2,4-Dinitroanisole (DNAN) has excellent properties as a replacement for 1,3,5-trinitrotoluene (TNT) in melt-cast explosives, and the polymeric modifier used is critical to the mechanical modification of the DNAN/RDX energetic composite. In our research, the typical polymeric modifier acrolein-pentaerythritol resin (APER) was successfully added experimentally to the DNAN/RDX system, and the effects of interfacial interactions on the mechanical properties of these polymers in reinforcing the DNAN/RDX energetic composites were investigated by molecular dynamics simulations, scanning electron microscopy (SEM) and mechanical testing. The results showed that strong attractive interactions exist between the polymer and the explosives, wherein van der Waals forces were found to play the main role. The morphological micro-images also showed tight binding between the polymer/explosive interfaces, which supported the calculated strong interfacial interactions. The mechanical tests confirmed that adding the polymers can obviously reinforce the mechanical strength and toughness of DNAN/RDX systems. The above observations revealed that the cooperative effects of the APER polymer can help to reinforce the interfacial interactions and mechanical properties of DNAN/RDX composites, which is of importance in the formulation and mechanical evaluation of advanced energetic composites.
EN
According to the modal superposition method, the vortex vibration procedure of submerged floating tunnel cable was compiled using Matlab, based on the calculated results, the fatigue damage was predicted. The effects of various factors, such as cable density, cable length, and pretension and velocity distribution on vortex induced fatigue damage in the cable were studied. The results show that velocity distribution has more effect on the cable fatigue damage than cable length, cable density and pretension. Secondly, cable length has also relatively effect on the cable damage fatigue, cable density and pretension has limited in a certain range.
EN
Elastomeric micro- and ultrafine-rubber are first considered as binders in melt-cast explosives for improving the mechanical properties. Acrylonitrile-butadiene rubber (NBR), in ultrafine fully vulcanized form (UF-NBR), carboxylated acrylonitrile-butadiene rubber (CNBR), in ultrafine fully vulcanized form (UF-CNBR), styrene-butadiene rubber (SBR), in ultrafine fully vulcanized form (UF-SBR), carboxylated styrene-butadiene rubber (CSBR), in ultrafine fully vulcanized form (UF-CSBR), acrylic rubber (ACM), in ultrafine fully vulcanized form (UF-ACM), room temperature vulcanized silicone rubber (RTV), in ultrafine fully vulcanized form (UF-RTV) and polytetrafluoroethene (PTFE) in micro-rubber form (PTFE-M) were utilized for modifying 2,4,6-trinitrotoluene (TNT) based melt-cast explosives. Based on their dispersity in TNT and RDX slurry, only UF-NBR, UF-CNBR and PTFE-M can be used. In the modification experiment, their influence on the mechanical and detonation performance of the matrixes were studied, as well as the impact sensitivity. Compared with PTFE-M and UF-CNBR, UF-NBR improved the tensile and compressive strength of the original formulation CYCLOTOL-65/35. The toughening mechanism was also explained through interfacial interactions and fracture energy analysis. The predicted detonation properties of the modified formulations (detonation pressure variations from 26 to 28 GPa, detonation velocity variations from 7900 to 8100 m/s) are at the same energy level as CYCLOTOL-65/35. In addition, the drop hammer impact testing results confirm that the formulation containing UF-NBR is more sensitive than the one with UF-CNBR, with the same amount of additive.