Nowa wersja platformy, zawierająca wyłącznie zasoby pełnotekstowe, jest już dostępna.
Przejdź na https://bibliotekanauki.pl
Preferencje help
Widoczny [Schowaj] Abstrakt
Liczba wyników

Znaleziono wyników: 28

Liczba wyników na stronie
first rewind previous Strona / 2 next fast forward last
Wyniki wyszukiwania
help Sortuj według:

help Ogranicz wyniki do:
first rewind previous Strona / 2 next fast forward last
EN
Partition coefficient n-octanol/water is the most commonly used parameter for describing lipophilicity. The aim of this study was the usefulness of high performance liquid chromatography (HPLC) for determination of log Pow for chlorothalonil based on OECD 117: OECD Guidelines For The Testing of Chemicals – Partition Coefficient (n-octanol/water), High Performance Liquid Chromatography (HPLC) Method (2004). As reference substances: aniline, benzonitrile, nitrobenzene, chlorobenzene, toluene, 1,4-dichlorobenzene, 1,2,4-trichlorobenzene were selected. The dead time was measured by using methanol as an unretained substance. The obtained by HPLC technique value of log Pow for chlorothalonil amounted to 2.93, and was comparable to literature data 2.92. The results revealed the usefulness of presented method in registration studies on chlorothalonil.
PL
Zmiany, jakie dokonują się w strefie połączenia poszczególnych warstw w wyrobach spajanych wybuchowo są kluczowe dla zmian we właściwościach użytkowych platerów. W niniejszej pracy analizowano układ Ni/Ti (alloy 201/Gr.1) wykonany z blach o małej grubości (1 mm/1 mm), łączonych technologią zgrzewania wybuchowego. Badaniom poddano platery w stanie "po połączeniu" oraz po zabiegach obróbki cieplnej, symulujących rzeczywiste warunki pracy. Zmiany mikrostruktury, składu chemicznego oraz własności mechanicznych bimetalu analizowano z wykorzystaniem mikroskopii optycznej oraz elektronowej mikroskopii skaningowej (SEM), jak również poprzez pomiary mikrotwardości. Szczególną uwagę skoncentrowano na zmianach, jakie dokonują się w obszarach położonych w pobliżu strefy połączenia. Analiza zmian składu chemicznego, jakie dokonują się w pobliżu warstwy spojenia, prowadzona była z wykorzystaniem SEM wyposażonego w system EDX. Natomiast zmiany morfologiczne (np. formowanie się strefy drobnokrystalicznej) oraz zmiany w topografii orientacji w nanoobszarach analizowano z wykorzystaniem systemu pomiaru orientacji lokalnych w SEM. W pracy opisano zróżnicowane przypadki występowania obszarów warstwy przetopionej. W platerach w stanie "po połączeniu" zidentyfikowano obszary przetopione, występujące sporadycznie w zawinięciu fal. Badania stereologiczne tych obszarów pozwoliły na wyznaczenie, tzw. równoważnej grubości przetopień (współczynnik RGP). Współczynnik RGP dla tych złącz jest niewielki (max. do 4,73 [mi]m). W złączach po zgrzewaniu i obróbce cieplnej pomiędzy Ni a Ti zidentyfikowano również dodatkową warstwę przejściową, nie występującą w platerach w stanie wyjściowym bez obróbki cieplnej. Pomiary mikro-twardości wykazały znaczne umocnienie w obszarze złącza (do 200-250 HV0,2) oraz skokowo jego wzrost w warstwach przetopionych (do 811 HV0,2). Obróbka cieplna platerów spowodowała spadek umocnienia w tych obszarach. Analiza otrzymanych wyników wykazała, że technologia zgrzewania wybuchowego pozwala na uzyskanie bimetalu z blach o małych grubościach o dobrej jakości połączenia.
