EN
Yttria stabilized zirconia powders were synthesized by the reverse microemulsion method. Powders were calcined from 600 °C to 1000 °C and sintered at 1450 °C. Crystalline properties and microstructure of samples were characterized by X-ray diffraction and scanning electron microscopy, respectively. Oxygen ionic conductivity was measured by electrochemical impedance spectroscopy. Sizes of yttria stabilized zirconia particles calcined at 1000 °C are lower than 100 nm, and approximately, 1 žm grain was obtained after sintering at 1450 °C.