Ograniczanie wyników
Czasopisma help
Autorzy help
Lata help
Preferencje help
Widoczny [Schowaj] Abstrakt
Liczba wyników

Znaleziono wyników: 41

Liczba wyników na stronie
first rewind previous Strona / 3 next fast forward last
Wyniki wyszukiwania
Wyszukiwano:
w słowach kluczowych:  nonwovens
help Sortuj według:

help Ogranicz wyniki do:
first rewind previous Strona / 3 next fast forward last
EN
The study involved laminated nylon and viscose nonwovens, both perforated and non-perforated, with a view to using them for packaging of powders in mineral warmers. The nonwovens were examined in terms of morphology as well as tensile strength in dry and wet states. Thermal properties were determined by differential scanning calorimetry. Dynamic mechanical analysis was carried out in a broad range of temperatures. Surface wettability and water vapor permeability were assessed. The findings were analyzed to determine the utility of the studied materials as mineral warmer packaging materials in cold work or living environments.
EN
Fiber injection molding is an innovative approach for the manufacturing of nonwoven preforms but products currently lack a homogeneous fiber distribution. Based on a mold-integrated monitoring system, the uniformity of the manufactured preforms will be investigated. As no universally accepted definition or method for measuring uniformity is accepted yet, this article aims to find a suitable uniformity index for evaluating fiber injection molded nonwovens. Based on a literature review, different methods are implemented and used to analyze simulated images with given distribution properties, as well as images of real nonwovens. This study showed that quadrant-based methods are suitable for evaluating the basis weight uniformity. It has been found that the indexes are influenced by the number of quadrants. Changes in sample size do not affect the indexes when keeping the quadrant number constant. The quadrants-based calculation of the coefficient of variation showed the best suitability as it shows good robustness and steady index for varying degrees of fiber distribution.
EN
Nonwovens are one of the most versatile textile materials and have become increasingly popular in almost all sectors of the economy due to their low manufacturing costs and unique properties. In the next few years, the world market of nonwovens is predicted to grow by 7%–8% annually (International Nonwovens & Disposables Association [INDA], European Disposables and Nonwovens Association [EDANA], and Markets and Markets). This article aims to analyze the most recent trends in the global export and import of nonwovens, to present two case studies of Polish companies that produce them, and to present one special case study of the market of nonwoven geotextiles in China and India, which are the Asian transition economies among the BRICS countries (Brazil, Russia, India, China, and South Africa).
4
Content available remote Influence of Technology Process on Responsiveness of Footwear Nonwovens
EN
Nonwovens represent a part of technical textiles that are used for clothing (“cloth tech”). Nonwovens are also used in the footwear industry mainly for functional purposes, where the aesthetic properties are not of great importance. They are mainly used for support and reinforcement of footwear. All three groups of textiles are used for footwear, i.e. woven fabrics, knitted fabrics and nonwovens that are produced directly from fibres, yarns or threads mainly from chemical fibres and in a small proportion from natural fibres. Footwear textiles need to have good mechanical properties (at compressive loading), abrasion resistance, permeability properties and heat resistance. These properties are in close connection with the nonwoven structure or composite materials. The basic intention of the presented research was to analyse the influence of the technology process on nonwovens for footwear responsiveness. Analysed footwear nonwovens in the presented research were on one side coated but on the other side consisted of a two-layer laminate. For this purpose, two different technological processes were used (coating and lamination). The results of the presented research showed that laminated samples express higher elastic recovery at compressive loading than coated samples. The treatment does not have an important influence on elastic recovery at compressive loading. Laminated samples express higher water permeability and lower absorption of water than coated samples, even after 24 hours of treatment in distilled water and compressive loading. The treatment of specimens in distilled water for 24 hours and compressive load of 789.6 N does not have an important influence on elastic recovery at compressive loading, water vapour permeability, air permeability and absorption of analysed samples. Air permeability could not be measured on coated samples.
