EN
The experimental results concerning hydroxyapatite and struvite crystals' growth kinetics while calcium and magnesium ions precipitation from diluted solutions by ammonium dihydrogenphosphate(V) solution addition in alkaline environment are presented. The measurements were clone using continuous laboratory DTB MSMPR crystallizer. The influence of calcium/magnesium ions' concentration in the feeding solution, suspension residence time, temperature (hydroxyapatite) and pH (struvite) on the resulting Crystal Size Distributions (CSDs) courses was investigated. The ln n(L) dependencies' shapes suggested occurrence of the Size Dependent Growth (SDG) kinetics. The parameters' values in the size-dependent crystal growth kinetic equation (Rojkowski hyperbolic II model assumed) were evaluated. Both the experimental data and evaluated dependencies can be practically applied to the design of processes concerned with the removal of ca1cium and/ar magnesium ions from water or diluted solutions.
PL
Przedstawiono wyniki badań wzrostu kryształów hydroksyapatytu i struwitu w procesie strącania jonów wapnia i magnezu z roztworów rozcieńczonych za pomocą roztworu diwodorofosforanu(V) amonu w środowisku alkalicznym. Pomiary przeprowadzono w ciągłym krystalizatorze laboratoryjnym DTB MSMPR. Przebadano wpływ stężenia jonów wapnia lub magnezu w surowcu podawanym do krystalizatora, czasu przebywania zawiesiny w krystalizatorze, temperatury (hydroksyapatyt) i pH (struwit) na rozkład rozmiarów kryształów soli odprowadzanych z krystalizatora. Do obliczeń przyjęto model szybkości wzrostu kryształów uwzględniający zjawisko zależności szybkości wzrostu od rozmiarów kryształów (SDG). Obliczenia przeprowadzono dla modelu hiperbolicznego II SDG Rojkowskiego. Z rozkładu gęstości populacji kryształów produktu obliczono graniczne (maksymalne i minimalne) wartości szybkości wzrostu kryształów hydroksyapatytu i struwitu. Wyniki badań i obliczeń mogą być wykorzystane do projektowania procesu usuwania jonów wapnia i/lub magnezu z wody lub z roztworów rozcieńczonych.
EN
The measurement results of barium sulphate reaction crystallization kinetics are presented. The experiments were carried out in the crystallizer with internat circulation of suspension. The crystallizer was continuously fed with solution obtained after used quenching salts solubilization in water and (stoichiornetrically) crystalline ammonium sulphate. The barium sulphate nucleation and crystal growth rates were estimated from crystal size distributions taking into account a size dependent growth (SDG) models. The results may be applied in the proecological used quenching salts utilization processing technology.
PL
Przedstawiono wyniki badań kinetyki krystalizacji siarczanu baru. Proces krystalizacji strąceniowej przeprowadzono w krystalizatorze ciągłego działania z wewnętrzną cyrkulacją zawiesiny. Do krystalizatora podawano roztwór uzyskany po rozpuszczeniu w wodzie soli odpadowej po hartowaniu metali i krystaliczny siarczan(VI) amonu (w ilości stechiometrycznej). Przebadano trzy różne roztwory zasilające krystalizator, otrzymane po rozpuszczeniu w wodzie soli pohartowniczych o różnej zawartości chlorków: wapnia, sodu i potasu. Szybkości zarodkowania i wzrostu kryształów siarczanu baru obliczono z rozkładu rozmiarów kryształów produktu (mieszaniny [wzór] i [wzór]). Do obliczeń przyjęto model szybkości wzrostu kryształów uwzględniający zjawisko zależności szybkości wzrostu od rozmiarów kryształów (SDG). Wyniki badań mogą być wykorzystane przy projektowaniu technologii utylizacji stałych odpadów pohartowniczych.