EN
The events that occurs close to the interface of explosively welded bimetallic components are of key importance for functional properties of clads. This research study is focused on microstructural changes that occurs close to the interface of explosively welded Ni/Ti (alloy 201/Gr.1) sheets (1 mm/1 mm). The changes in microstructure, chemical composition and mechanical properties were analysed using optical microscopy, scanning electron microscopy (SEM) equipped with EDX and EBSD systems as well as through the microhardness measurements. The studies were focused on a detailed characterization of the intermediate layers close to the interface, i.e. an identification of the intermetallic phases and the possible interdiffusion between the Ni and the Ti. The obtained results showed that explosive welding technology allows manufacturing of a "good" bimetals composed of thin sheets. The wavy and the flat interfaces between the bonded metals were outlined by a characteristic sharp transition; there is no mechanical mixing between the welded materials in the solid state. However, the explosive jet heating gives rise to a significant increase of temperature and to melting some volumes of both sheets at the Ni/Ti interface. A few kinds of intermetallic compounds of the NimTin - type were identified inside the melted volumes and those mostly populated take a form a thin continuous layer. Interest is also directed towards the detailed characterization of the morphology of the intermetallic compounds.
PL
W pracy analizowano zmiany mikrostrukturalne oraz formowanie się nowych faz w wielowarstwowych układach platerów zbudowanych na bazie Ti i Al. Wykorzystano techniki mikroskopii optycznej i skaningowej mikroskopii elektronowej, pomiary mikrotwardości, a także próbę zginania w warunkach udarowych. Obserwacje w skali makro pokazały, że w procesie spajania wytworzono 15-warstwowy plater wolny od nieciągłości strukturalnych. Powierzchnie połączenia uległy silnemu odkształceniu i wykazywały mieszany falisto-płaski charakter ze strefami przetopień preferencyjnie lokowanymi na grzbiecie oraz w zawinięciach fal. Zaobserwowano, że silnie pofalowane granice połączenia zawsze formowały się w warstwach położonych w pobliżu ładunku wybuchowego. Analizy w mikro skali udokumentowały występowanie cienkiej warstwy przetopionej o silnie rozdrobnionej strukturze.
EN
Microstructure and phase in the bonding zone of explosively welded Ti/Al multilayer clads were examined by optical microscopy and scanning electron microscopy. The defect-free multilayer composite was successfully formed. The macro-scale observations showed that the interfaces between joined plates presented mixed wavy/flat shape with solidified melt inclusions located preferentially at the crest of each wave and in the wave vortex. It was found that interfaces of wavy character were always formed in layers near the explosive charge and flattened with the increase of the distance from the top surface. The micro-scale analyses observations revealed a presence of very thin reaction layer at the flat parts of the joint plates and nano-grained structure of melted zones.
EN
The structure near the interface of bimetallic strips strongly influences their properties. In this work, the interfacial layers of explosively welded aluminium and copper plates were investigated by means of a scanning electron microscope (SEM), equipped with a high resolution system for local orientation measurements (SEMFEG/EBSD), and a transmission electron microscope (TEM), equipped with energy dispersive spectrometry (EDX) for the analysis of chemical composition changes. The SEMFEG/EBSD-based local orientation measurements in the areas close to the interface, in both sheets, revealed fine-grained layers characterized by the clearly marked tendency of the copper-type rolling texture formation. The texture was described by an increased density of the orientations near the f112g<111>, f123g<634>and f110g<112>positions. The internal microstructure of the intermetallic inclusion is mostly composed of dendrites. The electron diffractions and the TEM/EDX chemical composition measurements in the intermetallic inclusions revealed only crystalline phases, both equilibrium and 'metastable'. Additionally, no significant regularity in the phase distribution with respect to the parent sheets was observed.
PL
Mikrostruktura w pobliżu strefy połączenia silnie wpływa na własności układów bimetalowych. W niniejszej pracy analizie poddano układy warstwowe Al/Cu wytworzone technologia zgrzewania wybuchowego. Badania prowadzono z wykorzystaniem skaningowej mikroskopii elektronowej wyposażonej w wysokorozdzielczy system pomiaru orientacji lokalnych oraz transmisyjnej mikroskopii elektronowej wyposażonej w analizator składu chemicznego. Systematyczne pomiary orientacji lokalnych w pobliżu strefy połączenia, w obydwu łączonych płytach, ujawniają formowanie się strefy silnie rozdrobnionych ziaren. Strefa ta scharakteryzowana jest przez formowanie się tekstury walcowania typu miedzi z dobrze uwidocznionymi składowymi zbliżonymi do położeń: f112g<111>, f123g<634> oraz f110g<112>. Wewnętrzna struktura 'intermetalicznych inkluzji' zbudowana jest z dendrytów. Badania z wykorzystaniem elektronowej mikroskopii transmisyjnej dokumentują, ze wewnątrz strefy przetopień następuje formowanie się faz krystalicznych, zarówno równowagowych jak i 'metastabilnych'. Skład chemiczny formujących się faz nie wykazywał związku z położeniem ziaren względem płyt bazowych.
