Nowa wersja platformy, zawierająca wyłącznie zasoby pełnotekstowe, jest już dostępna.
Przejdź na https://bibliotekanauki.pl
Preferencje help
Widoczny [Schowaj] Abstrakt
Liczba wyników

Znaleziono wyników: 32

Liczba wyników na stronie
first rewind previous Strona / 2 next fast forward last
Wyniki wyszukiwania
help Sortuj według:

help Ogranicz wyniki do:
first rewind previous Strona / 2 next fast forward last
1
Content available remote Wybrane aspekty prawne i techniczne norm wyrobów budowlanych
100%
PL
Wprowadzenie jednolitych wymagań w zakresie wytwarzania i montażu konstrukcji pozwala na swobodny obrót gospodarczy i ogranicza ryzyko związane z wejściem na nowe rynki.
EN
The paper analyzes, from the geometrical aspect, the quality of the new flux cored wire intended for cladding process in function of changes in cladding parameters such as welding speed, coefficient of thermal conductivity, power source setting, the length of projecting portion of the electrode. The results of bead geometry analysis allows to illustrate the nature of the impact of the examined input variables on parameters of generated surface. The most important parameters here are the depth of penetration and the height of clad. The experimental data were processed using the Plackett-Burman experiment, which describes the impact of technological parameters on the main parameters used during production of resisting panels. It shows mathematical relations describing correlations between the input parameters and the value of depth of penetration and hight of bead made by Flux Cored Arc Welding (FCAW).
3
Content available remote Analiza występowania niezgodności spawalniczych w podstawach wież wiatrowych
100%
PL
Artykuł przedstawia problematykę analizy kontroli jakości przy spawaniu wielkogabarytowych konstrukcji podstaw wież wiatrowych typu offshore. W pracy przedstawiono zagadnienia związane ze statystyką kontroli jakości dla jednego z typów fundamentowania wież wiatrowych. Wymagania odbiorowe konstrukcji fundamentu oprócz badań wizualnych i badań magnetyczno-proszkowych zostały uzupełnione wymaganiami badań ultradźwiękowych po realizacji montażu wielkogabarytowych elementów konstrukcji morskich wież wiatrowych. Praca zawiera analizę występowania niezgodności spawalniczych zaobserwowanych na 7 elementach ważących po 500 ton podstaw wież wiatrowych. Analizę przeprowadzono dla niezgodności wykrytych metodą ultradźwiękową po wykonaniu blisko 5 kilometrów spoin zrealizowanych na jednym z projektów zlokalizowanym na Morzu Północnym u wybrzeży Niemiec.
EN
The article presents the analysis of the problems of quality control in welding large structures of the towers foundations of offshore wind. The paper presents issues related to statistical quality control for one type of foundation wind towers. Requirements of construction of the foundation should be checked by visual and magnetic testing and ultrasonic testing after the execution of the assembly of large structural elements of marine wind towers. The paper contains an analysis of the occurrence of imperfections observed at 7 elements, which every is 500 tons heavy. The analysis was carried out for welding imperfection detected by ultrasonic testing after nearly five kilometers joints completed in one of the projects located in the North Sea coast of Germany.
4
100%
PL
W pracy przedstawiono zagadnienie zabezpieczania powierzchni narażonych na ścieranie pracujących w warunkach kopalni odkrywkowej. Zebrano informacje o najpowszechniej stosowanych materiałach na elementy zabezpieczające przed nadmiernym zużyciem ściernym. Podjęto charakterystykę materiałów hutniczych oraz materiałów wytwarzanych w procesach napawania prewencyjnego z zastosowaniem drutów rdzeniowych. Opisano zastosowanie poszczególnych materiałów wraz z ich charakterystyką dotyczącą własności i struktury. Szczególnie skupiono się na elementach wykonanych technikami spawalniczymi z wykorzystaniem drutów rdzeniowych.
EN
The paper presents the problem of protection of surface exposed to abrasion working in the conditions of the open-cast mine. Information on the most commonly used materials for abrasive wear protection has been collected. The characteristics of metallurgical materials and materials produced in the preventive surfactant processes using core wires were taken. The use of individual materials has been described together with their properties and structure characteristics. Particularly focused on elements made by welding techniques using core wires.
