Preferencje help
Widoczny [Schowaj] Abstrakt
Liczba wyników
Powiadomienia systemowe
  • Sesja wygasła!

Znaleziono wyników: 3

Liczba wyników na stronie
first rewind previous Strona / 1 next fast forward last
Wyniki wyszukiwania
Wyszukiwano:
w słowach kluczowych:  shear load
help Sortuj według:

help Ogranicz wyniki do:
first rewind previous Strona / 1 next fast forward last
EN
This paper investigates the influence of 1%, 2% and 3% zirconia (ZrO2) nanoparticles to the melting, microstructural and mechanical properties of the Sn58Bi solder. Melting temperatures of 145.11°C, 140.89°C and 143.84°C were attained correspondingly for the 1%, 2% and 3% ZrO2 reinforced Sn58Bi solder. The microstructures especially the spacing between the lamellar structures of the Sn58Bi solder alloy was narrower for 1% ZrO2 added with Sn58Bi solder alloy. The highest and lowest hardness value of 32.28 HV and 27.62 HV was recorded for 1% and 2% ZrO2 additions respectively. Highest shear strength value was noted for the 3% ZrO2 added SnBi/Copper joint with 0.8712 kN, while the lowest value of 0.4380 kN noted for the 1% ZrO2 added SnBi/Copper joint. The presence of small-sized ZrO2 nanoparticles can be seen to be properly dispersed at the solder joint to increase the shear load at maximum joint stress.
PL
W artykule przedstawiono wyniki badań zbrojonych ścian murowych wykonanych z autoklawizowanego betonu komórkowego (ABK). Zasadnicze badania przeprowadzono na 12 elementach ściennych. We wszystkich ścianach zastosowano zbrojenie w postaci stalowych kratowniczek oraz siatek z włókien szklanych. W sześciu modelach wykonano tzw. spoinę jednostronną (zbrojenie zagłębiano w zaprawie), a w kolejnych sześciu spoinę dwustronną (zbrojenie układano w warstwie zaprawy i przykrywano kolejną warstwą). Modele zbadano na ukośne ściskanie zgodnie z normą ASTM E519-81. Wyniki porównano z rezultatami badań ścian niezbrojonych. Wykazano, że stosując spoinę jednostronną, wyraźnie zmniejszono wartości naprężeń rysujących i niszczących w porównaniu ze ścianą bez zbrojenia.
EN
The paper presents the results of tests of reinforced masonry walls made of autoclaved aerated concrete (AAC). The main research was carried out on 12 models. All models were reinforced with truss type steel reinforcement or fiberglass geogrid. In 6 models, a so-called one-sided bed joints was used (reinforcement was embedded in the mortar), and the next in 6 models a two-sided bed joints was used (reinforcement was laid on the mortar joint and covered with another layer of mortar). The models were tested under oblique compression in accordance with ASTM E519-81. The results were compared with the results of tests of unreinforced walls. It was shown that using a one-sided bed joints a clear reduction in the value of crack and destructive stresses in relation to walls without reinforcement.
3
Content available Elastic buckling of vertical cantilevered cylinders
EN
The paper details numerical and experimental study on elastic buckling of cylindrical shells caused by external pressure, a horizontal edge force and combined action of both. The following three geometries of vertical cylinders are considered: (i) circular cylinders, (ii) concentric circular cylinders, and (iii) cylinders with elliptical cross-section. In total, test results on nineteen shells are given. The experimental data is benchmarked against the FE predictions of buckling loads. Good agreement has been obtained between the experimental results and numerical predictions for all tested shells except for buckling of the concentric cylinders loaded by the horizontal edge force. Possible reasons for discrepancies are discussed. The paper offers insight into buckling performance of vertical cylinders subjected to combined loading, and in the case of concentric cylinders, into the interaction between the inner and outer shells. Some of the interaction features, not immediately obvious, are discussed.
PL
Praca przedstawia wyniki obliczeń numerycznych oraz wyniki doświadczalne dotyczące sprężystego wyboczenia powłok walcowych poddanych: (i) działaniu ciśnienia zewnętrznego, (ii) działaniu skupionej siły poprzecznej przyłożonej do końca powłoki, (iii) równoczesnym działaniu obydwu obciążeń. Przedmiotem pracy są natępujące trzy konfiguracje geometryczne: (i) pojedyncza pionowa powłoka walcowa, (ii) układ dwóch pionowych i współosiowych powłok walcowych, (iii) pionowa powłoka walcowa o przekroju eliptycznym. Testy wykonano na 19 powłokach. Otrzymane wyniki doświadczalne porównano z wynikami obliczeń numerycznych. Dobrą zgodność wyni- ków doświadczalnych i teoretycznych otrzymano w przypadku wszystkich konfiguracji z wyjątkiem powłok współosiowych. Praca analizuje zachowanie się pionowych powłok walcowych w warunkach utraty stateczności, a w przypadku powłok współosiowych zajmuje się interakcją pomiędzy wewnętrznym i zewnętrzym walcem. Podano szczegółową analizę wzajemnej interakcji tych powłok.
first rewind previous Strona / 1 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.