EN
In this study beneficiation of a sulphide ore from the Gümüşhane-Black Sea Region of Turkey was investigated. Detailed flotation studies were carried out with the ore sample which contained 2.95% Pb, 6.72% Zn and 0.32% Cu. Mineralogical analyses showed that the sample includes pyrite, galena, sphalerite, chalcopyrite, tennantite, cerussite, anglesite and smithsonite. On the other hand, hematite, goethite, limonite, calcite and quartz were determined as gangue minerals. Selective sulphide concentrates with low arsenic content were tried to be produced by froth flotation. Individual concentrates of Pb, Zn and Cu assayed 67.54% Pb, and 61.49% Zn and 23.31% Cu where corresponding recoveries were 73.0% and 77.1% and 38.7%, respectively. Arsenic contents were less than 2000 ppm in the lead and zinc con-centrates. Copper concentrate assayed 5.03% As since the major copper minerals were in tennantite form (copper arsenic sulphide mineral). In flotation tests, non-toxic reagents such as metabisulphite, caustified starch, and activated carbon were used to depress minerals in relevant circuits.
PL
Przedstawiono wyniki badań, których celem była wstępna analiza wpływu odczynnika apolarnego na przebieg procesu flotacji siarczkowej rudy miedzi pochodzącej z rejonu Legnicko-Głogowskiego Okręgu Miedziowego (LGOM). Wykonano dwie serie eksperymentów flotacyjnych: jedną w warunkach standardowych z użyciem etylowego ksantogenianu potasu (KEtX) jako odczynnika zbierającego oraz drugą serię flotacji z zastosowaniem wodnej emulsji n-dodekanu (C12), jako modelowego odczynnika apolarnego oraz ksantogenianu (KEtX). We wszystkich eksperymentach odczynnikiem pianotwórczym był roztwór \alfa-terpincolu. Stwierdzono, że w obecności odczynnika apolarnego część minerałów miedzi ulega flotacji, a pozostała ich część może być 'doflotowana' przy użyciu standardowego kolektora - ksantogenianu. Dokonano również porównania wyników flotacji rudy miedzi z użyciem n-dodekanu z serią flotacji z wcześniejszych badań autorki z zastosowaniem krótszego homologu - n-heptanu. Stwierdzono, że przy zastosowanym reżimie odczynnikowym, n-heptan wykazuje się wyższą selektywnością w porównaniu z n-dodekanem. W obecności różnych dawek n-heptanu, badany materiał lepiej wzbogacał się w nośniki węgla organicznego niż w minerały miedzi.
EN
Investigations of n-dodecane used in flotation of copper ore from the Legnica-Glogow Copper Basin (LGOM) were presented in the paper. The aim of the work was estimation of influence of nonpolar reagent's on the results of copper ore flotation. Two series of flotation tests were conducted. The first series - flotation experiments with standard flotation with xanthate collector only (KEtX), were compared with the second series: flotation experiments with n-dodecane addition (C12) in the first stage and then xanthate addition (KEtX). n-dodecane was used in form of aqueous emulsion and frother was aqueous solution of \alfa-terpincol. Flotation results showed that a part of copper minerals float with n-dodecane, and the rest of them is recovered using xanthate collector. The best results were obtained for the first series (with xanthate only). These flotation results were compared with the results of copper sulphide ores flotation with n-heptane addition. It was found that with the doses reagent used, n-heptane has a higher selectivity in comparison with n-dodecane. In the presence of various doses of n-heptane, tested material enriched better in organic carbon carriers than in the copper minerals.
PL
W artykule przedstawiono porównanie wyników ługowania chemicznego i biologiczno-chemicznego rud antymonu i złota Sb-(Au) ze złoża Pezinok (Malé Karpaty Mts., Western Carpathians, Slowacja) przeprowadzonego w tych samych warunkach. Wyniki badań przedstawiają kolejność i postęp utleniania zaprezentowanych minerałów rudnych (lelingit, arsenopiryt, stybnit, antymon rodzimy, gudmunit, bertheryt, piryt, sfaleryt i chalkopiryt). Wykazano różnice między ługowaniem chemicznym i biologiczno-chemicznym szlifowanych powierzchni wybranych minerałów siarczkowych. Efekty ługowania biologiczno-chemicznego minerałów siarczkowych są znacząco wyższe od wyników ługowania chemicznego bez udziału bakterii.
EN
The article presents the results of the leaching experiments, the comparison of the chemical and biological-chemical leaching experiments with ores from the Sb-(Au-) base metal deposit of Pezinok (Malé Karpaty Mts., Western Carpathians, Slovakia) under the same conditions in solutions. The research study shows the oxidation order and the progression of presented ore minerals (löllingite, arsenopyrite, stibnite, native Sb, gudmundite, berthierite, pyrite, sphalerite and chalcopyrite). The differences between chemical and biological-chemical leaching activity of various ore minerals at the surface of polished sections have been discussed. The extent of the biological-chemical leaching of sulphide minerals is significantly higher than the chemical leaching of sulphide minerals without bacteria.
