The paper presents the results of the pitting resistance investigations of selected stainless steels in the chloride environment and the simultaneous impact of erosive factors using the cyclic polarization technique. Additionally, using electrochemical techniques, ie: electrochemical impedance spectroscopy (EIS) and measurement of corrosion potential, the behavior of the passive layer of selected stainless steels in the environment of chlorides and erosion was examined. On the basis of the obtained results, the resist-ance of stainless steels 1.4301 and 1.4404 was found, both on the effect of chloride ions and erosive factors in the studied systems. Both tested steels are susceptible to pitting corrosion. It was found that a good measure of erosive impact on stainless steel is both impedance spectrum analysis and continuous monitoring of the corrosion potential of steel.
The paper presents the results of the pitting resistance investigations of selected stainless steels in the chloride environment and the simultaneous impact of erosive factors using the cyclic polarization technique. Additionally, using electrochemical techniques, ie: electrochemical impedance spectroscopy (EIS) and measurement of corrosion potential, the behavior of the passive layer of selected stainless steels in the environment of chlorides and erosion was examined. On the basis of the obtained results, the resistance of stainless steels 1.4301 and 1.4404 was found, both on the effect of chloride ions and erosive factors in the studied systems. Both tested steels are susceptible to pitting corrosion. It was found that a good measure of erosive impact on stainless steel is both impedance spectrum analysis and continuous monitoring of the corrosion potential of steel.
Przedstawiono wyniki badań elektrochemicznych wykonanych metodą polaryzacji cyklicznej oraz emisji akustycznej technicznie czystego aluminium (stop 1050) oraz magnezu. W przypadku aluminium aktywność akustyczna jest związana z inicjacją i wzrostem wżerów. Aktywność akustyczna magnezu występuje w obszarze inicjacji i wzrostu wżerów oraz w czasie repasywacji wżerów.
EN
Results of electrochemical investigations by means cyclic polarization and acoustic emission of 1050 aluminum alloy and technical pure magnesium have been presented. Acoustic emission activity of aluminum alloys is connected to initiation and growth of pits. Acoustic emission of magnesium occur in initiation and pits growth area and during pits repasivation.
Przedyskutowano role jaką spełniają elektryczne schematy zastępcze wykorzystywane w analizie częstotliwościowej wyników impedancyjnych. W przypadku prostych procesów elektrochemicznych sens fizyczny elementów składowych zastępczych schematów elektrycznych jest prosty i nie wymaga dodatkowych wyjaśnień. Elektryczny schemat zastępczy wykorzystywany jest wówczas w sposób bezpośredni. Inna funkcję spełnia elektryczny schemat zastępczy gdy nie można określić w sposób jednoznaczny sensu fizycznego poszczególnych elementów elektrycznych złożonego procesu. W tym przypadku elektryczny schemat zastępczy pełni funkcję pośrednią i jest jedynie narzędziem w kompleksowej analizie badanego procesu.
EN
The indirect method of application electrical equivalent circuits is described. Correlation of electrical equivalent circuit and experimental impedance data allows schematically notice of impedance spectrum. Mathematical description of investigated electrochemical process allows give the physicochemical sense of an electrical elements of equivalent circuit.
W pracy przedstawiono wyniki badań impedancyjnych powłok barierowych w chlorku metylenu. Odpowiedni do badań poziom przewodnictwa chlorku metylenu uzyskano przez dodatek soli organicznej. Z uwagi na dużą agresywność roztworu pomiary wykonywano w systemie automatycznych pomiarów wielokrotnych. Uzyskano zróżnicowanie odporności badanych powłok barierowych. Stwierdzono, że hybrydowe powłoki siloksiranowe wykazują bardzo dobrą odporność w chlorku metylenu.
EN
The results of impedance measurements of barrier coatings in methylene chloride are presented. The required level of conductivity of methylene chloride was achieved by addition of organic salt. Tests were carried out in multiple measurements system because of the high aggressiveness of the methylene chloride. It has been stated that hybrid siloksirane coatings show excellent resistance to methylene chloride.
Staphylococcal food poisoning results from ingestion of food contaminated with toxins produced by enterotoxigenic Staphylococcus aureus strains. Common symptoms of this intoxication include vomiting, diarrhea, and abdominal cramps. Staphylococcal enterotoxins are resistant to heat and a number of environmental factors. Certain cheeses, milk powder, and whey powder are the only foodstuffs that are being routinely examined for the presence of staphylococcal enterotoxins SEA-SEE. The newly identified enterotoxins are not included in the current examination scheme. Enterotoxin-producing staphylococci were already isolated from meat, meat products, milk, dairy products, fermented food products, vegetables, pastries and fish products. It has been demonstrated that many environmental factors associated with food processing and storage can significantly influence the level of secreted enterotoxins by S. aureus strains. Nevertheless, only a few studies on the production of staphylococcal enterotoxins were conducted in foodstuffs. Most data on their expression is based on experiments performed with a low number of S. aureus strains, and usually only SEA-SEE enterotoxins are investigated. These results inclined many authors to the conclusion that milk and dairy products are unfavorable environments for expression of staphylococcal enterotoxins. However, recent research has indicated a significant heterogeneity in the ability of enterotoxin production in milk among S. aureus strains derived from diverse sources. S. aureus strains able to secrete high levels of enterotoxins in milk and meat juice were described. This research indicates that a high number of S. aureus strains should be used for studying staphylococcal enterotoxins expression in food. It seems to be the appropriate way to assess the risk of staphylococcal food poisoning.
