Fabrication of a ceramic-polymer hybrid structure with microchannel was accomplished. The structure for capillary electrophoresis is presented as an example system. The method of fabrication of such a structure is not complicated, makes use of well known technologies like thick film and photolithography, and commercially available materials. It could be used for manufacture of structures with different shapes and dimensions. The process relies on printing dielectric photosensitive paste onto a ceramic support, drying and exposing to UV light through a mask with suitable pattern, developing and firing. A thin glaze layer is deposited on the top of the structure in order to make possible reversible or irreversible bonding with transparent poly(dimethylsiloxane) (PDMS) and adapting this chip to measurements with the use of optical detection.
PL
Opracowano wytwarzanie ceramiczno-polimerowych struktur zawierających mikrokanał. Jako przykład zaprezentowano strukturę do elektroforezy kapilarnej. Metoda wytwarzania takich mikroukładów jest metodą prostą, wykorzystującą dobrze znane technologie, takie jak technologia grubowarstwowa czy fotolitografia i materiały komercyjnie dostępne. Może być wykorzystywana do wytwarzania struktur hybrydowych o różnej geometrii kanałów. Proces wytwarzania mikroukładów polega na nadrukowaniu światłoczułej pasty dielektrycznej na podłoże ceramiczne, wysuszeniu i naświetleniu przez fotomaskę z odpowiednim wzorem, wymyciu nienaświetlonej części warstwy i wypaleniu. Pokrycie struktury cienką warstwą szkliwiącą daje możliwość odwracalnego lub trwałego łączenia z transparentnym poli(dimetylosiloksanem) (POMS) i dostosowania takiego układu do pomiarów z detekcją optyczną.
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.