EN
The study discussed in the article aimed to analyse the effect of the peening of each bead on properties of butt joints made of steel S960QL and welded using the robotic MAG welding method (135) and a ceramic backing strip. In addition, the objective of the study was to identify the effect of the peening treatment on the level of stresses. The analysis involved the comparison of three butt joints in the post-weld state (i.e. only after welding), subjected to peening (preceded by welding) and to post-weld heat treatment (stress relief annealing). The purpose of the high-frequency peening (90 Hz) of each bead was to reduce stresses in the welded joint by introducing tensile stresses into the latter. The study-related tests involved the use of a Weld Line 10 air hammer (PITEC GmBH). The tests required by the EN ISO 15614-1 standard were supplemented with measurements of stresses involving the use of the Barkhausen effect (based on a testing procedure proposed by the technology provider, i.e. the NNT company). The tests revealed that the performance of high-frequency peening following the making of each bead did not lead to the obtainment of negative results of all the tests required during welding procedure qualification concerning the plate made of steel S960QL (in comparison with test plates after welding and stress relief annealing). The interpass peening of the weld face and that of the HAZ reduced post-weld residual stresses at a distance of 15 mm away from the joint axis (in comparison with stresses measured in the specimens after welding). The test results justified the positive assessment of peening in respect of tensile stress reduction in the fusion line area and in the HAZ.
PL
Celem badań była analiza wpływu przekuwania każdego ze ściegów na własności złącza doczołowego ze stali S960QL spawanego z wykorzystaniem podkładki ceramicznej na stanowisku zrobotyzowanym metodą 135 (MAG) oraz określenie wpływu przekuwania na poziom naprężeń. Analiza ta oparta była na porównaniu trzech złączy doczołowych w stanie po spawaniu, z przekuwaniem każdego ze ściegów oraz z przeprowadzoną pospawalniczą obróbką cieplną – wyżarzanie odprężające. Przekuwanie o wysokiej częstotliwości (90 Hz) każdego wykonanego ściegu miało na celu zmniejszenie naprężeń w złączu spawanym poprzez wprowadzenie do niego naprężeń rozciągających. Został do tego wykorzystany młot pneumatyczny Weld Line 10 firmy PITEC GmBH. Poza badaniami wymaganymi przez normę EN ISO 15614-1 wykonane zostały pomiary naprężeń z wykorzystaniem efektu Barkhausena w oparciu o procedurę badawczą dostawcy technologii – Firmę NNT. Przeprowadzone badania wykazały, że zastosowanie przekuwania o wysokiej częstotliwości po wykonaniu każdego ściegu nie wpłynęło na negatywny wynik wszystkich badań wymaganych podczas kwalifikowania technologii spawania blachy S960QL w porównaniu do płyt próbnych w stanie po spawaniu i po obróbce cieplnej – wyżarzanie odprężające. Przekuwanie międzyściegowe lica spoiny i SWC spowodowało redukcję naprężeń szczątkowych po spawaniu w odległości 15 mm od osi złącza w porównaniu do wyniku pomiaru naprężeń dla próbki w stanie po spawaniu. Pozwala to na pozytywną ocenę przekuwania w kontekście redukcji naprężeń rozciągających w obszarze linii wtopienia i SWC.
2
Content available remote Laser welding of high-strength steel S960QL
EN
The article discusses the results of tests concerning the effect of parameters used during the basic bead-on-plate laser welding (i.e. location of the laser beam focus, welding rate and linear welding energy) of 4.0 mm thick sheets made of high-strength steel S960QL on the quality and properties of simulated butt joints. The welding tests were performed using a YAG TruDisk 3302 Yb disk laser (TRUMPF) having a maximum output power of 3.3 kW and provided with a head focusing the laser beam spot to a diameter of 200 μm. The simulated butt welded joints were made without the filler metal, using a technique which consisted in the laser beam melting of sheets. Macroscopic and microscopic tests as well as impact strength tests, fractographic tests and microhardness measurements involved the cross-section of the simulated specimens.
PL
W artykule opisano wyniki badań wpływu podstawowych parametrów spawania laserowego (tj. położenia ogniska wiązki laserowej, prędkości spawania oraz energii liniowej spawania) blach o grubości 4,0 mm ze stali o wysokiej wytrzymałości S960QL na jakość i właściwości symulowanych złączy doczołowych. Próby spawania wykonano za pomocą lasera dyskowego Yb:YAG TruDisk 3302 firmy TRUMPF o mocy maksymalnej 3,3 kW z głowicą ogniskującą wiązkę do średnicy 200 μm. Symulowane złącza doczołowe blach spawano bez materiału dodatkowego techniką polegającą na przetapianiu blach wiązką laserową. Wykonano badania makro- i mikroskopowe, próby udarności, badania fraktograficzne oraz pomiary mikrotwardości na przekroju poprzecznym próbek.
