Content available Thermophysical properties of 904L austenitic steel
EN
This paper presents the results of the structural investigations and thermophysical properties of 904L steel parent material. Experimental studies on the structure of 904L steel proved a pure austenitic structure. Both the experimental research and analysis of the thermophysical properties of 904L steel were complemented with the results of the thermal conductivity calculations for the tested material. The paper presents a brief description of the measurements, the procedures for evaluating the data, and a set of the obtained results.
PL
W pracy przedstawiono wyniki badań strukturalnych i właściwości cieplnofizyczne materiału rodzimego stali 904L. Badania eksperymentalne struktury stali 904L wykazały strukturę czysto austenityczną. Badania doświadczalne i analizę właściwości cieplnofizycznych stali 904L uzupełniono wynikami obliczeń przewodności cieplnej badanego materiału. W pracy przedstawiono zwięzły opis wykonywanych pomiarów, charakterystykę procedur opracowania danych oraz komplet uzyskanych wyników.
2
Content available remote Assessing the Susceptibility of Welded Joints to Cold Cracking in the CTS Test
EN
The article presents the CTS tests used when assessing the susceptibility of welded joints to cold cracking as well as test results related to steel 7CrMoVTiB10-10. The research work involved macro and microscopic metallographic tests performed using light and scanning electron microscopy. The macro and microscopic metallographic tests were used to assess the nature of cracking. It was demonstrated than an increase in thermal severity was accompanied by an increase in the average length of cold cracks.
PL
Przedstawiono charakterystykę próby CTS stosowanej do oceny skłonności złączy spawanych do pęknięć zimnych oraz wyniki prób dla stali 7CrMoVTiB10-10. Wykonano badania metalograficzne makroskopowe oraz mikroskopowe przy zastosowaniu mikroskopii świetlnej oraz skaningowej mikroskopii elektronowej. Na ich podstawie dokonano oceny charakteru pękania. Wykazano, że wzrost liczby ostrości cieplnej powoduje zwiększanie średniej długości powstałych pęknięć zimnych.
3
Content available remote A New Look at the Classification of Cracks in Welded and Braze Welded Joints
EN
The making of structures using advanced materials and joining technologies is frequently accompanied by limited weldability problems. The obtainability of joints characterised by required properties can be limited, among other things, by susceptibility to crack formation. The article presents an overview of classification of cracks in welded and braze welded joints based on reasons for crack formation and the period of crack development. The primary division of fabrication/production-related cracks includes hot, cold, lamellar and annealing cracks. The study recommends the extension of the above-presented classification by including cracks occurring at a temperature higher than ambient temperature and lower than the lower limit of high-temperature brittleness range. The above-named temperature range could include cracks triggered by the loss of plasticity in the solid state resulting from the occurrence of ductility-dip brittleness and cracks related to liquid metal embrittlement.
PL
Wytwarzanie konstrukcji z użyciem nowoczesnych materiałów i technologii łączenia nierzadko niesie za sobą problemy związane z ich ograniczoną spawalnością. Zdolność do otrzymywania złączy o wymaganych własnościach może być ograniczona m.in. przez skłonność do występowania pęknięć. W pracy dokonano przeglądu sposobów klasyfikacji pęknięć złączy spawanych i lutospawanych opartych na przyczynach i okresie ich powstawania. Jako podstawowy podział pęknięć związanych z produkcją/wytwarzaniem przyjęto pęknięcia gorące, zimne, lamelarne oraz wyżarzeniowe. Zaproponowano rozszerzenie tej klasyfikacji o szczególne przypadki pęknięć występujących w temperaturze wyższej od temperatury otoczenia i niższej od dolnej granicy zakresu kruchości wysokotemperaturowej. W powstałym w ten sposób przedziale temperatury mogą wystąpić pęknięcia spowodowane utratą plastyczności w stanie stałym na skutek wystąpienia kruchości wysokotemperaturowej II rodzaju oraz pęknięcia spowodowane kruchością w obecności ciekłych metali.