EN
Post-flotation tailings from zinc- and lead-ore processing in the "Bolesław" mining-metallurgy plant are deposited in sedimentary ponds. Dolomite CaMg(CO3)2 is the main constituent (above 70 %) of the wastes. They contain also considerable amounts of sulphur (up to 14 %) and iron (up to 16 %) in form of sulphides, mainly of pyrite and marcasite (FeS2; 13-30 %). Therefore, the occurrence in them of bacteria possessing sulphur- and/or iron-oxidizing properties (considered to be especially useful in the metals bioleaching processes) bas been expected. We isolated such bacteria and evaluated their abilities to acidify liquid media containing sulphur S° or thiosulphates S2O32-,-and to oxidize Fe(II)-ions. These processes may lead to the tailings acidifying observed in the sedimentary pond deeper layers as well as to the metals release into environment - despite the low rates of bacterial oxidation of the sulphur and iron compounds under simultaneously high concentration of dolomites in the post-flotation waste materials being investigated.
PL
Odpady poflotacyjne z procesów przetwórstwa rud cynku i ołowiu w Kombinacie Gómiczo-Hu1niczyrn "Bolesław" są deponowane w stawach osadowych. Głównym składnikiem (powyżej 70 %) tych odpadów jest dolomit CaMg(CO3)2. Zawierają one także znaczne ilości siarki (do 14 %) i żelaza (do 16 %) w formie siarczków, głównie pirytu i markazytu (FeS2; 13-30 %). Dlatego oczekiwano występowania w nich bakterii, wykazujących zdolności utleniania siarki i/lub żelaza (uważanych za szczególnie użyteczne w procesach bioługowania metali). Izolowaliśmy takie bakterie i oceniliśmy ich zdolności do zakwaszania pożywek płynnych zawierających siarkę S° lub tiosiarczany S2O32- oraz do utleniania jonów Fe(II). Procesy te mogą prowadzić do zakwaszania odpadów, obserwowanego w głębszych warstwach składowiska, jak również do uwalniania metali do środowiska - pomimo małych szybkości bakteryjnego utleniania związków siarki i żelaza przy jednocześnie dużej koncentracji dolomitów w badanych odpadach poflotacyjnych.
EN
In this report it's looked through the problem about the research of the possibilities, by the change of the solid phase content in the pulp for improvement of the flotation process selectivity during the flotation of the multicomponent ores. It's searched for the relation between the lessened aeration in the conditions of the flotation with higher density of the flotation pulp and the competitive struggle between the main sulphide minerals which differ theirselves of it's hydrophobic mineral surface and of the processes, running in the three-phased froth as well. The results of the research indicate that the increased density doesn't always lead to the decrease of the process of selectivity. It's found that the rising of the solid phase content in the pulp up to a definite limit improves the selectivity of the process, but it can hardly get worse above this limit. The limit is most likely to be different for the different technological cases, but it's obviously to be always available.
PL
Artykuł ten przedstawia problem badania możliwości, poprzez zmianę zawartości fazy stałej w mętach, poprawy selektywności procesu flotacji podczas flotacji wieloskładnikowych rud. Poszukiwano relacji pomiędzy zmniejszeniem aeracji w warunkach flotacji większej gęstości mętów flotacyjnych, różnicowanie pomiędzy głównymi minerałami siarczkowymi, co do ich hydrofobowości powierzchni oraz procesami przeprowadzanymi w trójfazowej pianie. Wyniki badań wskazują, że zwiększana gęstość nie zawsze prowadzi do obniżenia selektywności procesu. Stwierdzono, że zwiększenie fazy stałej w mętach do pewnej granicy zwiększa selektywność procesu, a może ją pogorszyć powyżej tej granicy. Granica zazwyczaj jest różna dla różnych przypadków technologicznych, ale jest zawsze możliwa do określenia.
6
Content available remote Effects of EDTA on selective flotation of sulphide minerals
EN
Unwanted activation of sphalerite and pyrite by copper ions dissolved from copper minerals (mainly chalcopyrite) hampers flotation selectivity. Galvanic interaction between the sulphide minerals is considered as the main cause for such activation. Therefore, a complexing agent, EDTA, was used to prevent unwanted activation of sphalerite and pyrite by copper ions in the presence and absence of collector. In this study, unwanted activation of sphalerite and pyrite by copper ions and inhibition of this activation by using EDTA was investigated by using cyclic voltammetry and microflotation techniques. The influence of galvanic interaction between chalcopyrite-pyrite and chalcopyrite-sphalerite on flotation selectivity and the effect of EDTA were determined with microflotation tests performed with single mineral and mineral mixtures. The results pointed out dual effect of EDTA as preventing activation of sphalerite and pyrite by copper ions, but at the same time enhancing their collectorless flotation by removing the metal hydroxides from their surfaces.
PL
Proces aktywacji sfalerytu i pirytu przez jony miedzi, znajdujące się w roztworze, ma niekorzystny wpływ na selektywność procesu flotacji. Procesy galwaniczne są rozpatrywane jako główna przyczyna powodująca aktywację. Odczynnik kompleksujący- EDTA- został użyty w celu przeciwdziałaniu aktywacji sfalerytu i pirytu. Badania z wykorzystaniem EDTA prowadzone były bez i z udziałem kolektora. Metody cyklovoltamperometrii i mikroflotacji zostały wykorzystanie dla zbadania efektów wynikających z dodania EDTA. Dla układów chalkopiryt-sfaleryt i chalkopiryt-piryt określono wpływ EDTA na zjawiska galwaniczne i na selektywność flotacji. Otrzymane wyniki wskazują, ze dodanie EDTA zapobiega aktywacji sfalerytu i pirytu jonami miedzi, a także podwyższa bezkolektorową flotację tych minerałów przez usunięcie wodorotlenków metali z ich powierzchni.
first rewind previous Strona / 1 next fast forward last