EN
In the present paper magnetostriction, Young's modulus and primary crystallization were examined for a group of amorphous alloys of nanoperm family i.e. Fe78B22, Fe76B22X2 (X=Cr, Zr, Nb). It was shown that the alloying additions cause a correlated decrease of Young's modulus (over 2 times) and magnetostriction coefficients - parallel (about 40%) and spontaneous (about 30 %) in relation to the Fe7SB22, alloy. The observed decrease of Young's modulus and magnetostriction coefficients are correlated with the heat of crystallization Qr. The crystallization temperature (DSC maximum) and the apparent activation energy of crystallization decrease monotonically with increasing QT.
PL
W niniejszej pracy dla grupy amorficznych stopów typu nanosem tj. Fe78B22, Fe76B22X2 (X=Cr, Zr, Nb) badano zjawisko magnetostrykcji, modułYounga i krystalizację pierwotną. Pokazano, że dla grupy badanych materiałów dodatki stopowe powodują skorelowany spadek wartości modułu Younga (ponad 2 razy) oraz współczynników magnetostrykcji - równoległej (około 40%) i spontanicznej (około 30 %). Obserwowany spadek modułuYounga i współczynników magnetostrykcji koreluje ze spadkiem ciepła krystalizacji Qr. Temperatura krystalizacji i energia aktywacji krystalizacji także monotonicznie maleją ze wzrostem Qr.