The primary microstructure of new Co-based superalloy of Co-20Ni-7Al-7W (at.%) type was showed in this article. The alloy was manufactured by induction melting in vacuum furnaces. This alloy is a part of new group of high-temperature materials based on Co solid solution and strengthened by coherent L12 phase similar to Ni-based superalloys with γʹ phase. The final form of Coss/L12 microstructure is obtained after fully heat treatment included homogenization, solutionizing and aging processes. But first step of heat treatment thermal parameters determination is characterization of primary microstructure of alloys after casting process with special attentions on segregations of alloying elements in solid solution and presences of structural elements such as eutectic areas, and other phases precipitations. In analysed case the relatively high homogeneity of chemical composition was expected especially in the case of W distribution, what was confirmed be SEM/EDS analysis in dendritic and interdendritic areas.
first rewind previous Strona / 1 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.