4
Content available remote Structure and properties of welded joints of 7CrMoVTiB10-10 (T24) steel
EN
Gas Tungsten Arc butt welded joints of tubes of 7CrMoVTiB10-10 made using bainitic-martensitic P 24-IG filler metal were found to be susceptible to root cracking. This was avoided by using the CMS-IG filler metal and austenitic EPRI P87 filler metal. Detailed coefficient of thermal expansion analysis for both filler metals was performed. Unfortunately, CMS-IG filler metal is characterized by a lower creep rupture strength than P 24-IG. For this reason, the joints were produced by the 141 method with using two filler metals: P 24- IG and EPRI P87. All the welded joints was characterized by the B quality level. Macrostructural, microstructural and hardness data for both welded joints are presented. The standard requirement, < 350 HV10, was marginally not met and was achieved through post weld heat treatment.
PL
W artykule przedstawiono charakterystykę stali konstrukcyjnych o podwyższonej i wysokiej wytrzymałości. Omówiono mechanizmy umocnienia stali zapewniające korzystne właciwości mechaniczne. Przedstawiono wyniki badania mikrostruktury złączy doczołowych stali o gwarantowanej granicy plastyczności 1300 MPa wykonanych wiązką lasera bez materiału dodatkowego. W celu scharakteryzowania struktury przeprowadzono badania wizualne, makro- i mikroskopowe oraz pomiary twardości w przekroju poprzecznym złącza.
EN
The paper presents characterization ot structural high-strength steels and the fundamentais of steel strengthening and hardening to guarantee good mechanical properties. Moreover, the microstructure evaluation of laser beam butt welded joints of steel with yield strength 1300 MPa were carried out and the results were presented. In research the visual testing, macro- and microscopic analysis and hardness measurement were carried out.
PL
W artykule przedstawiono badania za pomocą mikroskopu świetlnego i skaningowego mikrostruktury odlewniczego stopu niklu umacnianego wydzieleniowo fazą międzymetaliczną Ni3(Al,Ti) po spawaniu metodą GTAW. Ujawniono, iż w rdzeniach dendrytów występują głównie pierwotne i wtórne wydzielenia fazy γ’ w osnowie γ, natomiast w obszarach międzydendrytycznych obserwowano eutektykę γ/γ’ oraz węgliki typu MC. Stosunkowo duże różnice mikrostruktury w tych dwóch charakterystycznych obszarach materiału rodzimego świadczą o dużej lokalnej niejednorodności. Podczas obserwacji za pomocą SEM po spawaniu zauważono mikropęknięcia gorące w strefie wpływu ciepła (SWC). Stwierdzono, że ciecz w SWC podczas spawania pojawia się w wyniku nierównowagowego nadtapiania fazy umacniającej γ’. Analiza przełomu autogenicznego połączenia ujawniła w materiale rodzimym złożony charakter pęknięcia. Kruchy charakter pęknięcia obserwowano na wydzieleniach fazy γ’, eutektyki γ/γ’ i węglików, natomiast ciągliwy w osnowie γ. W strefie wpływu ciepła ujawniono pęknięcie likwacyjne o charakterystycznej powierzchni swobodnej.
EN
Paper presents microstructural investigation using light and scanning electron microscopy of cast nickel based superalloy with trade name Rene 108 after Gas Tungsten Arc Welding. Analysis of base metal revealed that inside dendrite cores are mainly primary and secondary γ› precipitations, while constituents in interdendritic spaces are eutectic γ/γ› and MC-type carbides. Substantial differences in those two regions indicate on relatively high local inhomogeneities. SEM investigation showed microfissuring in heat affected zone. It was found that during welding liquid was created in HAZ via constitutional liquation of intermetallic γ› phase. SEM analysis of fracture revealed brittle failure of γ› phase, eutectic islands γ/γ› and MC-type carbides, in turn plastic deformation of γ-matrix. In heat affected zone the free surface of liquation crack was observed.