EN
The microstructure and the texture evolutions of partly recrystallized samples of pure Al and the Al-1%wt. Mn alloy have been characterized by a high resolution SEM/EBSD. The single crystals of the Goss{110}<001> and brass{110}<112> orientations, stable in the plane strain compression, were deformed in a channel-die up to 60% to develop a homogeneous structure composed of two sets of symmetrical primary microbands and then shortly annealed. It is documented that the orientations of the initial nucleus were scattered but not accidental. The disorientation axes in the orientation relationship across the recrystallization front usually coincide with one of the <112>, <221>, <102> or <111> crystallographic directions and were rather rarely close to the <110> or <001> directions. The disorientation axis of the <111>- type is only one of the few most often observed.
PL
Przemiany tekstury w poczatkowych stadiach rekrystalizacji sa przedmiotem intensywnych badan, zwłaszcza tych które dotycza półwyrobów płaskich stosowanych w przemysle do wytwarzania opakowan droga głebokiego tłoczenia. W niniejszej pracy wykorzystano wysokorozdzielczy system SEM/EBSD do analizy tych zmian w nieswobodnie sciskanych próbkach aluminium oraz stopu Al-1%Mn. Dla przejrzystosci prowadzonej analizy, w badaniach wykorzystano próbki monokrystaliczne, o orientacjach stabilnych w płaskim stanie odkształcenia, tj. Gossf110g<001> i brassf110g<112>. Poddano je nieswobodnemu sciskaniu (powszechnie uznawanemu za modelowe przyblizenie procesu walcowania) do 40% i 60%, a nastepnie analizowano ich zachowanie w poczatkowych stadiach rekrystalizacji. W stanie po deformacji obserwowano jednorodna strukture dwu symetrycznie usytuowanych rodzin mikropasm, która w procesie rekrystalizacji sprzyjała pojawieniu sie nowych ziaren. Udokumentowano, ze orientacje poczatkowych ziaren, wyrastajacych ze struktury stanu zdeformowanego nie sa przypadkowe, i tylko scisle okreslona liczba grup orientacji moze sie pojawic w poczatkowym stadium wyzarzania. Dezorientacja obliczona poprzez migrujacy front rekrystalizacji zwiazana jest najczesciej z rotacja dookoła kierunków krystalograficznych typu <112>, <221>, <102> lub <111>, oraz rzadziej <110> lub <001>. Os dezorientacji typu <111> jest tylko jedna z kilku czesciej spotykanych.
PL
W pracy analizowano zmiany struktury i tekstury zgrzewanych wybuchowo płyt aluminiowych i miedzianych o czystości technicznej ze szczególnym uwzględnieniem zmian, jakie następują w warstwach położonych w pobliżu strefy połączenia. Przeprowadzono badania z wykorzystaniem mikroskopii świetlnej, elektronowej mikroskopii skaningowej i analizatora GENESIS oraz systemu pomiaru orientacji lokalnych metodą dyfrakcji elektronów wstecznie rozproszonych. Dla zastosowanych parametrów technologicznych procesu spajania obserwowano silne zmiany geometryczne na powierzchni łączonych blach. W najczęściej obserwowanych przypadkach uzyskane połączenie można sklasyfikować jako płaskie lub faliste z fazą pośrednią. W wyniku przetopienia w strefie połączenia obserwowano tworzenie się fazy międzymetalicznej typu CuAln, przy wartości n zawartej w zakresie 1÷2,7. Wskazuje to na zmieniającą się koncentrację Cu w Al w zależności od analizowanego obszaru. Inną charakterystyczną cechą procesu spajania było występowanie silnego rozdrobnienia struktury po obu stronach warstwy fazy międzymetalicznej. Pomimo że proces rozdrobnienia obserwowany jest zarówno w miedzi, jak i w aluminium, to efekt ten wyraźniej występuje w miedzi; w blasze tej wy- stępuje grubsza strefa o ultradrobnym ziarnie.
