Small additions of Cr, Mo and W to aluminium-iron-nickel bronze are mostly located in phases &kappa i (i=II; III; IV),and next in phase &alpha (in the matrix) and phase γ2. They raise the temperature of the phase transformations in aluminium bronzes as well as the casts’ abrasive and adhesive wear resistance. The paper presents a selection of feeding elements and thermal treatment times which guarantees structure stability, for a cast of a massive bush working at an elevated temperature (650–750°C) made by means of the lost foam technology out of composite aluminium bronze. So far, there have been no analyses of the phenomena characteristic to the examined bronze which accompany the process of its solidification during gasification of the EPS pattern. There are also no guidelines for designing risers and steel internal chill for casts made of this bronze. The work identifies the type and location of the existing defects in the mould’s cast. It also proposes a solution to the manner of its feeding and cooling which compensates the significant volume contraction of bronze and effectively removes the formed gases from the area of mould solidification. Another important aspect of the performed research was establishing the duration time of bronze annealing at the temperature of 750°C which guarantees stabilization of the changes in the bronze microstructure – stabilization of the changes in the bronze HB hardness.
first rewind previous Strona / 1 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.