zachowaniem się powłok w długim okresie czasu. Opracowując nowy krótkotrwały test, próbowaliśmy jak najlepiej spełnić te wymagania. W celu przyspieszenia starzenia powłok stosowaliśmy wymuszone naprężenia wewnętrzne, powodowane przez cykliczne zmiany temperatury w połączeniu z działaniem elektrolitu oraz narażeniami chemicznymi i UV. Rodzaj starzenia/narażenia pozwala zarówno na modelownie badań powłok w warunkach atmosferycznych, jak i standardowych badań laboratoryjnych oraz na skrócenie czasu badań. Do wykrywania zmian w powłokach, prowadzących do zmniejszenia ich właściwości ochronnych, wybrano metodę elektrochemicznej spektroskopii impedancyjnej (EIS) i metodę skanowania sondą Kelvina. Otrzymane tymi metodami charakterystyczne parametry umożliwiają ilościową ocenę ochronnych właściwości powłok we wczesnym etapie ich badania.
2
Content available remote Laser marking of coatings
80%
EN
Laser marking of coatings on plastics can be realized nowadays by the ablation of laser sensitive coatings, when additional supporting coatings are applied beneath them. By a modification of laser sensitive coatings with special additives, it was possible to perform the laser marking without a supporting coating and thus to simplify the laser marking process. An interesting alternative to the ablative laser marking of coatings represents the non-ablative process. However, it can not be realized by a conventional carbonization or foaming of coatings without their complete or at least partial damage. By a modification of laser sensitive coatings with thermochromic additives and the usage of optimal laser parameters, the non-ablative laser marking was achieved, without any signifi cant damage of the coating.
PL
Znakowanie laserowe może być aktualnie realizowane na drodze ablacji, czyli lokalnego usuwania powłoki reagującej na promienie laserowe, pod warunkiem stosowania pod powłoką właściwą dodatkowej powłoki wspomagającej. Na drodze modyfikacji powłoki właściwej substancjami pomocniczymi okazało się możliwe znakowanie laserowe bez powłoki pomocniczej, prowadzące do racjonalizacji całego procesu. Interesującą alternatywę dla znakowania ablacyjnego przedstawia znakowanie bezablacyjne, które nie może być jednak realizowane na drodze konwencjonalnej karbonizacji lub pienienia powłok, prowadzących do ich niszczenia. Modifikacja powłok za pomocą substancji termochromowych z jednoczesną optymalizacją parametrów lasera umożliwiła znakowanie bezablacyjne bez uszkadzania powłok.
3
Content available remote Corrosion protection with nanoscale anticorrosive pigments in coatings
80%
EN
For the efficient corrosion protection of metals and alloys with primers as well as self-healing effects, properties of anticorrosive pigments such as particle size, interaction with binder, barrier effect, release of active species and their transport to the metal surface are of great importance. Conventional and nanoscale corrosion protective phosphate derivates have been investigated to clarify their influence on all these factors and ultimately on the efficiency of the corrosion protection of metallic substrates. The chosen pigments were incorporated into a solvent based epoxy primer and tested on steel, galvanized steel and aluminium substrates with short time tests, electrochemical methods and atmospheric weathering. SEM images of paint cross sections were also taken to visualize the pigment particle distributions. Such advantages of nanoscale pigments as an efficient corrosion protection, good self-healing and barrier properties have been noticed. An influence of the metal surface roughness on these properties was also observed.
PL
W celu zapewnienia skutecznej ochrony antykorozyjnej metali i ich stopów za pomocą farb do gruntowania oraz w celu osiągnięcia właściwości samonaprawczych niezwykle ważne są takie właściwości pigmentów antykorozyjnych jak: wielkość cząsteczek, ich wzajemne oddziaływanie ze spoiwem, efekt barierowy, uwolnienie aktywnych związków oraz ich transport na powierzchnię metalu. Badaniu poddano tradycyjne antykorozyjne pigmenty fosforanowe oraz ich odmiany w nanoskali w celu ustalenia ich wpływu na powyższe czynniki i na skuteczność ochrony podłoża metalowego przed korozją. Wybrane pigmenty wprowadzono do rozpuszczalnikowego gruntu epoksydowego, który nałożono na podłoża stalowe, stalowe ocynkowane i aluminiowe, a następnie badano za pomocą testów krótkoterminowych, metod elektrochemicznych oraz poddając próbki działaniu warunków atmosferycznych. Wykonano również zdjęcia SEM przekrojów, aby zobrazować rozmieszczenie cząstek pigmentu. Do korzystnych właściwości nanopigmentów należy zaliczyć skuteczną ochronę przed korozją, dobre właściwości samonaprawcze oraz właściwości barierowe. Zaobserwowano również wpływ chropowatości powierzchni metalu na powyższe właściwości.
EN
In the past photoactive pigments have been surface passivated to reduce the photoactivity and thereby to avoid chalking. In new applications highly photoactive types of these pigments are used on glass or ceramic substrates for self cleaning and pollution reduction purposes. This initiated attempts to develop photoactivity test devices. In this contribution a test chamber method is presented which is based on a previous setup. The samples are placed in a chamber where various climatic and atmospheric conditions can be applied and controlled including exposure to model pollutants. During irradiation by UV light a FTIR spectrometer records the amount of pollutants and their decomposition products. This technique does not only allow to follow the photoactivity of the pigment and pigmented coating regarding the decomposition of model pollutants, but also to determine the photocatalytic stability of coatings by detecting products of the decomposition of the polymeric binder.
PL
Pigmenty fotoaktywne były dawniej pasywowane powierzchniowo w celu zmniejszenia ich aktywności fotokatalitycznej i tym samym uniknięcia kredowania. W nowych zastosowaniach pigmenty o dużej aktywności fotokatalitycznej wykorzystuje się na podłoża szklane i ceramiczne, w celu uzyskania właściwości samoczyszczących i odporności na zabrudzenia. Takie wykorzystanie pigmentów zainicjowało próby opracowania urządzeń do badania fotoaktywności. Przedstawiono komorową metodę badawczą, opartą na wcześniej opracowanym urządzeniu. Próbki umieszcza się w komorze, w której można modelować i kontrolować różne warunki atmosferyczne, obejmujące narażenia na modelowe zanieczyszczenia. Za pomocą spektrometru FTIR rejestruje się, podczas naświetlania próbek promieniami UV, ilość zanieczyszczeń i produktów ich rozkładu. Metoda ta pozwala nie tylko na śledzenie fotokatalitycznej aktywności pigmentu i pigmentowanych powłok na podstawie rozkładu modelowych zanieczyszczeń, ale również na oznaczenie fotokatalitycznej stabilności powłok, poprzez wykrywanie produktów rozkładu polimeru spoiwa.
first rewind previous Strona / 1 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.