EN
The changes of microstructure and texture in explosively bonded aluminium and copper sheets of technical purity observed in layers located near the bonding area were analyzed in the study (Fig. 1). The bonding process was investigated with multiscale analyzes using light microscopy and scanning electron microscopy equipped with electron backscattered diffraction facility for the measurements of local orientations. For the applied technological parameters of the bonding process, strong changes in geometry of surfaces of bonded plates have been observed (Fig. 2 and 3). In most observed cases, the bonding may be classified as 'flat' or 'wavy' one with an intermediate phase. As a result of melting in the bonding area, the formation of intermetalic layer phase of CuAln-type, with n= 1÷2.7 was observed (Fig. 4). This indicates changes in Cu and Al concentrations depending on the location of analyzed area, which leads to changes in mechanical properties (Fig. 5 and 6). Other characteristic features of the bonding process were: the strong grain refinement at the both sides of intermetalic layer (more clearly observed in Cu) and strong textural changes along ND in both sheets (Fig. 7÷10).
PL
Mechanizm stanowi ciągle silnie nierozpoznane zagadnienie. Jednym z kluczowych zagadnień związanych z opisem mechanizmów zarządzających procesem przemiany tekstury podczas wyżarzania jest identyfikacja typu granicy poprzez migrujący front rekrystalizacji. Celem niniejszej pracy było określenie dominujących relacji orientacji, pomiędzy stanem odkształconym a nowo powstałymi ziarnami we wczesnych stadiach rekrystalizacji w metalach o sieci regularnie ściennie centrowanej, o średniej i małej energii błędu ułożenia. Analizę prowadzono na monokryształach o orientacjach stabilnych w płaskim stanie odkształcenia, tj. „Goss”{110}<001> oraz „brass”{110}<112>. Monokrystaliczne próbki z Ni, Cu, Cu-2%Al odkształcono w próbie nieswobodnego ściskania do ok. 40 %. Następnie odkształcony materiał został poddany wyżarzaniu celem analizy preferencji w występowaniu relacji orientacji poprzez front rekrystalizacji. Analizę przeprowadzono z wykorzystaniem wysokorozdzielczej skaningowej mikroskopii elektronowej i techniki dyfrakcji elektronów wstecznie rozproszonych (SEM-FEG/EBSD). Przeprowadzona analiza preferencji w rozkładzie osi i kąta dezorientacji poprzez front rekrystalizacji pokazuje, że relacje dezorientacji zbliżone do 40°<111> są realizowane jedynie sporadycznie. Wykazano, że dominują rolę odgrywają dezorientacje określone kątami z zakresów 25-35° i 45-55° oraz obrotem dookoła osi <122>, <012>, <112> zgrupowanych zazwyczaj w pobliżu normalnych do wszystkich czterech płaszczyzn {111}.
EN
The objective of this paper is to identify the predominant crystallographic relations between deformed state and recrystallized grains during the early stages of recrystallization of fcc metals with medium and low stacking fault energy. The experimental investigations, based on high resolution SEM/EBSD measurements, have focused on the transformations which occur in plane strain compressed single crystals with stable orientations. After annealing the disorientation across the recrystallization front defines the final rotation by angles in the ranges of 25-35° and 45-55° around axes mostly grouped near the <122>, <012>, <112> and <111> directions located around the normals of all four {111} slip planes.
EN
Quality control of the products used in plant protection is provided mainly by producers of pesticides. According to EU regulations it is obligatory for countries to have an independent quality control system for pesticides present on the market. An independent system is very important for the appropriate functioning of the domestic plant protection. It ensures discipline towards producers and retailers. In Poland such monitoring has a long tradition. Post registration quality determination are provided by the Institute of Plant Protection, samples are taken by the inspectors from the Plant Protection and Seeds Inspectorate through the whole country. The 400 annual limit includes some samples analyzed as a result of a claim or a low suit for compensation due to improper effects or lack of effectiveness. Biologically active substance (a.s.) is the most important quality parameter. Many samples show discrepancies (either lower or higher results), however significantly defected is only about 1% of determinations. In cases of significant quality flaws the Plant Protection and Seeds Inspectorate may issue an administrative decision to withdraw a batch of a product from distribution and use. It is crucial to posses technical capabilities to provide quality testing for all pesticides that are currently or were in the past in use in Poland. Particularly, in cases of claims, recalls and law suits.
EN
In this paper we discussed using chromatographic techniques such as gas chromatography (GC and GC/MS), liquid chromatography (HPLC/DAD and RR-HPLC) and planar chromatography (TLC and HPTLC), also near infrared spectroscopy (NIR) in identification analysis of plant protection products falsifications. Examples are given of typical falsifications and methods of their detection.
first rewind previous Strona / 2 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.