Preferencje help
Widoczny [Schowaj] Abstrakt
Liczba wyników

Znaleziono wyników: 4

Liczba wyników na stronie
first rewind previous Strona / 1 next fast forward last
Wyniki wyszukiwania
Wyszukiwano:
w słowach kluczowych:  stripes
help Sortuj według:

help Ogranicz wyniki do:
first rewind previous Strona / 1 next fast forward last
EN
Very high-resolution modelling of the northeastern Baltic Proper shows that preferentially elongated along the flow, submesoscale inhomogeneities of hydrodynamic fields or stripes of the order of 10–20 km in length and 1 km in width, are typical for summer season both in surface mixed layer and for interior layers which are not directly exposed to atmospheric forcing. In surface layer, the presence of stripes is supported by the remote sensing imagery and their vertical extension is comparable with the mixed layer depth (approx. 5–8 m). In the interior layers, the vertical extension of stripes is considerably larger (approx. 10–50 m) and their slopes exceed the isopycnal slope. Four competitive mechanisms of formation of the mesoscale striped texture are considered: stirring of large-scale inhomogeneities by the eddy field, the classic, inviscid adiabatic fluid symmetric instability, the McIntyre instability, and the strain-induced frontogenesis. Based on the instability criteria and the growth rates and geometry of the disturbances, the classic symmetric instability and the strain-induced frontogenesis are probably responsible for the formation of submesoscale striped texture in the surface layer, while in the interior layers, the strain-induced frontogenesis and hypothetically the McIntyre instability can be essential. Stirring of large-scale inhomogeneities by the eddy field could be responsible for formation of striped texture in a passive tracer concentration and in temperature and salinity in the presence of thermohaline gradients on isopycnic surfaces (thermoclinicity), but it does not imply formation of stripes in dynamically active tracers, such as vertical vorticity, horizontal gradients of buoyancy, etc.
2
PL
W artykule przedstawiono wykorzystanie robotyzacji w automatyzacji pomiarów przeprowadzanych za pomocą skanerów optycznych. Umożliwia ona obniżenie kosztów wykonywania pomiarów dzięki skróceniu czasu ich wykonywania. Zbierane informacje o kształcie powierzchni badanych przedmiotów pozwalają na ich późniejsze wykorzystywanie do analizy jakości produkowanych elementów. Automatyzacja procesu pomiaru z wykorzystaniem robota przemysłowego umożliwia wyeliminowanie błędów przypadkowych popełnianych przez obsługujących go pracowników. Sposób przeprowadzania pomiarów jest niewrażliwy na błędy pozycjonowania manipulatora, co wynika z lokalizowania poszczególnych pomiarów za pomocą punktów referencyjnych, a nie pozycji skanera względem badanej części.
EN
In the paper use of robotization in the automation of measurements with optical scanners has been presented. It makes reduction of costs possible thanks to shortening of the time needed to perform the measurements. Captured data of the shape of examined surfaces may later be used for evaluating the quality of manufactured components. The automation of the measuring process employing an industrial robot makes it possible to eliminate random errors caused by the operators. The method of performing the measurements is insensitive to positioning errors of the manipulator because all individual measurements (scans) are located by the reference points and not by the position of the scanner in relation to the examined part.
EN
The Cu-10 wt %Co melt spun ribbons with giant magneto-resistance (GMR) properties were aged at 773 K for 0.5, 1, 2, 4, 16 and 32 hours. Quantitative transmission electron microscopy (TEM) microstructural analysis have been carried out to determine size distributions of beta -Co precipitates. The results of magnetisation, coercitivity and electrical magneto-resistivity measurements were correlated with the mean diameters of coherent beta-Co particles. It was shown, that the maximum GMR is achieved for the mean diameters of beta-Co particles less than 10 nm, whereas for larger particles the GMR effect is strongly reduced.
PL
Otrzymane metodą krystalizacji z ciekłej strugi taśmy stopu Cu-10% wag.Co, wykazującego gigantyczny magnetoopór, wyżarzono w temperaturze 773 K przez 0,5, 1, 2, 4, 16 i 32 godziny. W celu określenia rozkładów wielkości wydzieleń beta--Co po różnych wariantach wyżarzania przeprowadzono ilościową analizę mikrostruktury metodami transmisyjnej mikroskopii elektronowej. Wyniki pomiarów namagnesowania, koercji i magnetooporu skorelowano z wartościami średniej średnicy koherentnych wydzieleń beta-Co. Wykazano, że stop wykazuje maksymalny magnetoopór, gdy średnia średnica wydzieleń jest mniejsza niż 10 nm. Wzrost średniej wydzieleń powyżej 10 nm sprawia, że efekt magnetooporu wyraźnie maleje.