EN
Tetraphenyl phosphonium-modified organoclay (TPP-Mt) was prepared by modifying montmorillonite-rich Thai bentonite via ion exchange. TGA results revealed that TPP-Mt possessed high thermal stability, where degradation occurred at a temperature range of 418-576°C. The obtained TPP-Mt/PP nanocomposites exhibited degradation at higher temperatures than PP (410-420°C vs. 403°C). Fibers of different cross-sectional shapes (circular, circular hollow, and cross) containing 1, 2 and 3%wt TPP-Mt were prepared and characterized. Nonwovens of 3%wt TPPMt/PP fibers were fabricated for flame retardant test. From results, nonwovens of TPP-Mt/PP fibers exhibited self-extinguishing characteristic and the areas of burning were less than that of PP nonwoven (14.5-31.6% vs. 95.6%). Nonwovens of cross-shaped fibers showed the best flame retardant property, followed by those of circular hollow and circular fibers. The flame retardant properties observed in nonwovens were explained due to the inter-fiber spaces between cross-shaped fibers and center hole in circular hollow fibers, which could trap initiating radicals inside, thus reducing flame propagation. In addition, large surface area in cross-shaped fibers could help in increasing the flame retardant effectiveness due to more exposure of TPP-Mt particles to the flame. Knowledge obtained in this study offered an approach to produce flame retardant nonwovens via a combination of modified organolcay and fiber shape.
EN
This study analyses tests influencing the selection of nonwovens for water absorbing geocomposites. The task of the nonwoven is to capture water infiltrating into the soil and to direct it to the superabsorbent located inside. The best results in the tests of water permeability (88 mm/s) and water absorption (1116.85 g/m2) were obtained for nonwoven of the lowest surface weight - 112.8 g/m2 and the largest average pore diameter - 206.5 μm. The lowest water absorption capacity (478.91 g/m2) and the smallest thickness changes under a load (19.3%) was noted in needle-punched nonwoven that had been subject to the calandering process. For one nonwoven, the presence of other significant fractions was noted, which proves that it is heterogeneous. For nonwovens applied in the unsaturated zone, not only water permeability should be taken into account, but also the size and fraction distribution of pores, in order to avoid breaking the continuity of capillaries.
PL
W pracy przedstawiono badania właściwości włóknin, jako osłon do geokompozytów sorbujących wodę. Zadaniem włókniny jest przechwycenie filtrującej wody i przekazanie do znajdującego się wewnątrz superabsorbentu. Najlepsze wyniki w badaniu wodoprzepuszczalności (88 mm/s) i wodochłonności (1116.85 g/m2) uzyskano dla włókniny o najniższej masie powierzchniowej 112.8 g/m2 i największej średniej średnicy porów 206.5 μm. Włókninę 100% PET kalandrowaną cechowała niska wodochłonność (478.91 g/m2) i niewielkie zmiany grubości pod obciążeniem (19.3 %). Dla jednej z włóknin zanotowano obecność innych istotnych frakcji co świadczy o jej niejednorodności. W przypadku zastosowania włókniny w strefie aeracji należy zwracać uwagę nie tylko na wodoprzepuszczalność, ale i rozmiary oraz rozkład frakcyjny porów, aby nie przerwać ciągłości kapilar.
EN
A biofunctionalization of nonwoven fabrics was carried out with 0.1 - 4 wt.% of copper silicate. Polypropylene (PP), polyethylene (PE) and biodegradable polymers [poly(lactic acid) (PLA), polyhydroxyalkanoates (PHA)] or their mixtures were used as polymer components. Mostly liquid oligomers of ethylene glycol (PEG) or copolymers of ethylene oxide and propylene oxide (2.5 - 5 wt.%) were applied as plasticizers. New composite nonwovens containing CuSiO3 were prepared by the melt-blown technique [1]. They showed very good antibacterial and antifungal properties against colonies of gram-negative bacteria (Escherichia coli), gram-positive bacteria (Staphylococcus aureus) and a yeast fungus (Candida albicans). Nonwovens containing ≥ 0.5 wt.% of CuSiO3 can be used, e.g. as hygienic and bioactive filter materials in air-conditioning systems. The application of PLA and PHA affects the ability of these hybrid nonwovens to biologically decompose. DSC analysis indicated that the incorporation of additives in PLA and PP nonwovens significantly affected their melting and crystallization processes.
