The effect of encapsulation of LaNi4.5Co0.5 hydrogen storage powdered material, with thin magnetron sputtered layer of SiC, on basic hydrogenation parameters of the composite hydride electrode has been discussed. The multicycle galvanostatic charge/discharge method allowed to determine electrode hydride capacity, exchange current density of the H2O/H2 system, and evaluate material tendency to corrosion degradation. The electrochemical diagnostic experiments carried out at room temperature, at charge/discharge rates of −186/+186 mA g−1 , revealed the initial discharge capacities on the level of 289 mA h g−1 for the tested electrodes. The presence of SiC layers on hydride powder improves kinetics of hydrogen electrosorption process.
PL
Badano wpływ enkapsulacji materiału magazynującego wodór LaNi4.5Co0.5 cienką warstwą SiC, uzyskiwaną przez rozpylanie magnetronowe, na podstawowe parametry kompozytowej elektrody wodorkowej. Galwanostatyczna wielocykliczna metoda ładowania/rozładowania pozwoliła określić pojemność wodorkową, gęstość prądu wymiany układu H2O/H2 i ocenić tendencję materiału do degradacji korozyjnej. Charakterystyki elektrochemiczne zmierzone w temperaturze otoczenia przy szybkościach ładowania/rozładowania równych −186/+186 mA g−1 pozwoliły ustalić, iż początkowe pojemności rozładowania badanych elektrod są na poziomie 289 mA h g−1 . Obecność warstw SiC na materiale proszkowym poprawia kinetykę procesu elektrosorpcji wodoru.
2
Content available remote Evaluation of hydride electrode parameters at different discharge rates
EN
The effects of hydride electrode discharge rate on its discharge capacity and exchange current density of H2O/H2 system are discussed. The LaNi4.5Co0.5 hydrogen storage alloy has been applied as the powder composite electrode active material. In all experiments the electrode was being galvanostically charged with a medium rate of –0.5 C. For electrode discharging, low rates of hydrogen oxidation (idisch ≤ 0.35 C) have been applied. It is shown that for idisch between 0.1 C and 0.35 C the electrode material capacity linearly increases with discharge rate decrease. Similarly, soft discharge conditions favor increase of H2O/H2 exchange currents.
PL
Dyskutowany jest wpływ szybkości rozładowywania elektrody wodorkowej na jej pojemność prądową i gęstość prądu wymiany układu H2O/H2. Jako materiał aktywny kompozytowej, proszkowej elektrody wodorkowej wybrano stop LaNi4.5Co0.5. We wszystkich eksperymentach elektrodę ładowano galwanostatycznie ze stałą, umiarkowaną szybkością, równą –0,5 C. Do rozładowywania zastosowano niskie prądy utleniania wodoru (idisch ≤ 0.35 C). Pokazano, że w zakresie gęstości prądów rozładowania 0,1 C do 0,35 C pojemność prądowa materiału liniowo wzrasta ze spadkiem szybkości rozładowania. Podobnie, łagodne warunki rozładowania sprzyjają wzrostowi prądu wymiany układu H2O/H2.
EN
The hydrogenation properties of La2Ni9CoAlx (x = 0.2, 0.3 and 0.4) non-stoichiometric alloys, in terms of their discharge capacity, the H2O/H2 exchange current density, hydrogen diffusivity and high rate dischargeability have been studied. The electrochemical tests have been carried out using chronopotentiometric and chronoamperometric methods. Electrochemical hydrogenation experiments at –185/+185 mA·g-1 charge/discharge rates revealed the discharge capacities of 329÷339 mA·h·g-1 for the tested electrodes. Increase of aluminium addition in the tested alloys results in decrease of exchange current density and confines hydrogen diffusivity. The high rate dischargeability (HRD) of La2Ni9CoAl0.2 alloy electrode at 1000 mA·g-1 reaches 80% of maximum value and is distinctly higher than these of La2Ni9CoAl0.3 and La2Ni9CoAl0.4 alloy electrodes, respectively.
PL
Badano zdolności pochłaniania wodoru przez niestechiometryczne stopy La2Ni9CoAlx (x = 0,2, 0,3 lub 0.4) pod kątem pojemności rozładowania, gęstości prądu wymiany układu H2O/H2, dyfuzyjności wodoru i odporności na rozładowanie wysokoprądowe. Testy elektrochemiczne wykonano metodami chronopotencjometryczną i chronoamperometryczną. Pomiary elektrochemicznego ładowania/rozładowania przeprowadzono stosując szybkości ładowania/ rozładowania równe –185/+185 mA·g-1. Badane elektrody wykazywały pojemności rozładowania w zakresie 329÷339 mA·h·g-1. Wzrost zawartości aluminium w badanych stopach prowadzi do spadku gęstości prądu wymiany i do ograniczenia dyfuzyjności wodoru. Rozładowywalność wysokoprądowa (HRD) elektrody La2Ni9CoAl0.2 osiąga 80% wartości maksymalnej przy szybkości 1000 mA·g-1 i jest wyraźnie większa, niż dla elektrod na bazie stopów La2Ni9CoAl0.3 i La2Ni9CoAl0.4.
EN
The accuracy of determination of major parameters characterizing the composite, LaNi4.5Co0.5-based, hydride electrode (containing 0.03 g of active material) has been evaluated on the basis of 6 repetitions of 10-cycle charge/discharge curves. Relative error of discharge capacity decreases a little with electrode cycling and attains values on the level of 6% after 10 cycles. The exchange current density of the H2O/H2 system is charged with an error of 12–15%, irrespectively of cycle number. Material corrosion rate determined in 6 M KOH solution increases with cycling and is charged with ca 15% experimental error.
PL
Na podstawie 6 powtórzeń 10-cyklowych krzywych ładowania/rozładowania zmierzonych dla kompozytowych elektrod na bazie LaNi4.5Co0.5 (zawierających 0,03 g materiału aktywnego) oceniono dokładność wyznaczania podstawowych parametrów charakteryzujących kompozytową elektrodę wodorkową. Błąd względny wyznaczania pojemności rozładowania maleje nieco w miarę cyklowania, przyjmując po 10 cyklach wartości na poziomie 6%. Gęstość prądu wymiany układu H2O/H2 obarczona jest błędem ok. 12–15% (niezależnym od numeru cyklu). Szybkość korozji materiału w 6 M roztworze KOH wzrasta w miarę cyklowania i jest obarczona przeciętnym błędem 15%.
first rewind previous Strona / 1 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.