Knowing the reflection, transmission, and absorption properties of the yarns from which the woven fabric is made, prediction of a fabric’s UV-protective properties is simple. Using the geometrical properties of monofilament yarns and fabrics, which were determined optically, and following the cover factor theory, we have determined the areas of fabrics covered with no yarns, only one yarn, and two yarns. From a special selected set of high-module polyethylene terephthalate (PET) monofilament materials (e.g., fabrics), we have elaborated a method for determining the reflection, transmission, and absorption of yarns. By first defining the differently covered areas of fabrics, we were able to use them in a mathematical model for calculating and predicting the UV-protective properties of the fabrics. The calculated and measured values of the UV-protective properties of the selected test fabrics were highly correlated, with a correlation coefficient >0.98.
2
Content available remote Zastosowanie odpadowego PET do wzmacniania betonu
PL
Większość butelek z poli(tereftalanu etylenu) (PET) po użyciu staje się odpadem. W artykule przedstawiono metody recyklingu odpadowego PET jako dodatku do betonu. Zbadana została trwałość włókien PET w alkalicznym środowisku matrycy cementowej. Stwierdzono spadek wytrzymałości na rozciąganie, spowodowany degradacją chemiczną włókien. Odporność PET na hydrolizę została poprawiona przez zastosowanie powłoki ochronnej z kopolimeru EVA.
EN
Most poly(ethylene terephthalate) (PET) bottles become waste after their usage. This paper presents a method to recycle wasted PET as a concrete reinforcing material. The long-term durability performance of recycled PET fibers in the alkaline environment of cement matrix was measured. Recycled PET fibers showed reduced tensile strength. The chemical resistance of the PET against hydrolysis was improved by dip coating method in a solution of EVA copolymer.
PL
W pracy badano efekty ilościowe modyfikacji enzymatycznej włókien PET o zróżnicowanej wyjściowej fizycznej mikrostrukturze w zakresie budowy ich powierzchni, odnosząc je do efektów uzyskiwanych w stosowanej dotychczas obróbce chemicznej. Efekt modyfikacji rozpatrywano w aspekcie zmian właściwości powierzchniowych i wybranych właściwościach objętościowych badanych włókien.
EN
The subject of a doctoral dissertation was evaluation of quantitative effects of enzymatic treatment and a wide chemical surface modification of polyester fibres varying in physical initial micro-structure and the consequences in terms of surface properties and selected volume properties of investigated fibres. Glossy, continuous polyester fibres with poly(ethylene terephthalate) with different draw ratios (R = 3,0x; R = 3,5x; R = 4,0x; R = 5,2x) were used for the investigations. The modification of PET fibre by the chemical method was carried out with the use of sodium hydroxide solutions and amine solutions with different functionality and by the biochemical method using the enzymatic preparations diversified with respect to their origin, biochemical characteristics and application conditions. Effect of enzymatic modification, at proper selection of enzyme, it is more advantageous from gotten in classic chemical modification at utilization of solution NaOH, as well as amines one and two-function and it is subordinated from kind of enzymatic preparations. In the light of the test results obtained the method of PET fibres modification with the use of enzymatic preparations should be accepted as an effective, pro-ecological and energy-saving approach to changing the fibre surface structure leading to the elimination or essential reduction of several unfavourable fibre properties.
PL
Przedstawiono wyniki badań nad wpływem dodatku organicznych włókien z poli(tereftalanu etylenu) na właściwości tłoczyw poliestrowo-szklanych typu DMC. Badania są kontynuacją prac nad modyfikacją tłoczyw poliestrowych [1, 2] i polegają na częściowym zastąpieniu w nich włókien szklanych włóknami PET. Rezultatem badań jest opracowanie tłoczywa poliestrowego z hybrydowym wzmocnieniem rowing szklany-włókno PET w stosunku objętościowym 3:1. W porównaniu z tłoczywem standardowym wzmocnionym samym włóknem szklanym, charakteryzowało się ono wyraźnie zmniejszoną chłonnością wody oraz lepszą płynnością prasowniczą przy zachowaniu dobrych właściwości mechanicznych, dielektrycznych i termicznych. Do tłoczyw mogłyby być wykorzystane poliestrowe włókna techniczne, pochodzące z powtórnego przetworzenia odpadów z poli(tereftalanu etylenu), jak np. butelki, folie i in.
EN
This report presents some results of the use of PET fibers as a partial replacement for glass in polyester moulding compounds. It has been found that replacing 1/4 vol. part of the glass by chopped PET fibers gives almost identical physicomechanical properties of mouldings to compounds containing glass alone.