The article presents results of studies on metal resistance to erosive damage taking place under the influence of hydraulic cavitation. On the basis of earlier research, a hypothesis on fatigue character of erosive wear and a dependence of metal resistance to erosive damage on its crystalline lattice structure has been assumed. To verify this hypothesis, metals with different crystalline lattice structures like steel 45 (flat-centred structure), nickel 200/201 and nickel alloy Monel 400 (hexagonal structure) have been tested at a cavitation-strike stand. Results obtained there confirmed the assumed hypothesis, at the same time justifying the use of nickel protective coatings in fluid-flow machines.
PL
W artykule przedstawiono wyniki badań odporności metali na uszkodzenia erozyjne zachodzące pod wpływem kawitacji hydraulicznej. Na podstawie wyników wcześniejszych badań, przyjęto hipotezę o zmęczeniowym charakterze zużycia erozyjnego oraz zależności odporności metali na zniszczenia erozyjne od struktury ich sieci krystalicznej. Dla potwierdzenia przyjętej hipotezy na stanowisku kawitacyjno-udarowym sprawdzono metale z różnymi sieciami krystalicznymi: stal 45 (sieć płasko centralna), nikiel 200/201 oraz stop niklu Monel 400 (sieć heksagonalna). Otrzymane wyniki badań potwierdziły przyjętą hipotezę, wskazując tym samym na zasadność stosowania niklowych powłok ochronnych w maszynach przepływowych.
first rewind previous Strona / 1 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.