EN
A family of biodegradable aliphatic-aromatic co-polyesters (BAAC) was prepared by polycondensation in the melt. The synthesis was carried out with the addition of a small amount of alkaline metals salts which produced the effect of a distinctly improved colour of the polyesters as registered in the L*, a*, b* system. The yellow index of the tested samples was calculated from the chromaticity coordinates X, Y, Z. The colour could have been further improved by an exposure to UV radiation. No change was observed in the average molecular mass of the tested co-polyesters as result of the exposure, while an insignificant drop occurred of the inherent viscosity.
PL
Metodą polikondensacji w stanie stopionym otrzymano grupę biodegradowalnych kopoliestrów alifatyczno-aromatycznych (BAAC). Syntezę prowadzono z udziałem niewielkiej ilości soli metali alkalicznych otrzymując znaczną poprawę barwy kopoliestrów rejestrowaną w systemie L*, a*, b. Na podstawie współrzędnych trójchromatycznych X, Y, Z, obliczono indeks żółtości badanych próbek. Dodatkową poprawę barwy uzyskano naświetlając próbki polimerów promieniowaniem UV. Po naświetlaniu nie stwierdzono zmian w średnich masach molowych badanych kopoliestrów, stwierdzono natomiast niewielkie spadki wartości lepkości inherętnej.
2
Content available remote Solvent Pre-Treated Wool Fabric Permanent Set and Physical Properties
EN
We present the results of an investigation which shows that the yellowing of wool fibre which occurs during light exposure and treatment with boiling water is reduced by pre-treatment of loom state wool fabric with perchloroethylene. The changes in light reflectance and the yellowing index of the treated wool fabric were found to correlate with the data of wool fibre strength, permanent set degree, solubility in urea-bisulphite solution, fluorescence emission and thermogravimetric analysis
PL
W artykule przedstawiono wyniki badań nad zmniejszeniem zażółcenia włókien wełnianych, spowodowanego naświetlaniem i obróbką w gorącej wodzie. Stwierdzono dodatnie oddziaływanie nadchloroetylenu na tkaniny wełniane surowe, otrzymane z krosna. Stwierdzono korelacje pomiędzy odbiciem światła i współczynnikiem zażółcenia obrabianych tkanin a wytrzymałością włókien wełnianych, stopniem trwałości stabilizacji, rozpuszczalnością w roztworze mocznika wodorosiarczynu, emisją fluoroscencyjną i wynikami analizy termograwimetrycznej.