In the present study, Ti6Al4V titanium alloy plates were joined using robotic fiber laser welding method. Pre- and post-weld heat treatments were applied to laser welded joints. After welding stress relieving, solution heat treatment and ageing were also applied to preheated laser welded samples. Effects of heat treatment conditions on microstructural characteristics and mechanical properties of robotic fiber laser welded joints were studied. Aged samples were found to be made of coarsened grains compared to microstructures of non-aged samples. There were increases in ductility and impact toughness of samples applied to ageing increased, while hardness and tensile strength of non-aged samples were higher. The highest value for tensile strength and for impact toughness in welded samples have been identified as 840 MPa and 27 J, respectively. Fractures in tensile test samples and base metal impact test samples took place in the form of ductile fracture, while laser welded impact test samples had fractures in the mode of intergranular fractures with either a quasi-cleavage type or tear ridges. EDS analysis carried out for all heat treatment conditions and welding parameters demonstrated that major element losses were not observed in base metal, HAZ and weld metal.
first rewind previous Strona / 1 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.