In this paper, to produce a saleable magnetite concentrate with a sulfur level below 0.20% and recover sulfur concentrate, flotation and magnetic separation tests were undertaken. Results showed that the optimum conditions of flotation were established as follows: grinding fineness of 90% particles passing 0.074mm, pH 6, 400 g/t of CuSO4, and 400 g/t of combined collectors. Under these conditions and magnetic separation, S grade of the magnetite concentrate was reduced from 3.20% to 0.18%, and the Fe grade improved from 57.29% to 71.17%. At the same time a sulfur concentrate with S grade of 38.05% and recovery of 91.32% was also obtained. The XPS results showed that the addition of CuSO4 benefited the formation of hydrophobic Sn2-/S0 and Cu+-xanthate, enhancing pyrrhotite floatability. The flotation separation efficiency could be enhanced using a mixture of collectors, and collector mixture demonstrated three synergetic effects, namely enhanced S recovery, improved adsorption behavior of the collectors and enhanced hydrophobicity of pyrrhotite surface.
EN
The utilization of seawater in mineral flotation is the future development trend because of the shortage of fresh water resources. However, at present, the flotation behavior and mechanism of galena in seawater are not clear. Therefore, this paper comprehensively carried out the effect mechanism of seawater on the flotation of galena. Micro-flotation results illustrated that the recovery of galena was higher in deionized water than that in 5×10-2 mol/L MgCl2 solution, 1×10-2 mol/L CaCl2 solution and seawater. Contact angle determination and Zeta potential distribution measurements showed that hydrophilic substances adsorbed on the surface of galena under alkaline conditions. X-ray photoelectron spectroscopy (XPS) analysis further indicated that these substances were hydroxides precipitates, carbonate precipitates and hydroxyl complexes formed by divalent magnesium and calcium ions, which prevented the adsorption of collector on mineral surface. As a result, the galena recovery declined in 5×10-2 mol/L MgCl2 solution, 1×10-2 mol/L CaCl2 solution and seawater.
first rewind previous Strona / 1 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.