EN
The energy applied during breakage is the key to enhancing the magnetite liberation degree and improving quality. The relationship between energy and liberation properties remains unclear due to various complicated factors affecting mineral liberation. Therefore, this work aims to study the effect of energy on the breakage characteristics of magnetite ores; the impact breakage test was conducted on magnetite particle groups at different energies using a drop weight impact tester; the statistical analysis was performed based on the fractal theory to research the particle size distribution; the fracture morphology and liberation properties of these ores were analyzed using scanning electron microscope and mineral liberation analyzer. Results show that the particle size distribution of magnetite after breakage conforms to the fractal law. The larger the energy, the greater the fractal dimension for this distribution, showing a linear relation between them, which implies that the fractal dimension can evaluate the breakage degree. The fracture morphology of magnetite ores indicates that as the energy increases, the intergranular fracture evolves into transgranular fracture, proving the influence of energy on fracture modes. It is found that the magnetite liberation degree first increases and then decreases with the rising of energy, indicating that the magnetite liberation can be improved at an appropriate amount of energy. The above conclusions provide a theoretical reference for optimizing energy and improving broken product quality.
EN
The characterization of textural properties of minerals is closely related to the process of their respective liberation. Measurements of mineral liberation, related to grinded ore, can be performed using optical ore microscope, by conventional, classical methods – point counting, linear intercepts method or planimetric measurements method (2D). Modern automatic devices and sophisticated measurement techniques (QEMSCAN/MLA) imply recording free surfaces area of mineral grains on polished sections samples in order to determine mineral degree of liberation. Value of mineral liberation obtained over free surfaces area can be of interest to flotation concentration, although not for gravity separation or, for example, magnetic separation. The prediction accuracy for behavior of one feed ore during the concentration process depends on the method of measuring/recording mineral liberation. Considering raw materials with complex textural characteristics it is crucial which method will be applied for determination of mineral liberation respecting whether for concentration process is crucial physical or chemical method.
PL
Charakterystyka właściwości tekstury minerałów jest blisko związana z procesem ich uwolnienia. Pomiary uwolnienia minerałów powiązane są z mieleniem rudy i mogą być wykonane za pomocą mikroskopu optycznego przy zastosowaniu konwencjonalnych metod – liczenia punktów, metody linii przecięcia albo metody pomiarów planimetrycznych (2D). Nowoczesne urządzenia automatyczne, jak również wyrafinowane techniki pomiarowe (QEMSCAN/MLA) stosują pomiar pól powierzchni wolnych ziaren minerału na próbkach wypolerowanych przekrojów w celu określenia stopnia uwolnienia minerałów. Wartość tego uwolnienia otrzymana na podstawie pola powierzchni wolnej może być przedmiotem zainteresowania w kontekście prowadzenia procesu flotacji, aczkolwiek nie w przypadku wzbogacania grawitacyjnego, czy magnetycznego. Prawidłowość prognozy odnośnie zachowania rudy podczas procesu zależy od metody oceny uwolnienia minerałów. Biorąc pod uwagę surowce o skomplikowanej teksturze bardzo ważnym jest, którą metodę zastosuje się w celu określenia stopnia uwolnienia minerałów pamiętając także o tym, czy dany proces jest oparty o metody fizyczne, czy też chemiczne.
3
Content available Froth flotation of Aljustrel sulphide complex ore
EN
Froth flotation of copper-zinc-lead ores is a complex process based on similar metallurgy processing and strong interactions between chalcopyrite and sphalerite. These types of ores represent 15% of the world production and 7.5% of copper deposits all over the world. In the present study, an attempt is made to assess the feasibility of froth flotation of a complex sulphide ore, where the effect of liberation grade as well as depressant, collector and frother dosage was studied. Copper flotation is dependent on the mineral liberation grade, which is significantly related with the size distribution. It was shown that longer grinding time increased the Cu grade but decreased the copper recovery due to the presence of very fine particles. Lime and sodium metabisulphite, used as depressants, allowed to achieve a good flotation performance. It was shown that for this type of ore lower dosage of the collector should be applied. Finally, a higher frother dosage led to a greater selectivity and reduced entrainment of very fine particles, but also caused low kinetic ratio and low recovery of valuable minerals. A well-defined flotation objective was imperative for a good liberation grade and reagents dosage selection, mainly for complex sulphide ores. A useful contribute was given to a better technical understanding of flotation of a complex sulphide ore from the Moinho deposit.
