EN
Soil erosion by water is an important economical issue strongly deteriorating environment and requiring remedial actions. The study was designed to evaluate antierosion effect of changes in the layout of plots from along to across slope as an effect of land consolidation. Moreover, rightness of leaving newly set out boundaries of plots without any protection (i.e. sodding) was evaluated. For this purpose simulations of use of additional anti-erosive measures were done. The Water Erosion Prediction Project (WEPP) model was used. Studies have shown that in addition to the design of transverse layout of parcels during consolidation, further antierosion measures may be necessary to reduce soil loss and sediment yield. In order to minimize soil losses outside the slope, boundaries between the newly designed fields should be sodded already in the post consolidation management. Limitation the amount of erosion over the entire slope requires use of additional protection measures in the upper part of slopes e.g. shelterbelts and antierosion crop rotations. WEPP model can be recommended for Provincial Bureaus of Surveying as a tool to support the development of assumptions for consolidation projects of lands threatened by erosion.
PL
Erozja wodna gleb jest ważnym zagadnieniem gospodarczym, silnie pogarszającym stan środowiska, wymagającym działań zaradczych. Badania miały na celu ocenę przeciwerozyjnych efektów zmiany układu działek z wzdłużstokowego na poprzecznostokowy w wyniku scalenia gruntów. Oceniono też słuszność pozostawienia nowo wytyczonych granic działek bez zastosowania żadnych środków przeciwerozyjnych (np. zadarnień). W tym celu dokonano dodatkowej symulacji zastosowania różnych środków przeciwerozyjnych z wykorzystaniem modelu WEPP (ang. Water Erosion Prediction Project). Badania wykazały, że poza zaprojektowaniem w trakcie scalenia układu poprzecznostokowego niezbędne mogą być dalsze środki przeciwerozyjne, aby ograniczyć erozję gleby i jej wynoszenie poza obszar stoku. Aby zminimalizować straty gleby poza stok, należałoby już w trakcie zagospodarowania poscaleniowego zadarniać granice między nowo zaprojektowanymi polami. Ograniczenie rozmiarów erozji na całym stoku wymaga stosowania dodatkowych umocnień w górnych partiach zbocza, np. zadrzewień śródpolnych oraz płodozmianów przeciwerozyjnych. Model WEPP może być rekomendowany Wojewódzkim Biurom Geodezji jako narzędzie wspomagające opracowanie projektów scalania gruntów na terenach zagrożonych erozją.
EN
The paper presents a method for predicting the course of phenomenological abrasive erosion of metal alloys, using a simplified probabilistic process model. Based on the assumptions of the model, a formula for quantifying the volume of material loss in time under abrasive loads was proposed. The basis of the method is to establish the dependencies between the parameters appearing in the model: the function ofprobability distribution and distribution coefficient parameters and the strength test parameters of the materials, such as strength tensile strength, yield strength, fatigue parameter (number of cycles to break at a load of204 MPa in a tensile-compressive mode) hardness and work of breaking. Their values were obtained as a result of relevant experimental studies. Knowledge of the functional relationships between the model parameters and measurable parameters allows one to specify the body volume loss of known strength properties under certain load conditions. The values of the parameters appearing in the formula arising from the model were obtained by approximation of the experimental erosion curves designated on the basis of calculations. Materials such as aluminum, PA20, brass M58, Brown BA 1032 after heat treatment, hardened 2H13 steel, as well as lH18N9T and Duplex 2205 steels were used in the tests. The erosion studies were performed with broken SiC grainsas the erodent, with a hardness of 60 HRC and a diameter of 0.7 mm and the average kinetic energy was 16.4 J. The usefulness of the method was verified by determining the theoretical erosion curves for each material model parameter set depending on a the set. The result of the comparison of the experimental curves were in good agreement for PA20, MO58 and 2Hl3, while significant differences were observed in the case of brown and 1Hl8N9T. The reason for the discrepancies are errors resulting from the too small number of erosion samples, which has an infiuence on deterrnined relationships.
PL
W pracy przedstawiono fenomenologiczną metodę przewidywania przebiegu erozji abrazyjnej stopów metali, wykorzystującą uproszczony, probabilistyczny model procesu. Na podstawie założeń modelowych zaproponowano formułę kwantyfikującą ubytki objętości materiału w funkcji czasu w warunkach obciążeń abrazyjnych. Podstawą metody jest ustalenie zależności między parametrami występującymi w zapisie modelowym: parametrami funkcji rozkładów prawdopodobieństwa i współczynnikami podziału a parametrami wytrzymałościowymi testowanych materiałów, takimi jak: wytrzymałość na rozciąganie, granica plastyczności, parametr zmęczeniowy (liczba cykli do zerwania przy obciążeniu 204 MPa w trybie rozciągająco-ściskającym), twardość oraz praca zerwania. Ich wartości uzyskano w wyniku wykonania odpowiednich badań eksperymentalnych. Znajomość funkcjonalnych zależności pomiędzy parametrami modelowymi a parametrami mierzalnymi pozwala na określenie ubytków objętości ciała o znanych właściwościach wytrzymałościowych w określonych warunkach obciążeń. Wartości parametrów występujących w formule wynikającej z modelu uzyskano przez aproksymację doświadczalnych krzywych erozyjnych krzywymi wyznaczonymi na podstawie obliczeń. Do badań wykorzystano takie materiały, jak aluminium PA20, mosiądz M58, brąz BA1032 po obróbce cieplnej, stal 2Hl3 w stanie zahartowanym, a ponadto stale lH18N9T oraz Duplex 2205. Badania erozyjne wykonano na stanowisku, w którym erodentem były łamane ziarna SiC o twardości 60 HRC i średnicy 0,7 mm, a ich średnia energia kinetyczna wynosiła 16,4 J. Przydatność metody zweryfikowano przez wyznaczenie teoretycznych krzywych erozji poszczególnych materiałów dla parametrów modelowych określonych za pomocą wyznaczonych zależności. W wyniku porównania z krzywymi doświadczalnymi stwierdzono dobrą zgodność dla PA20, MO58 i 2H13, natomiast znaczące rozbieżności zaobserwowano w przypadku brązów i stali 1H18N9T. Przyczyną rozbieżności są błędy wynikające ze zbyt małej liczby prób erozyjnych, co ma decydujący wpływ na postać wyznaczonych zależności funkcyjnych (tab. 2).
EN
The work included the production of an actual water erosion risk map for the area of Bystra watershed, basing on vector layers: potential water erosion risk and CORINE Land Cover 2000 as a source of land use information. The results show relative high share of actual erosion in avegare to highest intensities - 32.5% of Bystra catchment. Compared to potential water erosion, where the same grades cover 41.0% of watershed’s area, the erosion risk at high grades decreased only by 8.5%. Actally, according to the land use structure derived from CLC2000, around 9694 hectares undergo high water erosion intensity grades and needs erosion control measures.