PL
Badano proces biofunkcjonalizacji włóknin za pomocą 0,1 - 4 % wag. krzemianu miedzi. Jako komponenty polimerowe zastosowano polipropylen (PP), polietylen (PE) i polimery biodegradowalne [polilaktyd (PLA) i polihydroksyalkaniany (PHA)] lub ich mieszaniny. Jako ciekłe plastyfikatory stosowano głównie oligomery tlenku etylenu (PEG) lub jego kopolimery z tlenkiem propylenu (2,5-5 % wag.). Nowe kompozytowe włókniny zawierające CuSiO3 otrzymywano metodą melt-blown – przez wytłaczanie i rozdmuchiwanie stopionych kompozycji polimerowych [1]. Wykazywały one bardzo dobre właściwości antybakteryjne (wobec szczepów bakterii gram-ujemnych Escherichia coli i gram-dodatnich Staphylococcus aureus) oraz antygrzybiczne (wobec grzyba Candida albicans). Włókniny zawierające ≥0.5% wag. CuSiO3 mogą być stosowane np. jako bioaktywne materiały higieniczne i filtracyjne w układach klimatyzacji. Zastosowanie PLA i PHA zwiększa podatność tych hybrydowych włóknin na rozkład biologiczny. Analiza termiczna metodą DSC wykazała, że dodatek CuSiO3 i plastyfikatorów do włóknin PLA i PP znacznie wpływa na przebieg ich procesów topnienia i krystalizacji.
EN
Poly(lactic acid) (PLA) nonwoven and PLA (85 wt %)/P(3HB) (15 wt %) [P(3HB) — poly(3-hydroxybutyrate)] composite nonwoven were obtained using the melt-blown technique. The thermal properties, physical-mechanical parameters, specific surface area and susceptibility to hydrolytic degradation were studied for the obtained nonwovens. DSC analysis indicated noticeable changes in the polymers structure during melt-blowing. The addition of P(3HB) to PLA nonwoven generally downgraded the physical-mechanical properties and caused specific surface area decrease. Both analyzed nonwovens were more susceptible to hydrolysis in alkaline than neutral medium.
PL
Techniką melt-blown otrzymano włókninę z poli(kwasu mlekowego) (PLA) oraz włókninę kompozytową PLA (85 % mas.)/P(3HB) (15 % mas.). [P(3HB) — poli(3-hydroksybutanian)]. Zbadano właściwości termiczne, parametry fizykomechaniczne, powierzchnię właściwą i podatność na degradację hydrolityczną uzyskanych włóknin. Termogramy DSC wykazały zmiany w strukturze polimerów na skutek przetwórstwa techniką melt-blown. Dodanie P(3HB) generalnie pogorszyło parametry fizykochemiczne włókniny z PLA i spowodowało zmniejszenie powierzchni właściwej. Badane włókniny hydrolizowały szybciej w środowisku zasadowym niż w obojętnym.
EN
The paper presents preliminary results of simulation studies evaluating moisture absorption from the air that indicate the possibility of applying a superabsorbent polymer (SAP) in the construction of protective footwear insoles. The performance of different types of nonwovens was tested in terms of moisture absorption from air of high relative humidity in a climatic chamber and on a thermal foot model. The tests simulated the temperature and humidity conditions that occur inside all-rubber protective footwear. It was found that insoles containing SAP dehumidified the air more effectively than either insoles not containing SAP or traditional wool felt insoles. The tests showed a new application potential of absorbent materials in protective footwear with a view to improving hygienic comfort during use.
