The influence of boron carbide and tungsten carbide on the apparent porosity, density, coercive force, hardness and micro-structure of metal matrix composite of the Ferro-TiC type, is presented in this paper. The samples of investigated steel/titanium carbide composite were produced by powder metallurgy process, i.e. by powders mixing and compacting followed by sintering in the vacuum furnace. According to the results, steel/titanium carbide composite materials with addition up to 11.9 vol.% of boron carbide are interesting to detailed investigation as well as materials having more than 17.2 vol.% of tungsten carbide because these compositions show significant changes in hardness and coercive force values.