In the environment in which the renovation plaster mortars are exposed to moisture, followed by the crystallization of salt, their required durability is obtained by aeration. Aeration increases the porosity and resistance to salt crystallization, significantly changing the properties of plaster mortars. The paper presents the results of research on the influence of aeration and hydrophobizing admixtures on the porosity and pore size distribution in renovation plaster mortars. It was found that when aeration admixtures are used together with hydrophobizing admixtures, there may be problems with maintaining the proper degree of aeration of the mixture.
first rewind previous Strona / 1 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.