PL
Artykuł prezentuje wstępne wyniki badań modelowych związanych z oceną sorpcji wilgoci z powietrza i wskazujących na możliwość zastosowania superabsorpcyjnego polimeru (SAP) w konstrukcji wkładek do obuwia ochronnego. Ocenę wydajności włóknin, pod względem pochłaniania wilgoci z powietrza o dużym nasyceniu parą wodną, przeprowadzono w laboratorium w komorze klimatyzacyjnej oraz z użyciem termicznego modelu stopy. Podczas badania wkładek zamodelowano warunki temperaturowo-wilgotnościowe jakie panują wewnątrz użytkowanego obuwia ochronnego całkowicie wykonanego z gumy. Zaobserwowano, że wkładki zawierające SAP, powodowały osuszanie powietrza (spadek wilgotności względnej wewnątrz obuwia ochronnego wykonanego z gumy) w porównaniu do wkładek niezawierających SAP oraz tradycyjnie stosowanego filcu wełnianego. Badania wskazują nowy kierunek aplikacji materiałów chłonnych w obuwiu ochronnym nóg do poprawy komfortu higienicznego podczas ich użytkowania.
PL
W artykule omówiono dwie technologie produkcji włóknin filtracyjnych oraz ich wpływ na właściwości elektrostatyczne. W sposób zwięzły opisano proces wytwarzania włóknin: igłowano – wykurczanej i klejonej. Przedstawiono wyniki pomiarów wartości czasu połowicznego zaniku ładunku elektrostatycznego oraz przedstawiono charakterystyki ładowania/rozładowania włóknin pod wpływem przepływu powietrza. Celem doświadczeń było poznanie wpływu struktury materiału (gęstość i układ włókien) na szybkość odprowadzania ładunku elektrostatycznego.
EN
This article discusses two producing nonwoven filtration technologies and their impact on the electrostatic properties. Concisely describes the process of producing nonwovens: needling – shrinkage and glued. Presents the results of measurements of the half-decay test of electrostatic charge.
11
Content available In-Compost Biodegradation of PLA Nonwovens
EN
Presented in this work are the results of an investigation into the biodegradation of selected nonwoven materials made of commercial poly[(DL)-lactide] – PLA 6252D supplied by Nature Works® LLC, USA. The biodegradation was examined under laboratory conditions, simulating composting by the mass-loss method at constant process parameters: temperature t = 58 ± 2 °C, pH 7 and inoculum humidity W = 52.6%. The nonwovens examined, with a surface density of about 60 g/m2, revealed a varied crystallinity degree in the range of 10.4 - 35.6% and fibre diameter of 8.2 - 10.9 μm. The nonwovens were formed by the spun-bond method from a melt at 211 - 213 °C on a laboratory stand. The commercial PLA 6252D was also examined. The polymer PLA 6252D and nonwoven materials made thereof are entirely biodegradable in the research environment applied, and after 16 weeks of biodegradation weight loss in the materials reaches 100%.
PL
Rozwój wiedzy w obszarze ochrony środowiska oraz rozporządzenia unijne stały się impulsem do ciągłego poszukiwania nowych materiałów, które będą degradowalne w środowisku naturalnym, a tym samym wzrastającą potrzebę wykorzystywania innowacyjnych metod badań ich biorozkładu. W artykule przedstawiono wyniki badań biorozkładu wybranych materiałów włókninowych wytworzonych z komercyjnie dostępnego poli[(DL)-laktydu)] – PLA o symbolu 6251D (Nature Works® LLC, USA). Badania prowadzono w symulowanych warunkach kompostowania laboratoryjnego, metodą wyznaczania ubytku masy w temperaturze 58 ± 2 °C, wilgotności podłoża badawczego 52.6% i przy odczynie środowiska pH 7. Włókniny poddane ocenie biodegradowalności o masie powierzchniowej ok. 60g/m2 charakteryzowały się różnymi stopniami krystaliczności w zakresie 10.4 - 36.5% i średnicami włókien w przedziale 8.2 - 10.9 μm. Formowano je ze stopu techniką spun-bonded w zakresie temperatur 211 - 213 °C. Badaniom biodegradacyjnym poddano również handlowy polimer PLA 6251D.
