EN
The investigation of surface modification of Egyptian calcium carbonate via polymers was achieved with simultaneous ultra-fine grinding. Attrition mill and planetary mill were used for wet and dry grinding, respectively. The parameters affecting the grinding were studied such as ball number, speed and grinding time. The rheological characteristics of the aqueous calcium carbonate suspensions were studied in the presence of different types of polymers. The results indicated that the mechanical force could clearly affect the modification characteristics of calcium carbonate due to its mechanochemical effects. The viscosity of calcium carbonate suspension depends on the volume percentage or weight percentage. The dispersing agent increases the solid concentration for a given particle fineness.
EN
El-Hudi gold deposit, located in the South Eastern Desert of Egypt, represent large vein- type gold occurrence. The representative sample revealed the abundance of quartz as main constituent with minor amounts of mineral impurities. Gold was detectable (12 g/t) as determined using atomic absorption. The petrographic study revealed that the gold grains ranged from 10-40 μm. The grain boundaries of quartz are highly stained with iron minerals as hematite and limonite. Sericite mineral is common in discrete gold-bearing veins. Eroded pyrite was detected with high alteration leaving only cubic-shaped cavities behind. Different techniques for gravity separation were used to separate gold from the quartz mineral. After crushing and grinding of the sample, shaking table was used to upgrade the coarser fractions while Falcon concentrator was employed to upgrade the fine fraction. The best concentrate was obtained through grinding the whole sample to less than 0.2 mm, followed by cleaning steps. The gold content is increased from 12 to 145 g/t with total recovery of 78%.
3
Content available remote Factorial design for column flotation of phosphate wastes.
EN
A factorial design was used to study effects, and their interactions, of the main parameters affecting column efficiency to recover phosphates from their wastes. Three-phase experiments were performed using a mixture of fatty acid and fuel oil as a collector for phosphate while pine oil was used as a frother. Meanwhile 2-phase experiments were conducted to correlate the results of 3-phase experiments with that of bubble diameter and air holdup. The result shown that application of statistical design reveals very interesting information about the interaction between the studied parameters. For example it is shown that the interaction (X1X2) between superficial gas velocity (X1) and frother concentration (X2) has a beneficial effect on grade but aversely affect recovery.
PL
Metoda planowania czynnikowego została zastosowana do opisania wpływu i współzależności między podstawowymi parametrami procesu flotacji kolumnowej zastosowanej do odzysku fosforytu z odpadów fosforytowych. Doświadczenia flotacyjne zostały przeprowadzone z wykorzystaniem kwasu olejowego i oleju napędowego jako kolektorów oraz oleju sosnowego jako spieniacza. Planowanie typu 23 zostało przeprowadzone w celu znalezienia korelacji między wynikami eksperymentu a średnicą pęcherzyków powietrza i parametrami procesu. Dla przykładu, zostało pokazane, że X1X2, czyli między prędkością przepływu gazu (X1) a stężeniem spieniacza (X2) na korzystny wpływ na wychód a niekorzystny wpływ na uzysk procesu flotacji.
4
Content available remote Carrier flotation of ultrafine Egyptian kaolin.
EN
This paper aims to study the amenability of application of the carrier flotation process for removing the anatase impurities, assocd. with the Egyptian kaolin pre-conc. (~80 wt.% below 2 mm) to be suitable for paper coating and fine ceramic industry. The tests were carried out using sodium silicate as a depressant and oleic acid as a collector. Limestone was used as a carrier in these tests. The size of the carrier as well as its quantity in the pulp were studied. The results showed that the size of the carrier played a major role in determining the efficiency of the carrier flotation process where a significant improvement in the grade of the concentrate was obtained by decreasing the carrier grain size. The TiO2% decreased to its min. content (0.6%), in comparison with 1.52% in the feed sample, with its lowest retention ratio when a carrier of grain size -25 + 10 mm was used. At such optimum carrier size the degree of whiteness reached its highest value (90) in comparison with 56 for the feed sample. At the same time, the quantity of the carrier flotation pulp had no greater influence on the grade of the product. The results showed also that the carrier flotation pulp had no greater influence on the grade of the product. The results showed also that the carrier flotation process can give a concentrate with TiO2% similar to that obtained with the conventional froth flotation technique in presence calcium acetate as an activator, yet the carrier flotation technique has the advantage of reducing the long conditioning time needed for the pulp with the reagents in the conventional technique. The flotation mechanism is discussed.
PL
Celem tej pracy jest określenie możliwości zastosowania flotacji nośnikowej do usuwania anatazu występującego w egipskich wstępnych koncentratach kaolinowych o uziernieniu ~80%ziarn poniżej 2um, aby koncentrat ten mógł być odpowiedni do produkcji papieru i ceramiki ozdobnej. W badaniach zastosowano krzemian sodu jako depresant i kwas olejowy jak kolektor. Jako nośnika użyto wapnia. Wyniki okazały, że rozmiar ziarn nośnika determinuje efektywność badanego procesu flotacji nośnikowej a znaczny wzrost jakości koncentratu otrzymano poprzez zmniejszenie rozmiaru ziarn nośnika. Zawartość procentowa TiO2 malała do minimum tj. do 0.6% w porównaniu do 1.52% w nadawie, gdy użyto nosnika o wymiarach ziarn nośnika. Zawartość procentowa TiO2 malała do minimum tj. do 0.6% w porównaniu do 1.52% w nadawie gdy użyto nośnika o wymiarach ziarn -25+ 10um. Przy optymalnym rozmiarze ziarn nośnika stopień białości kaolinu osiągał najwyższą wartość (90) w porównaniu do 56 dla nadawy. W tym samym czasie ilość nośnika we flotacji nie mialo wplywu na jakość produktu końcowego. Wyniki badań pokazały, że proces flotacji nośnikowej może dostarczyć koncentratów o zawartości TiO2 podobnej do zawartości w koncentratach otrzymywanych we flotacji pianowej w obecności octanu wapnia jako aktywatora ale flotacja nośnikowa ma tę przewagę, że redukuje długi czas agitacji pulpy z regentami przy wzbogacaniu konwencjonalnym. Przedyskutowano również mechanizm flotacji nośnikowej.