5
Content available remote Wpływ parametrów w metodzie TIG na odkształcenia kątowe stali X5CrNi18-10
100%
PL
W pracy przedstawiono zagadnienie wpływu nastaw natężenia prądu spawania oraz odległości elektrody od materiału rodzimego na wielkość kątowych odkształceń próbek przetapianych metodą TIG. Do tego celu wykorzystywano metody planowania eksperymentu. Prace doświadczalne przeprowadzono dla materiału gatunku X5CrNi18-10. Dokonano analizy zmian odkształcenia próbki w zależności od nastaw natężenia prądu spawania w zakresie od 100 do 200 A oraz zmiany odległości elektrody od przedmiotu spawanego w zakresie od 2 do 4 mm. Do prób technologicznych wykorzystano automatyczny przesuw uchwytu poprzez zastosowanie głowicy do mechanizacji spawania. Przygotowane próbki zostały poddane precyzyjnym pomiarom współrzędnościowym, celem określenia odkształceń kątowych.
EN
The paper presents the problem of the influence of the current setting and the distance between the electrode and the object welded by TIG method on the corresponding changes the angular deformation of the element. Design of the experiment method was used. Experimental test were performed for material grade X5CrNi18-10. The analysis of the changes in specimen deformation based on the current setting in the range from 100 to 200 A and the change of the distance between the electrode and the welded object in the range from 2 to 4 mm was made. Automatic travelling of the gun by using the head for welding mechanization was used to perform technological tests. Prepared specimen were subjected to precise coordinate measurement to determine the angular deformation.
6
Content available remote Płyty trudnościeralne - aspekty wytwarzania i zastosowania
100%
PL
Najskuteczniejszym sposobem przeciwdziałania zużyciu jest wykonywanie powierzchni roboczych technologiami spawalniczymi z materiałów o specjalnych własnościach. Jednym z tych procesów jest napawanie prewencyjne, stosowane do zabezpieczenia powierzchni roboczych, np. płyt przesypowych czy też obudów i przesypów taśmociągów wykorzystywanych w przemyśle wydobywczym i wytwórczym.
7
Content available Repair Welding of the Massive Cast
100%
EN
The rebuilding technologies are used to develop surface of ladle. Among many welding methods currently used to obtain surface layer without defects one of the most effective way of rebuilding is using metal arc welding. This additional material gives more possibilities to make expected quality of rebuild surface. Chemical composition, property and economic factors allow to use metal wire. Because of these reasons, solid wire gives opportunity to be wildly used as material to rebuild or repair the surface in different sectors of industry. The paper shows a few ways to rebuild the surface in the massive cast with the use of metal active gas welding for repair. The work presents studies of defect in the massive cast. It contains the pictures of microstructures and defects. The method of removing defects and the results of checking by visual and penetrant testing methods are shown. The papers describes the methodology of repair the ladle with metal active gas welding, preheating process and standards non destructive testing method.
PL
W pracy przedstawiono zagadnienie określania zmian nastaw prądu napawania i odpowiadające temu zmiany uzyskiwanych przekrojów napoin w przypadku użycia drutu rdzeniowego z wypełnieniem rutylowym. Wykorzystywane do tego celu próby pozwalają, zdaniem autorów, z dużą dokładnością określić ilość wykonywanych ściegów dla zadanych przekrojów napoin i spoin. W pracy zebrano wyniki badań nad wielkościami geometrycznymi złącza wykonanego przy zmieniających się nastawach prądu. Do prób napawania z automatycznym posuwem palnika wykorzystano materiał dodatkowy o średnicy 1,2 mm. Uzyskane napoiny zostały poddane badaniom metalograficznym makroskopowym i przeanalizowane pod kątem uzyskanej geometrii ściegu.
EN
The paper presents the problem of determining changes in the settings of the welding current and corresponding to the change in cross-section welds obtained when using rutil cored wire. Used for this purpose according to the authors attempt to allow has impact on the basic parameters characterizing the welded joint. The paper presents results of research on geometric quantities joint made at changing the parameters set welding current . Tests were carried out with automatic feed welding torch, using the additive material with diameter of 1.2 mm. The resulting welds have been tested and analyzed metallographic macroscopic for checking geometry.
EN
The paper discusses the effect of the heat input in the case of welding with solid and cored wire, respectively to the quality of the obtained joints. Formulas used for this purpose do not allow for the form of the filler, which, in the authors' opinion, has an effect on the basic parameters characterizing the welded joint. The paper presents the results of research on the geometric sizes of a joint made with a similar heat input, but using the filler in the form of, respectively, solid and cored wire. Investigations were carried out on fillet-weld joints that were subjected to macroscopic metallographic examinations. Studies have shown that the heat input given without allowing for the form of the filler does not reflect the changes that occur in the welded joint due to the thermal welding cycle.
