Preferencje help
Widoczny [Schowaj] Abstrakt
Liczba wyników
Powiadomienia systemowe
  • Sesja wygasła!
  • Sesja wygasła!

Znaleziono wyników: 17

Liczba wyników na stronie
first rewind previous Strona / 1 next fast forward last
Wyniki wyszukiwania
Wyszukiwano:
w słowach kluczowych:  zużycie materiału
help Sortuj według:

help Ogranicz wyniki do:
first rewind previous Strona / 1 next fast forward last
PL
W niniejszym artykule dokonano analizy oddziaływania wyrobów i obiektów budowlanych na środowisko naturalne w pełnym cyklu istnienia. Do przeprowadzenia analizy użyto programu komputerowego o nazwie SimaPro w wersji 7.1 holenderskiej firmy Pre Consultants wraz z dołączonymi bazami danych.
EN
The herein article carries out an analysis of impact the buildings and building products have on the natural environment, within the whole length of their lives. In order to carry out the analysis. Pre Consultants SimaPro 7.1 software has been used, along with the attached databases.
RU
V stat’e rassmotreny voprosy rascetnogo obosnovania racional’nych geometriceskich parametrov kombinirovannych metalliceskich konstrukcij s ponizennoj energoemkost’u za scet minimizacii raschoda metalla.
EN
The paper deals with the design of rational justification of the geometric parameters of combined metal structures with lower energy capaсity due to minimization of material consumption.
3
Content available remote Degradacja olejów smarowych
PL
Zjawisko tarcia towarzyszy nam na każdym kroku, zarówno w życiu codziennym, jak i podczas pracy w zakładach przemysłowych. Oprócz pozytywnych aspektów tarcia występują również te niepożądane. Jednym z nich jest zużycie, czyli strata materiału wywołana tarciem.
EN
Starting from the well-known fact that the rolling movement always has a lower friction compared to sliding friction, the authors have conceived and realized a pivoting movement joint on a “layer of balls” with “compensation space”, placed between the acetabular cup and the femoral head. This technical solution allows free self-directed migration of the balls, depending on the resistance opposed, with successive occupation of the “compensation space”. As a concept, the proposed technical solution excludes the existence of a cage for maintaining the relative positions of the spheres. It can be observed that the smallest values of the force and of the friction coefficient are obtained for the prostheses with balls and self-directed movement (approximately 5 times smaller than the values obtained for a classical prosthesis). For all the couples tested, the friction force grows with the growth of the normal load and of the oscillation speed. Changing the contact mechanism for the artificial hip joint from one sliding contact between two large surfaces, to a multitude of rolling contacts, could lead to some problems regarding functionality and durability of the active prosthesis elements. The key to an accurate evaluation of damaging mechanisms acting on THP with self directed rolling balls is a clear and complete picture of the load transfer mechanism.
PL
Przedstawiono konstrukcję dwóch sprężonych wiaduktów o przekroju skrzynkowym (długości 300,0 i 750,0 m). Oceniono wpływ technologii budowy przęseł tych wiaduktów na zużycie materiałów i inne parametry charakteryzujące ich budowę.
EN
Two long prestressed concrete box viaducts (300.00 m and 750.00 m), included in the Wroclaw Ring Road, are presented in this paper. The structures are similar in form but differ in terms of architectural features as well as in applied construction technologies, discussed and compared herein. The paper presents technological assumptions and conclusion drawn from the comparison of the technologies.
PL
Poniższa praca przedstawia opis koncepcji numerycznej symulacji procesu zużycia okładzin ciernych. Dodatkowo przedstawione zostaną poszczególne etapy budowy modelu numerycznego stanowiska badawczego okładzin ciernych. Analizę procesu hamowania przeprowadzono przy użyciu kodu numerycznego wykorzystującego jawny schemat całkowania z uwzględnieniem numerycznej zamiany sił tarcia na ciepło. Wstępnie przeprowadzone zostały symulacje zjawisk zużycia w skali mikroskopowej wykorzystującej metodę SPH.
EN
In this paper the concept of numerical wear process simulation of brake friction linings is presented. Moreover, the development process of the special test rig's numerical model is described. Performed computations of brake process were done based on the dynamic code with explicit solution scheme with heat generation. In order to represent the brake linings abrasive wear with numerical methods the Smooth Particle Hydrodynamics approach was finally adopted.
7
Content available remote Rynek materiałów pokryciowych w Polsce
PL
W artykule dokonano przeglądu odpornych na zużycie materiałów metalowych, ceramicznych I elastomerów, które zostały opracowane lub zaadoptowane na potrzeby górnictwa oraz przeróbki mechanicznej minerałów. W zarysie przedstawiono skład i morfologię takich materiałów, jak: żeliwa stopowe, materiały ceramiczne, węgliki spiekane, kauczuki i poliuretany. Na wybranym przykładzie pokazano wpływ cech konstrukcyjnych tribosystemu na intensywność zużycia jego elementów. Przedstawiono także wyniki badań eksploatacyjnych żeliw stopowych i wpływ ich składu chemicznego na trwałość.
EN
Wear - resistant metallic, ceramic and elastomeric materials developed or adopted for use the mining and mineral processing industries are reviewed. Composition and morphology of white cast irons ceramics, hard metals and elastomers such as natural and synthetic rubbers and polyurethanes are described. The effect of tribosystem design on wear rate is shown. The results from field testing the abrasive wear resistance of several cast irons alloyed with different elements are presented.
EN