EN
High Sb and As contents in zink and lead concentrations, have always been obtained by conducting experiments with flotation concentration of complex poly-mineral Pb-Zn-Sb-As-(Ag, Au) ore ground to varied grinding finenesses. Chemical analyses were not sufficient to explain this phenomenon. With the help of detailed mineralogical analyses of the run-of-mine ore, and, the obtained concentrates that followed, the problem has been solved. All ore minerals were identified, the degree of liberation of galena and marmatite measured, and the frequency of occurrences of certain types of binary, ternary and higher locked grains determined. The measurements of the liberation degree of galena and marmatite (at the fineness of grinding of 83% -0.074 mm), in the obtained concentrates have shown that the increase in a grinding fineness can only partially result in the increase in recovery and provide better concentration results. In addition, the use of new selective low-cost flotation reagents is required to separate hard-to-beneficiate pairs of sulphide minerals with very similar flotation properties.
PL
Wysokie zawartości Sb i As w koncentratach cynku i ołowiu zawsze były uzyskiwane przy prowadzeniu flotacji złożonych polimetalicznych mieszanin Pb-Zn-Sb-As-(Ag, Au) o drobnym uziarnieniu. Analizy chemiczne okazały się niewystarczające do wyjaśnienia tego zjawiska. Za pomocą szczegółowych analiz mineralogicznych przeprowadzanych na rudzie oraz otrzymanych koncentratach problem ten został rozwiązany. Zidentyfikowano wszystkie minerały rudne, stopień uwolnienia galeny oraz marmatytu oraz częstość występowania określonych związków dwu i trójskładnikowych lub bardziej złożonych. Pomiary stopnia uwolnienia galeny oraz marmatytu (o zawartości ziaren -0,074 mm równej około 83%) w otrzymanych koncentratach wykazały, że wzrost ilości drobnych ziaren może być jedynie częściowym powodem wzrostu uzysku i lepszych wyników jakości koncentratu. Dodatkowo, zastosowanie nowych, tanich odczynników flotacyjnych jest warunkiem rozdziału trudnych do wzbogacenia minerałów siarczkowych o podobnych właściwościach flotacyjnych.
EN
The methods are described of selective separation of thallium mineral lorandite from the Allchar hydrothermal-volcanogenic Sb-As-Tl deposit (FYR Macedonia) characterized by relatively complex mineralization. In addition to antimony and arsenic, the Allchar Mine at the village of Majden works one of the richest thallium mineral lorandite deposits. The aim of the research was to separate lorandite as much and as free grain as possible mainly through physical concentration. Thallium is very important because of a possibility to apply its mineral lorandite (TlAsS2) in obtaining knowledge in fundamental investigations. The reaction between Tl and solar neutrinos, producing Pb, is on the purpose of studying the neutrino flux from the Sun. For this purpose, a thallium-rich mineral is required as the target. Geochemically natural, pure thallium mineral lorandite is used to test solar neutrino under the current, two decades long LOREX Project. The Allchar ore from Crveni Dol contains a comparatively complex association of Sb-As-Tl minerals: pyrite, marcasite, antimonite, arsenopyrite, realgar, auripigmentum, barite, cinnabar, and accessory thallium lorandite, vrbaite, raguinite, picopaulite, parapierrotite, rebulite, greigite, tetrahedrite, and various sulphosalts that are found only in Allchar. The research used conventional laboratory methods for mineral fractionation and for liberation of lorandite grains, which included size reduction, sieve analysis, Wilfley table, sink and float analysis (bromoform, methylene iodide), electrostatic separation, electromagnetic separation and centrifugal separator. Gradual separation from successive communition and classification of fractions allowed separation of the free sink (heavy) product from which nonconductive minerals, including lorandite, were selected.
PL
Opisano wybrane metody separacji talu z minerału lorandytu ze złoża hydrotermalnego – wulkanogenicznego Sb-As-Tl w Allchar (Macedonia) charakteryzującego sie relatywnie złożoną mineralizacją. Oprócz antymonu i arsenu, kopalnia Allchar w wiosce Majden jest jednym z najbogatszych złóż talu w lorandycie. Celem badań było separacja lorandytu i uzyskanie jak największego uwolnienia minerałów za pomocą separacji mechanicznej. Tal występuje w minerale lorandyt (TlAsS2). Celem badań jest uzyskanie koncentratu bogatego w tal. Czysty tal w minerale lorandyt jest używany do badań neutrin w promieniowaniu kosmicznym w projekcie LOREX Project, realizowanym od 20 lat. Ruda Allchar z CrveniDol zawiera stosunkowo złożoną kombinację związków Sb-As-Tl: pirytu, markazytu, antymonianu, arsenopirytu, reaglaru, auripigmentu, barytu, cynobru, oraz dodatkowo związków talu lorandytu, vrbaitu, raguinitu, pikopaulitu, parapierrotytu, rebulitu, greigitu, tetrahedrytu i różnych sól siarkowych, które można znaleźć jedynie w Allchar. W badaniu zastosowano konwencjonalne metody laboratoryjne separacji mechanicznej i wydzielania ziaren lorandytu, uwzględniając rozdrabnianie, analizę sitową, wzbogacanie na stole Wilfley’a, analizę granulometryczna (w bromoformie, jodku metylenu), separację elektrostatyczną, separację elektromagnetyczną oraz separator odśrodkowy.