PL
W pracy przedstawiono wyniki badań nad napoinami trudnościeralnymi przeznaczonymi do pracy w warunkach przemysłu cementowego. Głównym celem pracy była próba wykonania pełnego kwalifikowania procesu napawania półautomatycznego zgodnie z wymaganiami PN EN ISO 15614-7 przy wykorzystaniu drutu dającego twardości sięgające do 60 HRC warstwy wierzchniej w jednym przejściu o ściegu szerokim na 10 i 20 mm. Następnie próbki poddano badaniom nieniszczącym to jest badaniom wizualnym i penetracyjnym oraz badaniom niszczącym w postaci badań metalograficznych makroskopowych i mikroskopowych, badaniu twardości. Zastosowanie niniejszej normy nie daje możliwości akceptacji kwalifikowania technologii napawania z wykorzystaniem materiałów dających bardzo twarde warstwy wierzchnie zawierające w swojej strukturze wydzielenia węglikowe.
EN
The paper presents results of research on surface hard wearing designed to work in the cement industry. The main objective of the study was to perform a full qualification semiautomatic welding process in accordance with the requirements of PN EN ISO 15614-7 using a wire giving a hardness of up to 60 HRC surface layer in a single pass with a bead wide for 10 and 20 mm. The samples were then subjected to non-destructive testing is testing and visual and liquid penetrant testing destructive testing in the form of macroscopic and microscopic metallographic, hardness test. Application of this standard does not allow acceptance of qualification of welding technology using materials with a very hard outer layer containing in its structure separating carbide.
PL
W pracy przedstawiono zagadnienie wpływu zmian nastaw prądu napawania z użyciem drutu rdzeniowego z wypełnieniem metalicznym i odpowiadające temu zmiany uzyskiwanych przekrojów napoin. Wykorzystywane do tego celu próby i określone równania pozwalają zdaniem autorów z dużą dokładnością określić ilość wykonywanych ściegów dla zadanych przekrojów napoin i spoin. W pracy zebrano wyniki badań nad wielkościami geometrycznymi złącza wykonanego przy określonych nastawach prądu. Do prób automatycznego napawania wykorzystano materiał dodatkowy T 46 3 MM 2 H5 o średnicy 1,2mm. Wykonane napoiny zostały przygotowane do badań metalograficznych makroskopowych i analizowane pod kątem uzyskanej geometrii ściegu oraz uzyskanej masy ściegu.
EN
The paper presents the problem of determining changes in the settings of the welding current and corresponding to the changes in cross-section welds obtained when using metal cored wire. Used for this purpose tests and determined equations, according to the authors, allows to determine the number of joints performed for specified sections of welding beads. Tests were carried out with automatic feed welding torch, using the additive material T 46 3 MM 2 H5 with diameter of 1.2 mm. The paper presents results of research on weight of bead and geometric quantities joint made by certain weldign current settings. The resulting welds have been tested and analyzed metallographic macroscopic for checking geometry and weight of bead.
EN
The surfacing technologies are used for constitution of protection layer against wear and is destined for obtaining coating with high hardness. Among many weldings methods currently used to obtain the hard surface layer one of the most effective way of hardfacing is using flux cored arc welding. This additional material gives more possibilities to make expected hard surface layer. Chemical composition, property and economic factors obtained in flux cored wire are much richer in comparison to these obtained with other additional materials. This is the reason why flux cored wires give possibilities of application this kind of material for improving surface in different sectors of industry. In the present paper the imperfection in the layers was used for hardfacing process in different situations to show the possible application in the surface layer. The work presents studies of imperfection of the welds, contains the picture of microstructures, macrostructures and shows the results of checking by visual and penetrant testing methods.
13
Content available remote Zużywanie erozyjne płyt trudnościeralnych wykonanych drutem SSA Corthal 61
63%
PL
W pracy został przedstawiony problem napawania płyt trudnościeralnych wykorzystywanych w przemyśle wydobywczym, pracujących w warunkach zużycia metal--minerał. Zebrane w pracy wyniki prezentują właściwości dwóch napoin wykonanych z różnymi parametrami. Badania zużycia erozyjnego przeprowadzono przy kącie padania strumienia erozyjnego równym 30° z wykorzystaniem piaskarki przemysłowej. Trudne warunki pracy napoin wskazują na większą rolę parametrów geometrycznych napoiny niż jej właściwości mechanicznych i struktury w odporności na zużywanie.