EN
The aim of the present study was to characterize the repair weld of serviced (aged) solid-solution Ni-Cr-Fe-Mo alloy: Hastelloy X. The repair welding of a gas turbine part was carried out using Gas Tungsten Arc Welding (GTAW), the same process as for new parts. Light microscopy, scanning electron microscopy, transmission electron microscopy, microhardness measurements were the techniques used to determine the post repair condition of the alloy. Compared to the solution state, an increased amount of M6C carbide was detected, but M23C6 carbides, sigma and mu phases were not. The aged condition corresponds to higher hardness, but without brittle regions that could initiate cracking.
PL
W artykule przedstawiono próbę implantacyjną oceny skłonności do pęknięć zimnych złączy spawanych. Przedstawiono również wyniki próby dla stali 7CrMoVTiB10-10 oraz badania w zakresie oceny charakteru przełomu.
EN
The paper presents the implant test method as useful for susceptibility to cold cracking evaluation of welded joints. Moreover, there are presented results of implant test for 7CrMoTiVB10-10 steel and fractures analyses with the use of light microscopy and scanning electron microscopy.
9
Content available remote Badania skłonności do pęknięć gorących metodą Blanchet’a
PL
W artykule przedstawiono wyniki oceny skłonności do pęknięć gorących dwóch stopów niklu 600 i 617. Próby przeprowadzono na blachach cienkich (1 mm) wykorzystując metodę Blanchet’a. Uzyskane wyniki wskazują na skłonność badanych materiałów do pęknięć gorących przy określonym stopniu odkształceń i naprężeń. Pęknięcia zlokalizowane są w obszarze stało-ciekłym. Nie zaobserwowano ich występowania w dalszej części spoiny.
EN
The paper shows the results of hot crack susceptibility tests of 600 and 617 nickel alloys. The thin plates (1 mm) in the Blanchet method were used for tests. The increase of hot crack susceptibility of tested alloys with strain and stress is obtained in the mushy zone (S+L). In the other areas of weld metal the cracks were not observed.
PL
W artykule przedstawiono wyniki oceny skłonności do pęknięć gorących dwóch stopów niklu 600 i 617. Próby przeprowadzono na blachach cienkich (1 mm), wykorzystując metodę Blanchet’a i grubych (5 mm) metodą Transvarestraint. Uzyskane wyniki wskazują na skłonność badanych materiałów do pęknięć gorących przy określonym stopniu odkształceń i naprężeń. Pęknięcia zlokalizowane są w obszarze stało-ciekłym. Nie zaobserwowano ich występowania w dalszej części spoiny.
EN
The paper shows the results of hot crack susceptibility tests of 600 and 617 nickel alloys. The thin plates (1 mm) in the Blanchet method and thick (5 mm) in the Transvarestraint method is used for tests. The increase of hot crack susceptibility of tested alloys with strain and stress is obtained in the mushy zone (S+L). In the other areas of weld metal the cracks were not observed.
11
PL
Przedstawiono wyniki oceny mikrostruktury stopów niklu 600 i 617. Badane stopy w formie blach poddano działaniu łuku elektrycznego w metodzie TIG. Ocenie poddano mikrostrukturę obszaru wtopienia, strefy wpływu ciepła i materiału rodzimego przy wykorzystaniu mikroskopii świetlnej i skaningowej mikroskopii elektronowej. Wykonane badania ujawniły duże różnice w budowie strukturalnej obszaru wtopienia stopu 600 i 617 wynikającą z różnic składu chemicznego i występowania znacznej segregacji pierwiastków stopowych pomiędzy dendrytami i obszarami międzydendrytycznymi.
EN
The paper presents the results concerning the assessment of the microstructure 600 and 617 nickel alloys. Test alloys delivered as plates were exposed to welding arc applied in the TIG method. The assessment involving the microstructure of the fusion zone, heat affected zone and of the base material was performed using light microscopy and scanning electron microscopy. The results revealed significant differences in the structures of the fusion zone in 600 and 617 alloys resulting from various chemical compositions as well as from the significant segregation of the alloying elements between dendrites and interdendritic zones.