EN
Investigations focused on physico-chemical modifications of a polyethylene terephthalate (PET) nonwoven fabric fibre surface. To improve the adhesive properties of textile products towards TiO2, their surface was treated in low-temperature plasma (cold plasma). Plasma treatment of PET fabrics was performed in carbon dioxide and/or argon pressure. Potential changes in the chemical structure of polyester fabric can be caused by the following: a homolytic splitting of the ester bonds, a release of volatile degradation products (mainly CO and CO2), a cross-linking, reactions of macro radicals [alkyl (CH2-CH2~) and phenyl (C6H4~)] with oxygen, and a subsequent formation of hydroxy-aromatic rings. Experimental investigations confirmed the fact of modification of the chemical structure of the PET surface caused by plasma treatment of the fibre surface.
PL
Badania dotyczyły fizykochemicznej modyfikacji powierzchni włóknin z poli(tereftalanu etylenu) (PET). W celu polepszenia właściwości adhezyjnych włóknin względem TiO2 ich powierzchnia była modyfikowana działaniem plazmy niskotemperaturowej (cold plasma). Obróbkę plazmą włóknin przeprowadzono w atmosferze dwutlenku węgla lub argonu. Autorzy zakładają, że obserwowane zmiany w strukturze chemicznej badanych włóknin mogą być spowodowane oddziaływaniem plazmy na powierzchnię włókniny, indukującym przebieg procesów: hemolitycznego rozszczepienia wiązań estrowych, uwolnienia lotnych produktów rozkładu (głównie CO i CO2), sieciowania przebiegu reakcji makro-rodników [alkilowych ( CH2- CH2 ~) i fenylowych ( C6H4 ~)] z tlenem i powstawaniem hydroksy-aromatycznych pierścieni. Zmiany w strukturze chemicznej powierzchni włóknin zostały potwierdzone eksperymentalnie.
EN
In this paper, an intelligent model of heat and moisture propagation in light nonwoven fabrics was designed by conversion of a numerical propagation model of a partial differential equation to a feed forward propagation neural network. Propagation coefficients of heat and moisture transfers were estimated from the intelligent model for nonwoven samples containing hydrophilic natural and hydrophobic synthetic fibres. The results presented that the error of the model is acceptable less than 4.7% and 7.9% for estimation of heat and moisture diffusivity coefficients, respectively. The Anova test revealed that while fibre type and fabric thickness affected heat and moisture transfer through the fabric, factors such as surface mass density, heat and the moisture transfer constant were not significant. Also it was found that the optimum transfer rate was observed in the case of samples containing viscose or a viscose and polypropylene blend in the ratio of 60%:40%, respectively.
PL
Inteligentny model przepływu wilgoci i ciepła przez włókniny o małej masie powierzchniowej został opracowany dla zasilania sztucznych sieci neuronowych na podstawie modelu numerycznego cząstkowych równań różniczkowych. Badano włókniny zawierające włókna hydrofobowe i hydrofilowe. Stwierdzono, że dokładność modelu jest akceptowalna dla modelu rozpatrywanych włókien. Test Anova wykazał, że rodzaj włókna i grubość włókniny wpływają na przepływ ciepła i wilgoci przez włókninę. Stwierdzono, że dla próbek zawierających wiskozę lub mieszankę wiskozy i polipropylenu w stosunku 60%:40% uzyskano optymalne prędkości przepływu.
EN
Solution viscosity can be regarded as the most important factor in determining the morphology of the product obtained in electrospinning. Viscosity can be adjusted for a given solution by tuning the solution temperature or by adding fillers to the solution prepared. The electrospinning of PLA solution was performed at a temperature ranging from 25 to 100 °C to determine the effects of temperature on fiber morphology. For the solution of sufficiently high entanglement density (i.e., 20 wt%), the as-spun fiber diameter was in the range of 330 ± 20 nm because the electrospinning was conducted at elevated temperatures. In contrast, for the solution without sufficient entanglement density (i.e., 13 wt%), the solution entanglement density was enhanced by the addition of fillers, which caused the as-spun fibers to become smooth. The fiber diameter obtained was in the range of 90 ± 10 nm. By varying the solution temperature, the chain entanglement status existing in the solution remained intact. In contrast, the chain entanglement density could be enhanced by the addition of fillers. However, both temperature and fillers significantly altered the solution viscosity. Therefore a complete understanding of the temperature and filler effect on the solution and electrospinning gave rise to a feasible route for manipulating the as-spun fiber diameter.