EN
This paper shows the problem of surfacing hard facing plates used in mining industry, working in the condition of metal-mineral wear. The results presented in the paper refer to 2 hard faced plates made according to different parameters. The research of the wear was carried out with the 30° angle erosive stream. Severe conditions of work of hard faced plates show the bigger role of hard faced plates geometrical parameters than its mechanical and structural properties in wear resistance.
14
Content available remote Statystyczna ocena wpływu parametrów napawania SSA na geometrię napoin
63%
PL
W artykule omówiono problem określenia parametrów istotnych dla napawania drutem rdzeniowym samoosłonowym. Metoda SSA jest jedną ze spawalniczych metod, która daje duże możliwości w wytwarzaniu napoin o zróżnicowanym składzie chemicznym i dobrej jakości. Istotne jest określenie, które z parametrów napawania mają znaczący wpływ na właściwości napoiny. Zastosowanie planu Placketta-Burmana umożliwiło statystyczną ocenę istotności wpływu wybranych parametrów napawania na geometrię napoiny.
EN
In this work problem of determining of parameters for surfacing by using self-shielded arc is concerned. Self shielded arc surfacing (SSA) is one of the welding methods that gives big opportunities for producing cladding with wide range of chemical composition and good quality. The problem is to determine which parameters have the significant influence for producing cladding with defined properties. Using Plackett-Burman's design gives opportunities to statistic evaluation of significant parameters on cladding properties especially its geometry.
PL
W artykule omówiono napawanie i eksploatację płyt trudnościeralnych wykorzystywanych w przemyśle wydobywczym, pracujących w warunkach zużycia metal-minerał. Otrzymane wyniki prezentują właściwości dwóch napoin wykonanych z różnymi parametrami. Badania zużycia erozyjnego przeprowadzono z wykorzystaniem piaskarki przemysłowej przy kącie padania strumienia erozyjnego 60°. Trudne warunki pracy napoin wskazują na jednoczesny wpływ parametrów geometrycznych napoiny oraz jej właściwości mechanicznych i struktury na odporność na zużywanie.
EN
The paper shows the problem of exploitation and hard-facing of abrasive-resistant plates used in mining industry, working in the condition of metal-mineral wear. In the paper presented results refer to two hard-faced padding welds made according to different parameters. The research of the wear was carried out with the 60° angle erosive stream. Severe conditions of work of hard-faced abrasive-resistant plates show the simultaneous role of hard-faced padding weld geometrical parameters and its mechanical and structural properties in the wear resistance.
16
Content available remote Plany jakości przy wytwarzaniu konstrukcji stalowych
63%
PL
Artykuł zawiera opis wymagań dotyczących planów jakości z uwzględnieniem norm przedmiotowych. Zawiera opis hierarchii systemów jakości, czynników produkcji mogących mieć wpływ na uzyskiwaną jakość wyrobów spawanych. Przedstawia kierunki działań jakościowych przy wytwarzaniu konstrukcji stalowych, wskazuje identyfikację punktów nadzoru, opisuje zasady tworzenia planów jakości w odniesieniu do wymagań PN EN ISO 9001, PN EN ISO 3834, PN ISO 10005 oraz PN EN 1090.
EN
The article contains a description of the requirements for quality plans with regard to these standards. Contains a description of the hierarchy of quality systems, production factors which may affect the quality of welded products obtainable. Qualitative ways forward the manufacture of steel structures, indicates the identification of points of supervision, describes the rules for creating quality plans in relation to the requirements of the PN EN ISO 9001, PN EN ISO 3834, PN ISO 10005 and PN EN 1090.
17
Content available remote Wybrane aspekty napraw odlewów korpusów urządzeń energetycznych
63%
PL
Praca przedstawia analizę sposobu usuwania wad odlewniczych i wpływ wstępnego podgrzewania na jakość napawania drutem proszkowym. W artykule została przedstawiona charakterystyka ogólna materiałów używanych na odlewy korpusów ze wskazaniem na skład chemiczny oraz podstawowe właściwości mechaniczne. Wymieniono także główne cechy jakimi powinny się charakteryzować materiały użyte na odlewy oraz omówiono zabiegi obróbki cieplnej mającej wpływ na jakość naprawianych powierzchni z szczególnym uwzględnieniem zagadnień podgrzewania przed pracami naprawczymi -regeneracyjnymi. Omówiono wady powstałe w procesie odlewania jak i zasygnalizowano niezgodności spawalnicze mogące powstać w trakcie prac spawalniczych. Wymienione zostały występujące wady, przyczyny ich występowania jak i sposoby, dzięki którym można ich uniknąć. Część pracy została poświęcona praktycznym zagadnieniom napraw odlewów. Omówiono główne czynności przygotowawcze przed rozpoczęciem prac spawalniczych mających istotne znaczenie na jakość prowadzonych prac. Opisano doświadczenia w zakresie żłobienia palnikiem propanowo-tlenowym wad odlewniczych w połączeniu z napawaniem powstałych ubytków przy wykorzystaniu drutu proszkowego i konsekwencji braku zastosowania podgrzewania przed żłobieniem.