12
EN
The paper presents the some aspects of the optimization of filler metals consumption in the production of welded steel structures. Correct choice of beveling method can allow to decrease cost of production and increase quality. The review of calculation methods of filler metal consumption at the design stage was carried out. Moreover, the practical examples of amount of filler metals calculation were presented and analyzed. The article also contain examples of mobile apps which are makes it easy to see welding costs in just a few seconds. Apps as well as simple excel spreadsheets with correct mathematic equations allows to optimize welding process.
EN
The aim of the study was to determine the possibility of joining dissimilar joints of zinc coated E275D and X5CrNi18-10 steels by braze welding process. The experiment was performed by the Puls-Arc method with argon as the shielding gas. The process was carried out using a Lincoln Electric Power Wave S500 welding device. Joints was carried out in two variants: without treatments before braze welding, and when the zinc coating was removed by mechanical means. Macro- and micro metallographic examinations and an analysis of mechanical properties of joints based on Vickers hardness distribution were carried out. The average hardness of the welds is 99 HV10. No effect on hardness of the removal of the zinc coating before braze welding was observed. For welds in the presence of a liquid metal, LME (Liquid Metal Embrittlement) cracks were observed. The results may be useful in the design of dissimilar materials joining technology using braze welding method.
PL
Celem badań było określenie możliwości łączenia złączy różnoimiennych z ocynkowanej stali E275D i stali X5CrNi18-10 metodą lutospawania. Eksperyment wykonano łukiem pulsującym w osłonie argonu. Proces przeprowadzono na urządzeniu Power Wave S500 firmy Lincoln Electric. Złącza wykonywano w warunkach bez dodatkowych zabiegów przed procesem i gdy w miejscu złącza usunięto warstwę cynku w sposób mechaniczny. Zaprezentowano wyniki badań makro- i mikroskopowych złączy oraz analizę ich właściwości mechanicznych wykonaną w oparciu o rozkład twardości w złączu. Pomiary prowadzono sposobem Vickersa. Średnia twardość w złączu wynosi 100 HV10. Nie stwierdzono wpływu usuwania powłoki cynkowej na twardość w złączach. W złączach zaobserwowano pęknięcia spowodowane kruchością w obecności ciekłych metali. Uzyskane wyniki mogą być przydatne podczas projektowania technologii łączenia materiałów różnoimiennych przy użyciu metody lutospawania.
14
EN
The aim of this study was to present the hot cracking behavior of a blade originating from a turbine blade segment. The crack was induced by a gas tungsten arc welding process, and the research material was a MAR-M247 nickel based superalloy. This alloy is considered to be difficult to weld because of its high tendency to crack. Light microscopy and scanning electron microscopy show the occurrence of cracking in the melted zone, heat-affected zone, and base alloy. A scanning electron microscopy investigation revealed that cracks are propagated by stresses and liquation of the low temperature constituent.
PL
Celem pracy była analiza mikrostrukturalna pęknięcia gorącego na powierzchni łopatki z segmentu van cluster. Pęknięcie powstało w wyniku oddziaływania skoncentrowanego źródła ciepła, jakim był łuk elektryczny jarzący się w osłonie argonu. Łopatka została wykonana z nadstopu na osnowie niklu o nazwie handlowej MAR-M247. W przypadku konwencjonalnych metod spawania jest on uważany za trudno spawalny. Przeprowadzono badania makrostruktury i mikrostruktury za pomocą mikroskopii świetlnej i skaningowej. Na podstawie wykonanych badań stwierdzono występowanie pęknięć ciągłych zarówno w obszarze przetopionym, strefie wpływu ciepła, jak i materiale rodzimym. Obserwacje za pomocą skaningowej mikroskopii elektronowej pozwoliły na stwierdzenie, że pęknięcie propagowało w wyniku naprężeń, jak również likwacji niskotopliwych składników mikrostruktury.
