Based on the available literature data and our long-term experience, this paper characterises the microstructure of two-phase TiAl based alloys, its influence on properties of the alloys, and possibilities of forming it in manufacturing processes. It presents a new original way of forming the microstructure that is regarded as the optimum for this group of alloys, without plastic deformation, by only using multi-stage heat treatment consisting of the following consecutive operations: homogenising, cyclic heat treatment, under-annealing, and short-term full annealing.
PL
W pracy w oparciu o dane literaturowe i wieloletnie doświadczenia własne scharakteryzowano mikrostrukturę dwufazowych stopów na osnowie fazy międzymetalicznej TiAl, wpływ mikrostruktury na właściwości stopów (rys. 2-5) i możliwości jej kształtowania w procesach technologicznych (rys. 6-9). Zaprezentowano nowy autorski sposób kształtowania uważanej za optymalną dla tej grupy stopów mikrostruktury, bez udziału odkształcenia plastycznego, wyłącznie zabiegami wieloetapowej obróbki cieplnej, składającej się z kolejno następujących po sobie zabiegów: wyżarzania ujednorodniającego, cyklicznej obróbki cieplnej, wyżarzania niezupełnego oraz krótkotrwałego wyżarzania zupełnego (rys. 10).