EN
The paper presents an analysis of how to remove casting defects and the influence of preheating on the quality of welding flux cored wire. This article presents the general characteristics of the materials used for casting bodies with an indication of the chemical composition and the basic mechanical properties. Also highlights the main features of which should be characterized by the materials used for casting and heat treatment procedures discussed having an impact on the quality of the repaired area with particular emphasis on the heating before repair work. Defects which are discussed in the process of casting and welding signaled discrepancies that may arise during welding. These defects are present, their causes, and ways in which they can be avoided. Part of the work has been devoted to practical issues casting repairs. These are the main preparatory activities before welding which are important to the quality of the work. Experiments are described in terms of gouging torch propane-oxygen casting defects in conjunction with the resulting loss hardfacing using flux-cored wire and the consequences of non-application of heating before gouging.
18
63%
PL
W pracy przedstawiono wyniki badań nad napoinami wykonanymi prądem pulsującym. Głównym celem pracy było określenie wielkości geometrycznych wykonanych napoin przy założonych wartościach napawania impulsowego. Podczas prób napawania zmieniano częstotliwość impulsu, napięcie impulsu, czas impulsu i długość wolnego wylotu drutu. Parametry procesu były tak dobierane by uzyskać jak najwyższe i najszersze napoiny przy zachowaniu dużej stabilności procesu napawania. Jednym z głównych kryteriów określających przydatności napoiny do użycia jest stopień wymieszania materiału napoiny z materiałem podłoża. We wszystkich badanych napoinach procentowy udział metalu podłoża w napoinie wahał się między 20% a 30%. Uzyskanie niższych wartości wymieszania prowadziło w tym przypadku do zmniejszenia stabilności procesu napawania i wpływało negatywnie na jakość otrzymywanych napoin.
EN
The paper presents results of research on cladding made with pulse current. The main objective of this study was to determine geometric size of the welds made with the assumed values of pulse welding. During the experiment surfacing pulse frequency, pulse voltage, pulse duration and length of the stick wire were varied. The process parameters were so diverse to achieve the highest and widest of the deposit while maintaining the high process stability surfacing. One of the main criteria for determining the suitability of the deposit to use is the dilution of the material of the deposit with the parent material. In all examined welds percentage of the base metal in the weld pad fluctuated between 20% and 30%. Obtaining the lower dilution rate led to diminishing the stability of the deposition process and affected adversely the quality of the welds.
19
Content available remote Wpływ nastawy prądu na zmiany wielkości geometrycznych przekrojów napoin
63%
PL
W pracy przedstawiono zagadnienie określania zmian nastaw prądu napawania i odpowiadające temu zmiany uzyskiwanych przekrojów napoin w przypadku użycia drutu litego. Wykorzystywane do tego celu próby pozwalają zdaniem autorów z dużą dokładnością określić liczbę wykonywanych ściegów dla zadanych przekrojów napoin i spoin. W pracy przedstawiono wyniki badań nad wielkościami geometrycznymi złącza wykonanego przy zmieniających się parametrach prądu przy nastawach 150, 200, 250, 300 A. Wykonano próby napawania z automatycznym posuwem palnika, przy wykorzystaniu materiału dodatkowego w postaci drutu litego o średnicy 1,2 mm. Uzyskane napoiny zostały poddane badaniom metalograficznym makroskopowym i przeanalizowane pod kątem uzyskanej geometrii ściegu.
EN
The paper presents the problem of determining changes in the settings of the welding current and corresponding to the change in cross-section welds obtained when using solid wire. Used for this purpose according to the authors attempt to allow has impact on the basic parameters characterizing the welded joint. The paper presents results of research on geometric quantities joint made at changing the parameters set welding current by settings of 150, 200, 250, 300 A. Tests were carried out with automatic feed welding torch, using the additive material with diameter of 1.2 mm. The resulting welds have been tested and analyzed metallographic macroscopic for checking geometry.
first rewind previous Strona / 2 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.