In the paper, verification of welding process parameters of overlap joints of aluminium alloys EN AW-6082 and EN AW-7075, determined on the grounds of a numerical FEM model and a mathematical model, is presented. A model was prepared in order to determine the range of process parameters, for that the risk of hot crack occurrence during welding the material with limited weldability (EN AW-7075) would be minimum and the joints will meet the quality criteria. Results of metallographic and mechanical examinations of overlap welded joints are presented. Indicated are different destruction mechanisms of overlap and butt joints, as well as significant differences in their tensile strength: 110 to 135 MPa for overlap joints and 258 MPa on average for butt joints.
This paper outlines issues associated with gas-shielded braze welding of CU-ETP copper with austenitic steel X5CrNi18-10(1.4301) using a consumable electrode. The possibilities for producing joints of this type using innovative low-energy welding methods are discussed. The paper provides an overview of the results of metallographic and mechanical (static shear test, microhardness) tests for braze welded joints made on an automated station using the Cold Metal Transfer (CMT) method. Significant differences in the structure and mechanical properties are indicated, resulting from the joint configuration and the type of shielding gas (argon, helium).
3
Dostęp do pełnego tekstu na zewnętrznej witrynie WWW
W artykule przedstawiono problematykę związaną z lutospawaniem łukowym elektrodą topliwą w osłonie gazów blach ze stopu aluminium 5754 z tytanem Grade 2. Omówiono możliwości wytwarzania tego rodzaju połączeń przy użyciu innowacyjnych niskoenergetycznych metod spawalniczych. Przedstawiono wyniki badań metalograficznych oraz mechanicznych (statycznej próby ścinania, pomiarów mikrotwardości) złączy lutospawanych wykonanych półautomatyczną metodą CMT (ang. Cold Metal Transfer).
EN
The article presents the problems related to arc welding-brazing hot-melt electrode in the gas shield of 5754 aluminum alloy sheets with titanium Grade 2. The possibilities of making such joints using innovative low-energy welding methods have been indicated. The results of metallographic and mechanical tests (static shear test, microhardness measurements) of weld brazed joints made by the semi-automatic CMT (Cold Metal Transfer) method have been presented.
4
Dostęp do pełnego tekstu na zewnętrznej witrynie WWW
The article presents issues related to the braze welding process, discusses primary methods applied in industry as well as indicates characteristic features of the process, discusses the structure of joints most commonly used in industry and advanced braze welding methods enabling the obtainment of joints satisfying strict quality requirements. In addition, the article assesses the possibility of using the braze welding technology when repairing casts made of various casting alloys, discusses application areas for braze welded joints of materials characterised by different mechanical and physicochemical properties as well as presents metallographic and mechanical test results concerning brazed welded joints made using a robotic CMT (Cold Metal Transfer) braze welding station.
PL
Przedstawiono problematykę związaną z procesem lutospawania i omówiono podstawowe metody stosowane powszechnie w przemyśle. Wskazano charakterystyczne cechy procesu, rodzaje najczęściej wytwarzanych w przemyśle złączy pod względem ich konstrukcji oraz nowoczesne metody lutospawania umożliwiające wykonanie złączy spełniających duże wymagania jakościowe. Oceniono możliwość zastosowania technologii lutospawania do naprawy odlewów wykonanych z różnych stopów odlewniczych. Omówiono obszary zastosowania złączy lutospawanych materiałów o zróżnicowanych właściwościach fizykochemicznych i mechanicznych. Przedstawiono wyniki badań metalograficznych oraz mechanicznych przykładowych złączy lutospawanych wykonanych na zrobotyzowanym stanowisku do lutospawania metodą CMT (Cold Metal Transfer).