Content available remote Extrusion control of ceramic microstructure
EN
The objective of work is to indicate the possibilities of controlling the microstructure in porcelain body during extrusion process in relation to the resulting mechanical properties of the final material. The method of mathematical modeling the flow of composite mixture through an extruder die was used to express the effect of forming parameters on the arising body microstructure. The orientation of the anisotropic particles can be influenced by the character of velocity field during the flow of mixture through the circular extruder die. The various orientation of the particles and their combinations enable control over directional mechanical strength of the ceramic.
PL
Przedmiotem pracy jest ocena możliwości kontroli mikrostruktury i własności mechanicznych masy ceramicznej w procesie wytłaczania. Orientacja anizotropowych cząstek, mająca decydujący wpływ na własności mechaniczne masy ceramicznej, determinowana jest polem prędkości w dyszy wylotowej wytłaczarki. Zastosowano metodę modelowania przepływu przez dyszę wytłaczarki do określania parametrów masy ceramicznej.