This paper presents the experimental results of the role of ball burnishing in improving of the surface integrity produced in finish hard machining of hardened 41Cr4 steel. The characterization of the surface integrity includes two standardized sets of 2D and 3D roughness parameters, the distributions of microhardness, residual stresses and the microstucture of the sublayer which was examined using SEM/EDS technique. The functional properties of the surface layer were predicted and discussed. This study reveals that ball burnishing performed on hard turned surfaces improves not only surface roughness but also results in better service properties compared with those generated by CBN hard turning.
PL
W artykule przedstawiono analizę wyników doświadczalnych dotyczących roli nagniatania tocznego kulką ceramiczną w polepszeniu właściwości warstwy wierzchniej wytworzonej podczas wykończeniowego toczenia utwardzonej stali 41Cr4. Charakteryzacja wytworzonej warstwy wierzchniej obejmuje określenie dwóch zbiorów znormalizowanych parametrów chropowatości powierzchni, rozkład wartości twardości naprężeń własnych oraz badania mikrostruktury metodami mikroskopii elektronowej EM/BSE/EDX. Analiza wyników badań pozwala stwierdzić, że nagniatanie kulką po toczeniu na twardo poprawia nie tylko chropowatość powierzchni, ale również polepsza właściwości eksploatacyjne w porównaniu z efektami toczenia narzędziami z CBN.