Purpose: of this paper is the verification of multi-layer SAW welding the raw material “1.6946” by different welding consumables (TOPCORE 838 B, Thermatit MTS 616) in the „ultra” narrow gap using the prescribed temperature cycle and subsequent heat treatment. Design/methodology/approach: An evaluation of the mechanical properties of the test for both types welding consumables. The measured values of yield strength and the tensile strength exhibit comparable properties to the RAW material “Inspection Certificate” for welding consumable “TOPCORE 838 B”. Findings: Thermatit MTS 616” was found falling below the specified values of impact energy, ductility. The welding consumable TOPCORE 838 B shows less susceptibility to the brittleness. Based on the results will be verified by the existence of internal structures arising using the microstructure analysis & ARA diagram of the base material 1.6496. Research limitations/implications: Obtained results will be subsequently verified the existence of internal generated microstructures using the ARA chart of the base material (W Nr. 1.6496) for the future design of the new temperature cycles in all phases of the production. Originality/value: The welding consumable “TOPCORE 838 B” showed the low tendency to embrittlement in the heat-affected zone using the defined heat treatment. On the basic of the examination the welding consumable “TOPCORE 838 B” can be recommended to be used for the welding process, thermal cycle and heat treatment.
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.