10
Dostęp do pełnego tekstu na zewnętrznej witrynie WWW
Przedstawiono wyniki badań elektrochemicznych stali stopowej 1.4301 w środowisku korozyjnym zawierającym jony Cl-. Powierzchnia stali została poddana przed badaniami różnym typom obróbki powierzchniowej. Porównano odporność na korozję wżerową stali poddanej trawieniu, trawieniu i pasywacji oraz samej pasywacji. Stwierdzono poprawę odporności stali poddanej dodatkowej obróbce powierzchniowej w stosunku do stali przygotowanej jedynie w sposób mechaniczny.
EN
Results of electrochemical measurements of 1.4301 stainless steel in chloride ion containing environment have been presented. Surface of investigated stainless steel was chemically treated before investigations in several ways. Resistance to pitting corrosion of as received, passivated and etched steel has been compared. Increase in resistance to pitting corrosion has been found for chemical treatment steels compared to mechanically polished only.
11
Dostęp do pełnego tekstu na zewnętrznej witrynie WWW
Przeprowadzono badania trawienia stali wysokostopowej w mieszaninie kwasu HF i HNO3, wykorzystując elektrochemiczną spektroskopie impedancyjną. W celu odwzorowania warunków naturalnych, eksperyment przeprowadzono przy użyciu deis w trybie galwanostatycznym z wypadkowym prądem równym zero. Wyznaczone zostały zmiany parametrów elektrycznych opisujących układ w czasie. Zaobserwowano wpływ stężenia HF na czas trwania procesu.
EN
Pickling of stainless steel in mixed acid of HF-HNO3 was investigated based on impedance measurements. Experiment was carried out in the galvanostatic mode to reflect real conditions by means of DEIS technique. Changes of particular equivalent circuit parameters have been determined as a function of time. As a result significant effect of the HF concentration on duration time of the investigated process has been observed.
12
Dostęp do pełnego tekstu na zewnętrznej witrynie WWW
Przedstawiono wyniki z badań terenowych i laboratoryjnych wykładzin organicznych stosowanych do ochrony wewnętrznych powierzchni w absorberach instalacji odsiarczania spalin w obszarach gdzie kondensują się spaliny oczyszczone. Badania laboratoryjne powłok winyloestrowych przeprowadzono na dwóch wyrobach różniących się wypełnieniem. Pierwsza badana powłoka posiadała wypełnienie płatkowe natomiast druga sferyczne. Stwierdzono różnice w odporności korozyjnej obydwu powłok.
EN
Results of fi eld and laboratory investigations of organic linings have been presented. The linings are used to corrosion protection of inner part of fl ue gas desulphurization units in clean gas moisture area condensation. Two vinylester coatings have been investigated. The coatings had different fi ller, one of them was in the form of fl akes while the other one was in the spherical shape. Differences in corrosion resistance of investigated coatings have been found.
13
Dostęp do pełnego tekstu na zewnętrznej witrynie WWW
Przedstawiono wyniki badań korozji w zanurzeniu stopów metali i korozji powłoki kadmowej na stali w nowym płynie do odladzania samolotów (typ I) i nowym płynie zapobiegającym ich ponownemu oblodzeniu (typ II). Opracowane kompozycje oparto na ekologicznej, trójskładnikowej mieszaninie glikolu 1,2-propylenowego (MPG) i 1,3-propylenowego (PDO) oraz glicerolu, uzyskując wartości ChZT o 10% niższe od preparatów handlowych. Ponadto przeprowadzone testy potwierdziły wysoką skuteczność pakietu inhibitującego procesy korozyjne, na jakie narażone są elementy konstrukcyjne samolotów podczas procesu odladzania i zapobiegania oblodzeniu, dzięki czemu preparaty gwarantują bezpieczeństwo stosowania zgodnie z przeznaczeniem.
EN
Two novel fluids for deicing and antiicing aircrafts based on 1,2-propylene glycol, biomass-derived 1,3-propylene glycol and glycerol were developed. The deicing fluid contained 18.45, 10.25 and 53.30% of the components, resp., and the antiicing one 22.40, 7.00 and 26.60%, resp. The crystn. temps. of the fluids were -21.4 and -36.0°C, resp., and the COD values 1.152 and 0.794 kg/kg, resp.
14
Dostęp do pełnego tekstu na zewnętrznej witrynie WWW
Przedstawiono wyniki badań korozji kadmowej powłoki na stali oraz korozji po zanurzeniu stopów metali w mrówczanie sodu z nowym pakietem inhibitorów korozji, zawierającym synergiczną kompozycję poliasparaginianu sodu oraz imidazolu. Ponadto wyznaczono zdolność penetracji lodu przez badany układ. Właściwości opracowanej kompozycji odladzającej porównano z właściwościami środków dostępnych na rynku. Uzyskane wyniki wskazują, że otrzymany stały preparat może być stosowany jako nowy ekologiczny środek do odladzania infrastruktury lotniczej.
EN
Na formate was added to a Na polyaspartate and imidasole-contg. corrosion inhibitor package and used for studying the corrosivity of Cd-coated steel and Al, Mg and Ti alloy machine parts for 24 h at 35°C. The parts were weighed, cleaned, degreased and dipped in a 5% aq. soln. of the agent. After the study, the parts were washed again with water, dried and weighed. The mass loss was a measure of the corrosion resistance of the parts. Addnl., the ability of the agent to penetrate the sample of ice was detd. by measuring the depth of the ice dissolved under its action. For comparison, 4 other com. agents were used. The agent showed the lowest corrosivity and the best penetration ability when compared with the com. ones.