The study discussed in the article aimed to analyse the effect of the peening of each bead on properties of butt joints made of steel S960QL and welded using the robotic MAG welding method (135) and a ceramic backing strip. In addition, the objective of the study was to identify the effect of the peening treatment on the level of stresses. The analysis involved the comparison of three butt joints in the post-weld state (i.e. only after welding), subjected to peening (preceded by welding) and to post-weld heat treatment (stress relief annealing). The purpose of the high-frequency peening (90 Hz) of each bead was to reduce stresses in the welded joint by introducing tensile stresses into the latter. The study-related tests involved the use of a Weld Line 10 air hammer (PITEC GmBH). The tests required by the EN ISO 15614-1 standard were supplemented with measurements of stresses involving the use of the Barkhausen effect (based on a testing procedure proposed by the technology provider, i.e. the NNT company). The tests revealed that the performance of high-frequency peening following the making of each bead did not lead to the obtainment of negative results of all the tests required during welding procedure qualification concerning the plate made of steel S960QL (in comparison with test plates after welding and stress relief annealing). The interpass peening of the weld face and that of the HAZ reduced post-weld residual stresses at a distance of 15 mm away from the joint axis (in comparison with stresses measured in the specimens after welding). The test results justified the positive assessment of peening in respect of tensile stress reduction in the fusion line area and in the HAZ.
PL
Celem badań była analiza wpływu przekuwania każdego ze ściegów na własności złącza doczołowego ze stali S960QL spawanego z wykorzystaniem podkładki ceramicznej na stanowisku zrobotyzowanym metodą 135 (MAG) oraz określenie wpływu przekuwania na poziom naprężeń. Analiza ta oparta była na porównaniu trzech złączy doczołowych w stanie po spawaniu, z przekuwaniem każdego ze ściegów oraz z przeprowadzoną pospawalniczą obróbką cieplną – wyżarzanie odprężające. Przekuwanie o wysokiej częstotliwości (90 Hz) każdego wykonanego ściegu miało na celu zmniejszenie naprężeń w złączu spawanym poprzez wprowadzenie do niego naprężeń rozciągających. Został do tego wykorzystany młot pneumatyczny Weld Line 10 firmy PITEC GmBH. Poza badaniami wymaganymi przez normę EN ISO 15614-1 wykonane zostały pomiary naprężeń z wykorzystaniem efektu Barkhausena w oparciu o procedurę badawczą dostawcy technologii – Firmę NNT. Przeprowadzone badania wykazały, że zastosowanie przekuwania o wysokiej częstotliwości po wykonaniu każdego ściegu nie wpłynęło na negatywny wynik wszystkich badań wymaganych podczas kwalifikowania technologii spawania blachy S960QL w porównaniu do płyt próbnych w stanie po spawaniu i po obróbce cieplnej – wyżarzanie odprężające. Przekuwanie międzyściegowe lica spoiny i SWC spowodowało redukcję naprężeń szczątkowych po spawaniu w odległości 15 mm od osi złącza w porównaniu do wyniku pomiaru naprężeń dla próbki w stanie po spawaniu. Pozwala to na pozytywną ocenę przekuwania w kontekście redukcji naprężeń rozciągających w obszarze linii wtopienia i SWC.
EN
The article presents today's possibilities of modifying the fatigue strength of welded joints made in steel S700MC using the high frequency impact treatment (HiFIT). Research-related fatigue tests involved MAG-welded butt joints, T-joints with two-sided fillet welds as well as joints with a longitudinal rib and a girth fillet weld. The tests required the adjustment of appropriate parameters of the HiFIT and the performance ot' the above-named treatment in relation to the half of previously made joints. The article presents results of fatigue tests of joints after welding and after the HiFIT. The research also included the development of fatigue characteristics and the calculation of fatigue categories FAT, constituting the basis for the design of structures exposed to fatigue (in accordance with European standards). The results obtained in the tests unequivocally demonstrated the possibility of increasing the fatigue strength of welded joints made in steel S700MC by applying the HiFIT, with the level of fatigue strength modification depending on the type of a joint.
PL
Przedstawiono współczesne możliwości modyfikacji wytrzymałości zmęczeniowej złączy spawanych, wykonanych ze stali S700MC poprzez młotkowanie z dużą częstotliwością techniką HiFIT (z ang. High Freąuency Impact Treatment). Do badań zmęczeniowych wykonano za pomocą spawania metodą MAG złącza doczołowe, złącza teowe ze spoinami pachwinowymi dwustronnymi ora/, złącza z żebrem podłużnym i spoiną pachwinową obwodową. Dobrano parametry dla techniki młotkowania z dużą częstotliwością (HiFTT) oraz wykonano taką obróbkę na połowie uprzednio wykonanych złączy. Przedstawiono wyniki badań zmęczeniowych złączy w sta¬nie po spawaniu oraz w stanie po obróbce udarowej techniką HiFIT. Opracowano charakterystyki zmęczeniowe oraz obliczono kategorie zmęczeniowe FAT, stanowiące podstawę do projektowania konstrukcji narażonych na zmęczenie wg norm europejskich. Uzyskane wyniki badań jednoznacznie wskazują, że można zwiększyć wytrzymałość zmęczeniową złączy spawanych stali S700MC stosując technikę młotkowania HiFIT, a stopień tej modyfikacji zależy od rodzaju złącza.
PL
W pracy przedstawiono koncepcję zastosowania metody prądów wirowych, jako szybkiej, ekologicznej i nieniszczącej metody pomiarowej, do określania jednokierunkowego rozkładu naprężeń normalnych własnych, wywołanych kulowaniem strumieniowym warstwy wierzchniej ferromagnetyku. Badania przeprowadzono na 48 próbkach testowych ze stali 40 HM. Przedstawiono podstawy fizyczne metody prądów wirowych, cel, zakres i opis przeprowadzonych badań doświadczalnych.
EN
The study presents a concept of using the eddy current method, being a fast, ecological and nondestructive measuring method, for determination of uniavial residual normal stresses. These stresses are caused by shot peening onto the surface layer of a ferromagnetic material. The experiments have been performed on 48 samples made of 40HM steel. The samples have the form of flat beams of a rentangular cross-section.
4
Content available remote The investigation of chromium coatings pneumatic ball peening possibilities
EN
In the article the results of initial researches of chromium coating pneumatic ball peening possibilities are presented. The chromium layers of 50 µm placed on the 40H steel base of 230 HB hardness have been examined. Different times of processing, various degree of the peening traces covering and different stereometrical features of ball-peened surfaces have been achieved.