PL
Lepkość roztworu można uznać za najważniejszy czynnik dla określenia morfologii produktu otrzymanego w procesie elektroprzędzenia. Lepkość może być dostosowana do danego roztworu przez regulację temperatury roztworu lub przez dodanie wypełniaczy do przygotowanego wcześniej roztworu. Elektroprzędzenie roztworu PLA prowadzono w zakresie temperatur od 25 do 100 °C w celu wyznaczenia wpływu temperatury na morfologię włókien. Przy roztworach o wysokim stopniu splatania łańcuchów polimeru (np., 20 wt%), dzięki prowadzeniu procesu przędzenia w wysokiej temperaturze udało się zredukować średnicę włókien do 330 ± 20 nm. Przy mniejszym stopniu splatania łańcuchów polimeru (np. 13 wt%) dodawano wypełniacze i uzyskiwano średnice włókien 90 ± 10 nm. Pełne zrozumienie wpływu temperatury i zastosowanych wypełniaczy na roztwór i proces elektroprzędzenia jest ważny dla otrzymywania określonej średnicy przędzonych włókien.
EN
Development in the field of electronic circuit technology has resulted in the miniaturisation of radio transceiver integrated circuits. This gives the possibility of embedding radio transceivers directly into a garment. The product obtained (garment + electronic transmitter) can have new functions that significantly expand the basic functionality of textiles. To combine radio equipment with clothing, the electronic elements should be as flexible and lightweight as possible. The textile antennas that are being developed in many research institutions have constructions that combine high performance in radio communication together with a flexible and lightweight construction. The authors of this paper propose a vee-type textile antenna that can be used for wireless transmission in a 2.4 GHz band. The concepts of the electrical design of this antenna as well as the antenna structure and design methodology were discussed. The aim of this paper is to present textile materials and textile manufacturing technologies that were used for this design.
PL
Przygotowano ciecz gęstniejącą pod wpływem ścinania (STF) i zbadano jej właściwości reologiczne. Tkaniny z włókien szklanych były nasycane roztworem STF/etanol dla przygotowania kompozytów. Morfologię kompozytów badano za pomocą skaningowej mikroskopii elektronowej. Prowadzono quasi-statyczne badania na przebicie na tkaninach szklanych nienasączonych oraz na opracowanych kompozytach za pomocą noża o specjalnie zaprojektowanej konstrukcji. Niezależnie od testów porównawczych badano również mechanizm przebicia.
EN
Results of research in the preparation of nonwovens containing chitosan salts used as a binding agent are presented. The supermolecular structure of chitosan salts was assessed by the use of wide angle X-ray scattering (WAXS). The crystallinity degree and crystal dimensions were examined. Morphology was assessed by means of optical microscopy.
PL
Praca dotyczy selekcji soli chitozanu dla łączenia optymalnych warstw włókninowych struktur opatrunków medycznych. Jako włókninę stosowano runo z włókien wiskozowych i polipropylenowych. W artykule przedstawiono badania dotyczące otrzymywania włóknin z runa włókninowego z udziałem modyfikowanych soli chitozanu jako środka wiążącego. Strukturę nadcząsteczkową soli chitozanu oceniono przy wykorzystaniu metody szerokokątowego rozpraszania promieni rentgenowskich (WAXS): zbadano stopień krystaliczności i rozmiary krystalitów. Strukturę morfologiczną natomiast oceniono przy wykorzystaniu mikroskopu optycznego.
17
Content available remote Modification of PLA Fibres with Bioacceptable Hydrophilic Polymers
EN
This paper presents methods for the preparation of systems composed of polylactide (PLA) nonwoven and selected bioacceptable polymers such as poly(acrylic acid) (PAA), Carbopol, poly(N,N-dimethylaminoethyl methacrylate), (PDAMA), alginic acid (AlgA), chitosan (CHN) and gelatin. The modification was performed by the method of padding or entrapping. The possibility of further modification by the layer-by-layer (LbL) deposition method was also examined. The moisture absorption and water retention by the systems obtained were determined. Changes in the surface electric charge under the influence of the layers successively deposited and the biological activity of selected systems were examined.