A study was made on polymer based composite materials, which are usable without lubrication as sliding members of oscillating motion components which are difficult to lubricate with oil. In this study, polyetheretherketone (PEEK) was used as a matrix, was blend with polytetrafluoroethylene (PTFE) which is a friction-reducing material. Friction and wear characteristics of each specimen in oscillating motion and continuous rotation were studied. As a result, the wear of pure PEEK in oscillating motion was about 20 times that in continuous rotation, but the wear of PTFE blended PEEK in oscillating motion was improved about 3 times that in continuous rotation. And the wear of PTFE blended specimens reduced to about 1/50 that of pure PEEK in oscillating motion and about 1/2 in continuous rotation. When PTFE blended PEEK was filled with bronze particles, wear was even further reduced in oscillating motion and also in continuous rotation. Coefficient of friction of pure PEEK in oscillating motion was greater than that in continuous rotation. When PEEK was blended with PTFE, coefficients of friction were reduced to such an extent as to eliminate differences in friction characteristics according to the direction of motion. Further, pv limits of pure PEEK in oscillating motion were extremely small compared to those in continuous rotation. When PEEK was blended with PTFE, pv limits were improved in oscillating motion and also in continuous rotation.
10
Content available remote Electrodynamic wear - out in electromechanical systems
EN
In this work the questions of electrodynamic wear process of an the conductor with the current are considered. We offer a dynamic model of the wear process of the conductor material when the current is passing, and this model is based on original principle - "method of sections". The mathematical laws are obtained and the calculation ratio for definition of electrodynamic forces in micro- and macrovolumes of the material of the conductor are given.
PL
W referacie przedstawiono wyniki badań zużycia na testerze tribologicznym T-05 azotowanych próbek ze stali 40H. Badano próbki o różnym składzie fazowym strefy azotków. Mierzono ubytek masy próbek oraz sumaryczne zużycie liniowe próbki i przeciwpróbki. Stwierdzono, że zużycie azotowanych próbek ze stali 40H z fazą alfa+epsilon jest znacznie mniejsze niż próbek z fazą alfa+gamma.
EN
The results of wear resistance examinations carried out with the application of the tribological tester T-05 for nitrided samples made from the steel of 40H grade are presented in this paper. The samples with different nitrides zone phase composition were compared. Mass decrement and total linear wear of a sample and a contra-sample were measured in this test. It was found, that the wear resistance of nitrided samples with alpha+epsilon phase is significantly lower, than that of the samples with alpha+gamma phase.
12
Content available remote Metoda analityczna oceny wytrzymałości frykcyjnej układu rur wiertniczych
PL
Opracowana została analityczna metoda na obliczenie trwałości na zużycie rur wiertniczych, w której uwzględniono ważniejsze czynniki procesu zużycia, kinematyki, warunków eksploatacji. Przeprowadzono numeryczną ocenę trwałości rury wiertniczej dla typowych przypadków kontaktu i analizę wyników.
EN
In the model an analytical method of calculation of the wear resistance of drilling pipes was worked out. The most important factors of the wear process, kinetics and exploitation conditions were taken into account. The numerical calculation of the durability of the drilling pipe for typical cases of the pipe contact with the rock was performed.
PL
W opracowaniu przedstawiono analizę skutków azotowania stali o niskich zawartościach dodatków stopowych na przykładzie stali 40H, w kontekście ich wykorzystania na elementy maszyn rolniczych. Wyniki badań odporności na zużycie pozwalają stwierdzić, że stosując odpowiednią technologię azotowania można uzyskać warstwę wierzchnią o wysokiej odporności na zużycie i zacieranie. Szczególnie efektywne okazały się te technologie azotowania, które zapewniają uzyskanie stosunkowo grubych warstw z wyraźnie ukształtowaną strefą azotków.
EN
Considerations concerning nitriding effects for low-alloyed steel (40H steel as an example), used for production of machine elements, are presented in this paper. The results of wear resistance investigations show, that with application of suitable nitriding technology, winning of surface layer characterized by high wear and scuffing resistance, is possible. Especially effective are nitriding technologies, assuring the winning of relatively thick layers, with clearly formed nitrides zone.
PL
Każda maszyna rolnicza zużywając się w pewnym momencie staje się nieprzydatna w procesie eksploatacji. Ten etap istnienia maszyny nie był dotąd przedmiotem badań naukowych, co wynikało częściowo z nieświadomości skali zagrożeń, jakie stanowią one dla środowiska. W pierwszej części publikacji przedstawiono analizę statystyczną obrazującą skalę problemu na przykładzie byłego województwa poznańskiego. W dalszej części przedstawiono metody zagospodarowania wycofanych z eksploatacji maszyn rolniczych oraz analizę i ocenę tych metod pod względem zagrożenia dla środowiska.
EN
Every agricultural machine, getting worn out in the certain moment, becomes useless in the utilization process. This stage of machine's existence has not been the subject of the scientific research till now. It partly resulted from unawareness with the range of dangers, which such machines are for environment. The first part of this publication presents the statistic analysis, which shows the scale of this problem in the former poznanskie province. In the next part there are shown as well the utilization methods of agricultural machines, that are withdrawn from usage, as well as the analysis and the opinion of these methods as to their dangers for environment.
17
Content available remote Model analityczny zużycia ściernego materiałów w warunkach tarcia ślizgowego
PL
Opracowany został model analityczny badania kinetyki zużywania się materiału w warunkach tarcia ślizgowego ze ścierniwem lub skałą. Na podstawie przedstawionego modelu ustalono funkcje na obliczanie zużycia wyższej pary kinematycznej (krążek - skała). Przeprowadzono numeryczne rozwiaząnie zagadnienia.
EN
An analytical model of kinetic investigation of the materials was worked out. The model concerns the sliding friction of the material and the rock. The wear function of the higher kinematic pair (the roll and the rock) was derived. To confirm the validity of the model the numerical calculations were performed.
first rewind previous Strona / 1 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.