The article presents selected theoretical and experimental test results for cold forming of AlCu4MgSi aluminum alloy conducted on an oscillating die press PXW-100AAb. Cylindrical samples of aluminum alloy used in the tests were the T42 ones subjected to the process of natural ageing as well as the ones in transient W temper obtained by solution treatment. The experimental tests were supplemented with a numerical analysis based on the FEM. It was assumed in the calculations that a rigid-plastic material model, with thermal phenomena taken into account, and, additionally, the Cockroft-Latham material cracking model would be used. The obtained test results proved that additional heat treatment preceding cold forming allows for increasing the limit strain.
PL
W artykule przedstawiono wybrane wyniki badań teoretycznych i doświadczalnych dotyczących kształtowania na zimno stopu aluminium AlCu4MgSi, przy użyciu prasy z wahającą matrycą PXW-100AAb. Próbki cylindryczne wykonane są ze stopu aluminium w stanie naturalnym T42 oraz w stanie przejściowym W, który uzyskano przez obróbkę przesycania. Badania doświadczalne uzupełniono o analizę numeryczną bazującą na MES. Obliczenia wykonano zakładając model materiałowy sztywno-plastyczny z uwzględnieniem zjawisk termicznych, gdzie dodatkowo zastosowano model pękania materiału Cockrofta-Lathama. Uzyskane wyniki badań wykazały, że dodatkowa obróbka cieplna wsadu, poprzedzająca jego plastyczne kształtowanie na zimno pozwala zwiększyć zakres dopuszczalnych odkształceń.
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.