PL
Polilaktyd (PLA) jest biodegradowalnym i bioresorbowalnym alifatycznym poliestrem, który znalazł liczne zastosowania między innymi w medycynie i farmacji. Jego niekorzystną cechą jest mała higroskopijność, co ma istotne znaczenie w produkcji wyrobów medycznych i środków higienicznych. W celu poprawy właściwości, głównie hydrofilności tego polimeru, w pracy stosowano funkcjonalizację jego powierzchni m.in. poprzez szczepienie monomerami winylowymi, zakleszczanie polimerów hydrofilowych, nanoszenie warstw polikompleksów oraz reakcji grup końcowych. Obecność zaszczepionego lub zakleszczonego polimeru na włókninie potwierdzono metodą spektrometrii w podczerwieni. Wytworzoną ilość grup karboksylowych w warstwie wierzchniej modyfikowanych włóknin oznaczano metodą miareczkowania potencjometrycznego. Na włókninę z pierwszą warstwą zawierającą grupy karboksylowe nakładano metodą layer-by-layer warstwy polielektrolitów zasadowych takich jak poli(chlorowodorek alliloaminy), poli(4-winylopirydyny) lub poli(metakrylanu N,N-dimetyloaminoetylu) z warstwami polielektrolitu kwasowego tj. poli(kwasu akrylowego) lub poli(styrenosulfonianu sodu). Na podstawie otrzymanych wyników, stwierdzono zmianę niektórych właściwości modyfikowanych włókien takich jak: wybarwialność, sorpcja wilgoci, ładunek elektryczny.
EN
This article presents the influence of the formation temperature of nonwovens from biodegradable aliphatic polyesters (trade name Bionolle) on their structure and mechanical properties. Nonwovens were produced by spun-bonded technique at a laboratory installation at IBWCh, changing one of the process parameters i.e. the temperature of the polymer. Basic parameters of the polymer were evaluated in order to determine the spun-bonded process condition. Phase transition temperature - glass transition temperature (Tg), -melting point (Tm) and mass flow index (MFI)were assessed. The effect of manufacturing conditions on the properties of the nonwovens obtained was identified on the basis of the analysis of their mechanical parameters, the sorption rate, crystallinity and compost biodegradation rate. It has been shown that 238 °C is the best formation temperature to produce nonwovens with good mechanical properties and at the same time accessible biodegrability.
PL
W artykule przedstawiono badania wpływu temperatury formowania na właściwości mechaniczne i strukturę włóknin otrzymywanych z biodegradowalnego poliestru alifatycznego (nazwa handlowa Bionolle). Włókniny wyprodukowano metodą spun-bonded na instalacji laboratoryjnej IBWCh. Ocenione zostały podstawowe parametry polimeru, które służyły do określenia warunków formowania włóknin, są to między innymi temperatury przemian fazowych: temperatura zeszklenia (Tg), temperatura topnienia (Tm) i masowy indeks płynięcia (MFI). Wpływ warunków wytwarzania na właściwości włóknin został określony na podstawie analizy ich parametrów mechanicznych, szybkości sorpcji, krystaliczności i biodegradacji w środowisku kompostowym. Wykazano, że temperatura wytwarzania włóknin 238 °C pozwala na produkcję włóknin o dobrych właściwościach mechanicznych.
