Glasses in the Na2O–B2O3–SiO2–Fe2O3 system with a constant SiO2 content 70 mol% were synthesized using conventional melting in platinum crucibles in SiC-furnace in air. After synthesis and annealing, glasses were heat treated at 550°C for 96–144 hrs to promote phase separation. A tentative region of phase separation for this temperature was outlined. X-ray powder diffractometry results showed three iron-containing phases (Fe3O4, FeSiO3 and β-Fe2O3) forming in the investigated glasses with magnetite being the main phase as it is observed in most of the glasses. Chemical durability studies showed that compositions of phase-separated glasses suitable for synthesis of porous glasses, both iron-free and iron-containing lie in between 4 and 8 mol% of Na2O. Bulk samples of porous glasses were obtained within the chosen region having the following parameters: specific surface area 40–185 m2/g, porosity 30%–45%, pore diameter 3–14 nm. The parameters of porous structure of iron-containing porous glasses are of the same order of magnitude as the porous glass used for the multiferroic nanocomposite synthesis.
first rewind previous Strona / 1 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.