PL
W artykule przedstawiono wyniki badań mikrostruktury i odporności na korozję wżerową w środowisku chlorków doczołowych złączy jedno- i różnorodnych w stanie bez pasywacji i po pasywacji żelem i taśmą trawiąco-pasywującą. Badania przeprowadzono na złączach austenitycznych stali nierdzewnej i żaroodpornej. Wyniki oceny mikrostruktury ujawniły komórkowo-dendrytyczny charakter krzepnięcia spoiny. W spoinie i strefie wpływu ciepła (SWC) przy linii wtopienia obserwowana jest siatka ferrytu w stalach nierdzewnych. Obszarem szczególnie wrażliwym na korozję wżerową jest obszar spoiny i SWC przy linii wtopienia, gdzie obserwowano występowanie pojedynczych, dużych i stosunkowo głębokich wżerów bez względu na sposób zabezpieczenia powierzchni. Stal żaroodporna wykazała odporność na korozję wżerową w środowisku chlorków.
EN
The paper presents the microstructure and pitting corrosion resistance in chloride environment susceptibility of non-passivated and passivated similar and dissimilar butt-welded joints. Testing was carried out with the use of stainless steels joints. The microstructure evaluation showed the dendrite solidification character of the weld metal. In those area and also in the heat affected zone (HAZ) next to fusion zone the ferrite is observed. The high sensitivity area for pitting corrosion is weld metal and HAZ next to fusion zone, where the deep pitting is observed, The surface protection method is not improving the corrosion resistance in chloride environment.
16
Content available remote Ocena mikrostruktury wybranych stopów niklu
PL
W pracy przedstawiono wyniki oceny mikrostruktury wybranych stopów niklu, tzn. 600, 617 i 625. Stosując mikroskopię świetlną poddano ocenie obserwowane mikrostruktury w odniesieniu do ich składu chemicznego. Przedstawiono również typowe mechanizmy utwardzania występujące w stopach niklu.
EN
The paper presents the results of selected nickel base alloys assessment - 600, 617 and 625. Using light microscopy observed microstructure were comparised with chemical composition of tested alloys. The typical for nickel base alloys strengthening mechanisms are presented.
PL
Przedstawiono wyniki obserwacji wizualnych, badań makro- i mikroskopowych oraz pomiarów twardości złączy doczołowych blach ze stali 7CrMoVTiB10-10 (T24). Złącza spawane wykonano łukiem krytym, wiązką laserową i metodą hybrydową (wiązka laserowa + spawanie łukowe elektrodą topliwą w osłonie gazów). Obserwacje wizualne pozwoliły na ujawnienie nielicznych niezgodności spawalniczych, których obecność została potwierdzona w badaniach makroskopowych. Badania mikroskopowe nie wykazały istotnego wpływu technologii spawania na mikrostrukturę SWC, natomiast spoiny uzyskane w poszczególnych procesach charakteryzowały się zróżnicowaną mikrostrukturą, determinowaną m.in. szybkością odprowadzania ciepła. Pomiary twardości wykazały, iż niezależnie od zastosowanej technologii maksymalna wartość twardości przekracza 350 HV10.
EN
The paper presents the results of visual observation, macro- and microscopic examination and hardness testing of butt-welded joints of 7CrMoVTiB10-10 steel. Welded joints was made by Submerged Arc Welding, Laser Beam Welding and a hybrid method (Laser Beam Welding + Gas Metal Arc Welding). Visual observation shown the presence of a few imperfections, what confirmed the macroscopic examination. Microscopic examination shown no significant effect of welding processes in the HAZ microstructure, while weld metal obtained by different processes is characterized by varied microstructure, that is determined i.e. heat removal rate. Hardness measurement shown that maximum hardness value exceed 350 HV10, regardless of welding process.
PL
W pracy przedstawiono właściwości i strukturę połączenia spawanego pomiędzy elementem ze stali eksploatowanej 14 MoV6-3 oraz elementem nowym, nieeksploatowanym, również ze stali 14 MoV6-3. Oba elementy w postaci płyt o wymiarach 110x220x20 mm połączono dwoma metodami spawania łukowego. Grań spoiny wykonano metodą spawania elektrodą nietopliwą w osłonie gazu obojętnego (TIG), natomiast wypełnienie metodą spawania elektrodą otuloną (MMAW). Pospawany element został poddany wyżarzaniu odprężającemu. Powstałe złącze spawane zostało poddane badaniom nieniszczącym: VT, PT, RT oraz badaniom niszczącym: badaniu udarności, rozciąganiu złącza, badaniom metalograficznym oraz badaniu rozkładu twardości w złączu. W wyniku badań ustalono, iż istnieje możliwość wykorzystania zastosowanych metod spawania do wykonywania remontów lub modernizacji instalacji energetycznych.