EN
In this work, preliminary investigations on the influence of the structure of nanofibre based composites on their strength properties were made. As a 'matrix' material, needle punched nonwoven from classical polypropylene fibres was used. Polyamide 6.6 nanofibres electrospun directly onto 'matrix' nonwoven were used as a reinforcement. In order to obtain composites, the nanofibre/'matrix' multilayer structures of different architecture but with the same weight percentage of nanofibres were pressed. On the basis of the investigations realised, it was found that collecting the nanofibres spun in the electrospinning process directly onto the 'matrix' nonwoven is more advantageous than transferring the layer of nanofibres from the collector onto the nonwoven. The tensile test indicates the influence of the composite structure on its strength properties. The composite obtained from the multilayer structure consisted of two thin layers of nanofibres uniformly arranged between the layers of 'matrix' nonwoven, characterized by a higher value of tensile stress and Young's modulus than a composite based on one thicker layer of nanofibres. From the results comes that the use of a higher number of nanofibre layers between the layers of 'matrix' nonwoven gives a more uniform arrangement of nanofibres in the composite space, favouring more the precise wetting of nanofibres by the matrix.
PL
Przedstawiono sposób formowania płaskich wyrobów włókienniczych zawierających warstwę nanowłókien oraz wstępną analizę wpływu struktury ułożenia warstw nanowłókien i włókniny "osnowowej" w pakiecie na właściwości wytrzymałościowe kompozytu termoplastycznego. Materiał osnowowy stanowiła włóknina igłowana ze standardowych włókien PP. Wzmocnienie stanowiły nanowłókna PA 6.6 wytwarzane w procesie elektroprzędzenia bezpośrednio na włókninę osnowową. Warstwy tworzyły pakiety zawierające procentowo taki sam udział wagowy nanowłókien, ale różnie rozmieszczone w przestrzeni pakietu. Na podstawie przeprowadzonych doświadczeń stwierdzono, że odbiór nanowłókien bezpośrednio na włókninę przeznaczoną na osnowę kompozytu jest znacznie korzystniejszy niż przenoszenie warstwy nanowłókien z kolektora na tę włókninę. W wyniku sprasowania pakietów w prasie hydraulicznej otrzymano gotowe kompozyty. Średnie wartości naprężenia maksymalnego i modułu Younga wyraźnie wykazują znaczny wpływ struktury kompozytu na jego właściwości wytrzymałościowe. Kompozyt ze struktury zawierającej dwie cieńsze warstwy nanowłókien równomiernie rozmieszczone pomiędzy warstwami włókniny, wykazuje większe naprężenie zrywające niż kompozyt na bazie jednej grubszej warstwy nanowłókien. Rezultat taki wskazuje, że użycie większej liczby warstw nanowłókien przedzielonych warstwami włókniny, daje bardziej równomierny rozkład nanowłókien w objętości kompozytu, a więc sprzyja dokładniejszemu ich zwilżaniu poprzez osnowę.
EN
The structural changes and mechanical properties of spun-bonded polylactide (PLA) nonwovens resulting from artificial weathering were analyzed in respect to their application in agriculture. The spun-bonded nonwovens were stabilized on a calender at various temperatures ranging from 60 to 110°C. The weathering process was carried out with the use of a Q-SUN weathering chamber under two selected climatic conditions resembling temperate and subtropical climate, respectively. The artificial aging effect on the nonwovens was assessed by measuring their physical parameters and mechanical properties as well as by analyzing their structural changes by means of Fourier infrared spectrophotometry (FTIR), polarization-interference microscopy (PIM) and wide angle X-ray scattering (WAXS).
PL
W pracy zbadano efekty sztucznego starzenia włóknin z polilaktydu (PLA) wytworzonych techniką spun-bonded w aspekcie ich zastosowania w rolnictwie. Włókniny stabilizowano w procesie wytwarzania na kalandrze w temperaturach od 60 °C do 110 °C. Proces sztucznego starzenia przeprowadzono w komorze Q-SUN w warunkach zbliżonych do klimatu umiarkowanego i podzwrotnikowego. Efekty starzenia włóknin badano oceniając zmiany parametrów fizycznych i właściwości mechanicznych w aspekcie zmian ich budowy wykorzystując metody: spektrofotometrii absorpcyjnej w podczerwieni (FTIR), mikroskopii polaryzacyjno-interferencyjnej (MPI) oraz dyfraktometrii rentgenowskiej (WAXS).
first rewind previous Strona / 3 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.