This paper presents the oxidation behavior of tungsten-free γ-γ’ Co-10-Al-5Mo-2Nb and Co-20Ni-10Al-5Mo-2Nb cobalt-based superalloys. This type of alloys is an alternative materials for tungsten contains alloys of Co-Al-W type with γ′- Co3(Al. W) intermetallic phase adequate to γ’- Ni3Al phase identified in Ni based superalloys. Applications of Mo and Nb as a replacement of W is related to tendency to lowering the density of alloys. The investigation included thermogravimetric studies up to 1200°C. The oxidized layer was evaluated, therein microstructure, chemical and phase composition analyses were performed using various methods, inclusive of x-ray diffraction, SEM/EDS analysis and light microscopy.
PL
W artykule przedstawiono wyniki badań dotyczące zachowania się nowych nadstopów kobaltu Co-10Al-5Mo-2Nb i Co-20Ni-10Al-5Mo-2Nb i strukturze typu γ-γ` w warunkach utleniania. Ta grupa materiałów stanowi alternatywę dla stopów wolframowych o ogólnym wzorze Co-Al-W, w których fazą umacniająca jest faza międzymetaliczna typu γ’- Co3(Al, W), będąca odpowiednikiem fazy γ’- Ni3Al, identyfikowanej w nadstopach na bazie niklu. Wprowadzenie Mo i Nb jako zamienników W jest związane przede wszystkim z chęcią obniżenia gęstości stopów. Przedstawione badania obejmują badania termograwimetryczne do temperatury 1200°C. Ocenie poddano warstwę powstałych tlenków, ich mikrostrukturę, jak również skład chemiczny oraz skład fazowy. Zastosowano metody badawcze obejmujące analizę rentgenowską składu fazowego XRD, analizę mikrostruktury oraz składu chemicznego metodami SEM/EDS jak również ocenę mikrostruktury z zastosowaniem mikroskopii optycznej.
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.