1
Content available remote Structure and properties of welded joints of 7CrMoVTiB10-10 (T24) steel
EN
Gas Tungsten Arc butt welded joints of tubes of 7CrMoVTiB10-10 made using bainitic-martensitic P 24-IG filler metal were found to be susceptible to root cracking. This was avoided by using the CMS-IG filler metal and austenitic EPRI P87 filler metal. Detailed coefficient of thermal expansion analysis for both filler metals was performed. Unfortunately, CMS-IG filler metal is characterized by a lower creep rupture strength than P 24-IG. For this reason, the joints were produced by the 141 method with using two filler metals: P 24- IG and EPRI P87. All the welded joints was characterized by the B quality level. Macrostructural, microstructural and hardness data for both welded joints are presented. The standard requirement, < 350 HV10, was marginally not met and was achieved through post weld heat treatment.
first rewind previous Strona / 1 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.