EN
The paper presents the structure and properties of the weld joint between the operated steel 14MoV6-3 and a new, non-operated steel 14MoV6-3 element. Both elements in the form of plates of dimensions 110 x 220 x 20 mm were joined by two methods of arc welding. Ridge welds made by welding tungsten inert shielding gas TIG, while filling was made by welding with coated electrode MMAW. Welded item has been heat treated stress-relief annealing. The resulting joint has been subjected to non-destructive testing: VT, PT, RT and destructive testing: impact test, tensile joints, metallographic examination and testing of hardness distribution in the joint. The research found that there is a possibility to use the methods of welding for repair or upgrading of power plants structures.
EN
The article presents the results concerning hot crack susceptibility of selected steels having an austenitic structure. The tests were based on the analysis of the chemical composition of these steels and utilising special stations for the Transvarestraint tests and the Blanchet method. During the tests it was possible to observe cracks in the liquid-solid area. The results obtained indicate the existence of an area free from solidification cracks for a certain strain value at a pre-set welding rate. It was also possible to observe the absence of a distinct boundary between such areas, which was reflected in the crack length.
PL
W artykule przedstawiono wyniki oceny skłonności do pęknięć gorących wybranych stali o strukturze austenitycznej. Badania przeprowadzono w oparciu o analizę składu chemicznego tych stali oraz wykorzystując specjalne stanowiska dla próby Transvarestraint i metody Blancheta. Obserwowano występowanie pęknięć w obszarze ciekło stałym. Uzyskane wyniki wskazują na istnienie obszaru, gdzie przy pewnej wartości odkształcenia przy zadanej prędkości spawania, nie ma pęknięć krystalizacyjnych oraz obszaru ich występowania. Stwierdzono, że nie istnieje wyraźna granica pomiędzy tymi obszarami, co znajduje odzwierciedlenie w długości pęknięcia.
EN
The article presents the microstructure and properties of dissimilar welded joints of pipes made of the 304HCu (X10CrNiCuNb18-9-3) and P92 (X10CrWMoVNb9-2) steels in the as welded state and after PWHT. The test-related TIG welding was carried out using two filler metals in the form of the Thermanit 304HCu and the EPRI P87 filler metal wires. The tests revealed the significant influence of heat treatment time extension on the decrease in the hardness of the martensitic steel and its HAZ as well as an on the increase in the hardness of the austenitic steel, its HAZ and of the weld made using the Thermanit 304HCu filler metal. The microscopic observations revealed the presence of a carburised zone on the fusion line between the P92 steel and the weld made using the Thermanit 304HCu filler metal wire.
PL
W artykule przedstawiono mikrostrukturę oraz własności połączeń różnoimiennych rur ze stali 304HCu (X10CrNiCuNb18-9-3) i P92 (X10CrWMoVNb9-2) w stanie surowym po spawaniu oraz po obróbce cieplnej. Do spawania metodą TIG wykorzystano dwa materiały dodatkowe – drut Thermanit 304HCu oraz drut EPRI P87. Badania wykazały istotny wpływ wydłużenia czasu obróbki cieplnej na obniżenie twardości stali martenzytycznej i jej SWC oraz wzrost twardości stali austenitycznej, jej SWC i spoiny wykonanej spoiwem Thermanit 304HCu. Obserwacje mikroskopowe ujawniły występowanie strefy nawęglonej na linii wtopienia pomiędzy stalą P92 a spoiną utworzoną przy użyciu drutu Thermanit 304HCu.
first rewind previous Strona / 2 next fast forward last