Content available remote The formation of zinc coatings in nanocrystallised zinc powders
EN
The kinetics of and mechanism for galvanising low-carbon steel (0.2% C) were examined in powder media which were pre-treated to obtain a fine nanostructured ZnO layer on the surface of zinc powder particles. The effective diffusion coefficient of Zn atoms through the ZnO shell was estimated to be in the order of 1·10ˉ¹º m²·s­­­­­ˉ¹. The contribution of the Zn-gas evaporation/condensation microprocesses, which could occur in relation to the above diffusion through a nanostructured surface layer, was evaluated with numerical calculations in the temperature range of 550–950 K and for an average particle size of ZnO up to 100 nm. Our results suggest that the outward diffusion of metallic zinc takes place from the core of powder microparticles across the nano-grain boundaries of their modified surface layer, and can be further intensified by the presence of other inter-phase defects, such as nano porosity.
2
Content available remote Wpływ modyfikacji bentonitu na jego właściwości adsorpcyjne
PL
Przeprowadzono kwaśną aktywację bentonitu za pomocą kwasu solnego, uzyskując wzrost powierzchni właściwej BET adsorbentu o 228 p.p. Zmianie uległy również inne parametry powierzchniowe, takie jak średnica i objętość porów, a także powierzchnia i objętość mikroporów. Impregnacja bentonitu nanometrycznym tlenkiem cyrkonu(IV) nie przyniosła zamierzonych efektów i przyczyniła się do pogorszenia właściwości adsorpcyjnych bentonitu. Efektywność adsorpcji określano, przeprowadzając testy adsorpcji siarkowodoru w warunkach beztlenowych. Skuteczność impregnacji bentonitu oceniano na podstawie obrazów powierzchni adsorbentów, wykonanych za pomocą skaningowego mikroskopu elektronowego (SEM).
EN
Com. bentonite was activated with HCl soln. to increase its sp. surface area by 228 percentage points (p.p.). Changes of diam., pore volume, as well as area and volume of micropores were also obsd. The impregnation of bentonite with nanometric ZrO₂ resulted in deterioration of the adsorption capacity of bentonite. The bentonite adsorbents were used for removal of H₂S from biogas under anaerobic conditions. The ZrO₂ modified bentonite was less efficient than the HCl-activated one, where 99% removal H₂S from N₂ stream was achieved.
PL
Metodą SEM/EDS określono skład jakościowy odpadów pochodzących z oczyszczania ulic Krakowa. Odpady analizowano pod kątem frakcji organicznej i mineralnej oraz metali ciężkich. Stwierdzono obecność Zn, Mg, Cu, Ni, Cd, Pb i Cr.
EN
Street cleaning waste was analyzed for org. and mineral fractions and for heavy metals by SEM/EDS methods. The presence of Zn, Mg, Cu, Ni, Cd, Pb and Cr was evidenced.
EN
In this work the analysis of corrosion for ductile iron pipes with diameters of 350 and 500 mm was performed. Two phenomena regarding the pipes coating deterioration have been recognized: corrosion and abrasion. The corrosion tests performed on different coatings in a neutral salt spray for up to 1000 hours indicate that this method is applicable for a rough external surface of centrifugally casted ductile iron pipes. The abrasion tests have been performed manually, using a grinding paper 1000#, due to an irregular profile of the external pipe surface transferred from the casting mold. It helped to obtain “spotted” sections, which were further microscopically analyzed (layer-by-layer). The last procedure, however not standardized, could be in some regards more convenient comparing to traditional cross-sections.
PL
W pracy dokonano analizy korozji rur z żeliwa sferoidalnego o średnicach 350 i 500 mm. Wykryto dwa zjawiska związane z pogorszeniem się powłoki rur: korozja i ścieranie. Testy korozyjne przeprowadzone na różnych powłokach w neutralnej mgle solnej przez okres do 1000 godzin wskazują, że metoda ta ma zastosowanie do szorstkiej zewnętrznej powierzchni odlewanych wirowo rur z żeliwa sferoidalnego. Testy na ścieranie przeprowadzono ręcznie przy użyciu papieru ściernego 1000 #, ze względu na nieregularny profil zewnętrznej powierzchni rury przeniesionej z formy odlewniczej. Pomogło to w uzyskaniu „plamkowych” przekrojów, które poddano dalszej analizie mikroskopowej (warstwa po warstwie). Ostatnia procedura, choć nie znormalizowana, może być pod pewnymi względami wygodniejsza w porównaniu do tradycyjnych przekrojów poprzecznych.