Content available remote SCC of cold-worked austenitic stainless steels in PWR conditions
EN
A strong susceptibility for SCC of heavily cold worked austenitic stainless steels is observed in hydrogenated primary water typical of PWRs. This susceptibility to cracking increases with the extent of cold-work and/or localization of deformation. The levels of cold-work involved in this study are very high when compared to the maximum cold-work levels required by the usual international codes relevant to PWRs (ASME and RCC-M). These high values of cold-work could be eventually encountered on the surface of same components (grinding) or in the case of improper manufacturing. The specific cold-work procedures including a compressive stage (fatigue, shot-peening) strongly favors SCC susceptibility in PWRs conditions under dynamic deformation. For a given cold-working procedure, SCC susceptibility of austenitic stainless steels materials increases with an increasing intensity of cold-work. A threshold of SCC susceptibility was identified in the ease of the shot-peening procedure of cold-working for AISI 304L stainless steels through the value of the initial surface hardness before SCC testing (CERT). SCC crack propagation is thus only observed beyond 300+-10HV on shot-peened specimens.
first rewind previous Strona / 1 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.