EN
The mineral deposit Bor-Cerovo is a relatively simple Cu-(Fe)ore that is becoming poorer and more complex in texture with the depth of mining. The Bor Copper Mine has expanded mine workings to the Cerovo field margins, where the same type of porphyry copper ore was found for which the Bor Mine is known as one of largest in Europe. Under the oxidized zone in the vertical deposit section lie paragenetic mineral associations typical of the cementated zone, or a transitional layer from the primary mineralized rock. Average concentrations of sulphide copper and oxide copper in the primary rock range from 0.263% to 0.164% and from 0.102% to 0.008%, respectively. Concentration of the ore of simple mineral composition has given a product of unsatisfactory both concentrate quality and metal recovery. More study is felt necessary of the structural/textural properties, of the identified mineral relations, and of the rate of mineral product liberation for the given grind fineness. Mineralogical analyses were conducted in the course of laboratory (and technological) tests. It has been learned that chemical analyses of the floatation concentrated material alone were inadequate, especially where complex texture of intergrowths and poor ore were involved. Structural properties and complex integrowths, and concequently low liberation degree, were found to be the reason of poor concentration. This paper discusses importance of the mineral liberation measurement for the technological results of copper ore concentration at the Bor-Cerovo flotation plant, and explains the functional relation between the mineral liberation and the grind fineness. Data on the microscopy of ore texture and the mineral liberation degree presented in this paper are aimed at improving the recovery and grade of chalcopyrite concentrate in the Veliki Krivelj Flotation Plant. Ore microscopy in the laboratory and technological tests indicate that chemical analysis as a tool for monitoring ore flotation is insufficient, especially where the processed ore is complex-textured and poor.
PL
Złoże mineralne Bor-Cerovo jest stosunkowo prostą rudą Cu-(Fe), która staje się uboższa i bardziej złożona w teksturze wraz z głębokością wydobywania. Kopalnia miedzi Bor rozszerzyła prace wydobywcze do granic obszaru Cerovo gdzie znaleziono ten sam typ porfirowej rudy miedzi, z którego kopalnia Bor jest znana jako największa w Europie. Poniżej strefy utlenionej w pionowej strefie złoża znajduje się zespół paragenetycznego minerału typowego dla strefy cementacji, lub warstwa przejściowa ze skały pierwotnie zmineralizowanej. Średnie stężenie siarczanu miedzi i tlenku miedzi w skale pierwotnej znajduje się w przedziale kolejno od 0,263% do 0,164% oraz od 0,102% do 0,008%. Stężenie w rudzie niezłożonego minerału daje produkt niezadowalający pod względem zarówno jakości koncentratu jak i odzysku metalu. Koniecznych jest więcej badań na temat właściwości strukturalnych/tekstury, identyfikacji zależności minerału, oraz na temat stopnia wyzwalania produktu mineralnego dla danego stopnia rozdrobnienia. Przeprowadzono analizę mineralogiczną podczas badań laboratoryjnych (i technologicznych). Dowiedziano się, że analiza chemiczna i flotacja koncentratu mineralnego była nieadekwatna, szczególnie gdy zaangażowana była skomplikowana struktura narostów między ziarnami i uboga ruda. Odkryto, że właściwości strukturalne i skomplikowane narosty, a co za tym idzie niski stopień uwalniania, były powodem ubogiej koncentracji. Artykuł ten omawia znaczenie pomiarów uwalniania minerału dla wyników technologicznych koncentracji miedzi w rudzie w zakładzie flotacyjnym Bor-Cerovo, i wyjaśnia funkcjonalną zależność miedzi uwalnianiem minerału a stopniem rozdrobnienia. Dane mikroskopowe tekstury rudy i stopnia uwalniania minerału prezentowane w tym artykule mają na celu polepszenie odzyskiwania i stopnia koncentratu chalkopirytu w zakładzie flotacyjnym VelikiKrivelj. Laboratoryjne i technologiczne badania mikroskopowe rudy wykazują, że analiza chemiczna jako narzędzie monitorowania flotacji rudy jest niewystarczająca, szczególnie jeśli przetwarzana ruda ma skomplikowaną teksturę i jest uboga.
first rewind previous Strona / 1 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.