PL
Bardzo często podczas wytwarzania konstrukcji stalowych zachodzi konieczność usuwania ewentualnych wad i niezgodności spawalniczych powstałych w trakcie spawania. Dodatkowy cykl cieplny towarzyszący ponownemu wykonaniu spoiny ma niewątpliwie negatywny wpływ na właściwości mechaniczne SWC. W artykule przedstawiono wyniki badań technologicznych nad wpływem ponownego spawania łukowego metodą MAG, prowadzonego w ramach naprawy, na właściwości SWC złączy doczołowych ze stali S960QL.
EN
The fabrication of steel structures is often accompanied by the necessity of removing defects and welding imperfections formed during welding. An additional thermal cycle accompanying the making of a new weld has an undoubtedly detrimental effect on the mechanical properties of the heat affected zone (HAZ). The article discusses results of technological tests concerning the effect of MAG repair welding on the properties of the HAZ butt joints made of steel S960QL.
EN
The article discusses the advantages of the hybrid laser + MAG welding method as well as the advantages and exemplary applications of high yield point steel S960QL. The study involved the performance of the hybrid welding of butt joints having various thicknesses and made of high yield point steel (960 MPa) in the flat and in the horizontal position. In addition, the study included macro and microscopic metallographic tests of the test joints.
PL
Opisano zalety procesu spawania hybrydowego laser + MAG. Podano korzyści oraz przykłady zastosowania stali o wysokiej granicy plastyczności S960QL. Przedstawiono wyniki badań spawania hybrydowego złączy doczołowych o różnych grubościach ze stali ulepszonych cieplnie o podwyższonej granicy plastyczności 960 MPa zarówno w pozycji PA, jak i PC. Przedstawiono także wyniki badań metalograficznych makro i mikroskopowych uzyskanych złączy.
PL
W artykule opisano podstawy technologii spawania hybrydowego laser + metoda MAG. Przedstawiono współczesne stanowiska do spawania hybrydowego i przykłady zastosowań przemysłowych tej metody. Opisano zalety procesu spawania hybrydowego w porównaniu do spawania laserowego i łukowego stosowanych jako odrębne procesy spawania.
EN
The article describes the basics of laser-MAG hybrid welding technology. Modern stations for hybrid welding and examples of industrial applications of this method are presented. The advantages of the hybrid welding process as compared to laser and arc welding are described.
PL
W artykule opisano zalety metody spawania hybrydowego laser+MAG. Przedstawiono wyniki badań spawania hybrydowego złączy doczołowych 5 + 5 i 5 + 7 mm ze stali S960QL oraz wyniki badań wytrzymałości, udarności i twardości uzyskanych złączy. Badanie złącza doczołowego blach o grubości 5 + 7 mm wykazało, że spełnia ono wymagania PN-EN ISO 15614-14.
EN
The article describes the advantages of laser + MAG hybrid welding method. The results of research hybrid welding of 5 + 5 and 5 + 7 mm butt joints S960QL steel and strength and toughness tests of obtained joints were presented. Testing of 5 + 7 mm thick butt joints showed that it meets the requirements of the PN-EN ISO 15614-14 standard.
7
Content available remote Welding of High Strength Toughened Structural Steel S960QL
EN
The article discusses the effect of the thermal conditions applied during the MAG welding of steel S960QL and the mutual annealing of runs on the mechanical properties as well as on the macro and microstructure of welded joints made using various values of cooling time t8/5. The research described in the article also involved the comparison of the above-named results with those obtained during a thermal simulation. In addition, the article presents the test results concerning the examination of the coarse and fine-grained areas of the HAZ of welded joints. The test results made it possible to optimise the value of cooling time t8/5 when welding steel S960QL.
PL
Omówiono wpływ warunków cieplnych spawania stali S960QL metodą MAG oraz wzajemnego wyżarzania ściegów na własności mechaniczne oraz makro- i mikrostrukturę złączy spawanych, wykonanych z zastosowaniem różnych czasów chłodzenia t8/5, a następnie porównano te wyniki z rezultatami prób symulacji cieplnej. Przedstawiono również wyniki badań obszaru grubo- i drobnoziarnistego strefy wpływu ciepła złączy spawanych. Wyniki badań umożliwiają optymalizację czasu chłodzenia t8/5 spawania stali S960QL.
PL
W artykule przedstawiono wyniki badań doświadczalnych i teoretycznych niskocyklowej trwałości zmęczeniowej połączeń spawanych stali S960QL stosowanej na stalowe konstrukcje spawane. Badaniom poddano złącza doczołowe, krzyżowe i z żebrem wzdłużnym. Największą trwałością cechuje się złącze doczołowe, a najmniejszą złącze krzyżowe. Zastosowany model obliczeniowy dobrze koresponduje z wynikami doświadczeń oraz pozwala bezpiecznie oszacować trwałość zmęczeniową dla naprężeń nominalnych powyżej 530 MPa.
EN
This paper presents the results of experimental and theoretical research of the low-cycle fatigue strength of welded joints. There was investigated S960QL steel used on steel welded structures. Butt and cruciform joints and joints with a longitudinal rib were chosen for fatigue testing. Fatigue life is the highest in case of the butt joints and it is the lowest for the cruciform. Analytical model corresponds well to experimental results. In addition, the used model makes it possible to estimate safely fatigue life under nominal stresses being above 530MPa.
first rewind previous Strona / 1 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.