The present study modelled the effects of operational parameters on the performance of the Falcon concentrator. For this purpose, the Falcon L40 concentrator was tested in narrow particle-size fractions (−600 + 425 μm, −425 + 300 μm, −300 + 212 μm, −212 + 150 μm, −150 + 106 μm, and −106 + 75 μm) at different washing water pressures and artificial gravity forces generated by a spinning bowl. The test samples were prepared artificially, comprising 2% magnetite (Fe3O4) and 98% calcite (CaCO3) by weight. The recovery and grade values of the 60 experimental conditions were investigated and compared for different operational parameters, including particle-size distributions, water pressures, and artificial gravity forces. Two empirical models were developed using non-linear regression analysis to indicate the effects of the operating parameter of the Falcon concentrator on its recovery and grade values. The operational parameters were found to impact the separation performance considerably. Therefore, the Falcon concentrator should operate under optimum conditions, which can be easily predicted using these models, to achieve improved recovery and grade values.
EN
This investigation is concerned with the extraction of nugget copper particles from copper recovery plant slag which recycled of copper scrap. For this purpose, the Falcon concentrator was used because of its enhanced gravity properties. The Falcon concentrator has a fast spinning bowl which creates a centrifugal force to separate fine size minerals on the basis of their density differences. In the tests, the tailings of the copper recovery plant were used and the test sample was divided into two groups and one of them was classified in narrow particle sizes. The operational parameters were determined as particle size, centrifugal force and washing water pressures. The water pressure and centrifugal force have an inversely proportional relationship. Because of this phenomenon, the G/P parameter was created. The test conditions were applied to the whole distribution sample and narrow size distribution samples in the same way. The test results indicate that the average grade was elevated from 1.04% to 6.50% with the recovery of 15.07% and 619% enrichment ratio for narrow sizes, whereas grade was elevated to 4.36% with 13.24% recovery and 415.94% enrichment ratio for the whole distribution. As a result, the recovery and grade values of concentrates are not good enough for gravity concentration process for both samples. However, this process was applied to the double recycled material and the lower recovery, grade values can be tolerated because of concentrate is nugget copper metal. The concentrate can also be washed in cleaning table for increasing the grade value for adding to initial feed of plant. This process can, therefore, supply important earnings not only economically but also environmentally.
PL
Badanie dotyczy ekstrakcji rodzimych cząstek miedzi z żużlu z zakładów recyklingu. W tym celu zastosowano wzbogacalnik Falcon ze względu na jego zwiększone właściwości wzbogacania grawitacyjnego. Wzbogacalnik Falcon ma szybko obracającą się misę, w której wytwarzana siła odśrodkowa powoduje rozdział minerałów o niewielkich wymiarach cząstek w zależności od ich różnych gęstości. W testach wykorzystano odpady z instalacji odzysku miedzi, a próbkę podzielono na dwie grupy, jedną z nich zaklasyfikowano do klasy cząstek o niewielkich wymiarach. Parametry technologiczne zostały określone i są to: wielkość cząstek, siła odśrodkowa i ciśnienia wody płukającej. Ciśnienie wody (P) i siła odśrodkowa grawitacji (G) charakteryzują się zależnością odwrotnie proporcjonalną. Z powodu tego zjawiska został utworzony parametr G/P. Zastosowano takie same warunki testu do rozdzielonych próbek o niewielkich wymiarach cząstek. Wyniki wskazują, że średnia ocena została podwyższona z 1,04 do 6,50% przy odzysku 15,07% i stopniu wzbogacania 619%. Dla cząstek niewielkich wymiarów ocena została podniesiona do 4,36% przy odzysku 13,24% i stopniu wzbogacania 415,94% dla całej dystrybucji. W rezultacie odzyski i wartości stopni wzbogacania koncentratów nie są wystarczająco dobre dla procesu wzbogacania grawitacyjnego dla obu próbek. Jednak proces ten został zastosowany do materiału z podwójnego recyklingu, a niższy poziom odzysku i stopnie wzbogacania mogą być akceptowane, ponieważ koncentrat stanowi rodzima miedź. Koncentrat może być również wzbogacany na stole koncentracyjnym w celu zwiększenia wartości stopnia wzbogacania do dodania do nadawy na zakład przeróbczy. W ten sposób proces ten może przynieść istotne zyski nie tylko w wymiarze ekonomicznym, ale także środowiskowym.