EN
Poly(hexamethylene 2,5-furanate) (PHF) was obtained by melt polycondensation. The process was carried out at temperatures of 230, 235 and 240°C. It has been shown that the selection of the optimal parameters of the synthesis process leads to the obtaining of biomaterials of high molecular weight, and thus better mechanical and thermal properties. The relationship between the molecular weight and the mobility of polymer chains, and consequently the temperature of phase changes and mechanical properties, was determined.
PL
Poli(2,5-furanian heksametylenowy) (PHF) otrzymano metodą polikondensacji w stanie stopionym. Proces prowadzono w temperaturze 230, 235 i 240°C. Wykazano, że dobór optymalnych parametrów procesu syntezy prowadzi do otrzymania biomateriałów o dużej masie cząsteczkowej, a tym samym lepszych właściwościach mechanicznych i termicznych. Określono zależność między masą cząsteczkową a ruchliwością łańcuchów polimerowych, a w konsekwencji temperaturą przemian fazowych i właściwościami mechanicznymi.