Preferencje help
Widoczny [Schowaj] Abstrakt
Liczba wyników

Znaleziono wyników: 6

Liczba wyników na stronie
first rewind previous Strona / 1 next fast forward last
Wyniki wyszukiwania
Wyszukiwano:
w słowach kluczowych:  mikronaprężenia
help Sortuj według:

help Ogranicz wyniki do:
first rewind previous Strona / 1 next fast forward last
EN
The substructure anisotropy of real textured metal materials was studied by use of the X-ray method of Generalized Pole Figures. Substructure states of rolled material along different directions form an extremely wide spectrum. Three laws of substructure anisotropy were revealed for the first time. The 1st law describes the distribution of residual deformation effects in textured materials, the 2nd law concerns variation of lattice parameters in metal products due to elastic microstrains and the 3d law considers non-uniformity of the lattice condition in connection with sign of residual microstrains.
PL
Anizotropia substruktury w metalach posiadających teksturę krystalograficzną była badana za pomocą rentgenowskiej metody uogólnionych figur biegunowych. Stany substruktury walcowanego materiału wzdłuż rożnych kierunków stanowią bardzo szerokie spektrum. Po raz pierwszy zostały przedstawione trzy prawa anizotropii substrukturalnej. Pierwsze prawo opisuje szczątkowe efekty odkształcenia w teksturowanych materiałach w zależności od orientacji ziaren. Drugie prawo dotyczy zmienności parametrów sieci krystalicznej w wyrobach metalowych w wyniku elastycznych mikronaprężeń. Trzecie prawo dotyczy niejednorodności stanu sieci krystalicznej w związku ze znakiem mikronaprężeń szczątkowych.
PL
W pracy oceniono wpływ mikronaprężeń na pękanie elementów oprzyrządowania technologicznego eksploatowanych w piecach do nawęglania. Doświadczalnie oceniono możliwość wystąpienia przemiany fazowej w warunkach oddziaływania podwyższonej i zmiennej temperatury w staliwie austenitycznym typu Fe-Ni-Cr-C. Numerycznie, metodą elementów skończonych, wyznaczono naprężenia strukturalne σx, σy, σz, powstające wskutek różnic, głównie w wartościach współczynników rozszerzalności cieplnej węglików i austenitu, w modelu węglika częściowo osłoniętego austenityczną osnową, podczas jego gwałtownego chłodzenia. Dla przyjętego modelu węglika, stosując hipotezę niezmienników Burzyńskiego określono obszar, w którym węglik ulegnie uszkodzeniu. Wykazano, że naprężenia strukturalne wynikające z różnic we właściwościach fizycznych faz są bezpośrednią przyczyną pękania badanych elementów.
EN
In the study, the effect of microstresses on the cracking of techno-logical instrumentation elements used in carburising furnaces was evaluated. A possibility of the appearance of phase transition in austenitic cast steel of the Fe-Ni-Cr-C type under raised and variable temperature effect conditions was evaluated experimentally. Structural stresses – σx, σy and σz, - developing due to differences, for the most part, in carbide and austenite thermal expansion coefficient values were determined numerically with the finite element method in the carbide model partially surrounded by the austenitic matrix during its rapid cooling. For the adopted carbide model, the area where the carbide will be damaged was determined using the Burzyński’s hypothesis of invariants. It was shown that microstresses resulting from differences in the physical properties of phases are a direct cause of cracking of the examined elements.
EN
This work presents the analysis the effort of phases which are present in the austenitic cast steel Fe-Ni-Cr-C, applied for elements of technological instrumentation for carburising furnaces. The reduced stresses [sigma]_red in the carbides and the austenitic matrix were determined in accordance with the assumed hypotheses of effort, on the basis of the structural stresses [sigma]_x [...] calculated by the finite element method for two model location cases of the carbides towards the cast steel surface. The hypotheses referred to the crack condition were applied to evaluate the elastic carbide efforts, while for the elastic-plastic austenitic matrix - the hypotheses referred to the plasticity condition were used. There were compared the reduced stresses óred determined in accordance with various hypotheses and the correctness of their applying. It was demonstrated on the basis of the executed analysis of the effort that the carbides are destroyed only when they are not entirely surrounded by the austenitic matrix.
EN
In the present paper, three approaches (point grids in mechanics, the electrochemical microcell technique in electrochemistry and Auger electron spectroscopy in surface analysis) were conducted on the same duplex stainless steel microstructure to propose mechanical-electrochemical criteria leading to significant changes in the chemical composition of oxide films and enhancement of pitting susceptibility of multiphase alloys.
PL
W niniejszej pracy zaprezentowano trzy komplementarne podejścia dla opisu fizykochemicznych parametrów lokalnych fragmentów powierzchni stali nierdzewnej typu duplex, a mianowicie: metodę "sieciowania punktowego" (mikroanaliza mechaniczna), technikę "mikroceli galwanicznej" (ocena elektrochemiczna) i spektroskopii elektronów Augera (lokalna analiza chemiczna). Techniki te stosowano na tych samych fragmentach mikrostrukturalnych stali, co pozwoliło na sformułowanie mechano- elektrochemicznych uwarunkowań skutkujących znacznymi zmianami w składzie chemicznym pasywnych warstw tlenkowych a także wzrostem skłonności do tworzenia wżerów przez stopy wielofazowe.
EN
The energy storage process is characterised by the energy storage rate de(s)/dw(p) as a function of plastic strain epsilon^p (e(s) is stored energy, w(p) is plastic work). At the initial stage of plastic deformation the dependence of de(s)/dw(p) on epsilon^p has a maximum. The present work is devoted to the experimental verification of a hypothesis that the maximum of de(s)/dw(p) can be related to the internal micro-stresses caused by incompatible slip in grains of different orientation. Experiments that make it possible to estimate the influence of internal micro-stresses on the rate of energy storage are presented. The obtained results confirm the hypothesis.
PL
Proces magazynowania energii można opisać zależnością wielkości de(s)/dw(p), zwanej zdolnością magazynowania energii, od odkształcenia plastycznego epsilon^p (e(s) - energia zmagazynowana, w(p) praca odkształcenia plastycznego). W początkowym stadium odkształcenia plastycznego zależność ta ma maksimum. Niniejsza praca jest poświęcona eksperymentalnej weryfikacji hipotezy, według której występowanie maksimum de(s)/dw(p) może być skutkiem mikronaprężeń wewnętrznych powstałych w wyniku niekompatybilnego poślizgu w ziarnach o różnej orientacji. Przedstawiono eksperymenty, które pozwalają pokazać wpływ mikronaprężeń na zdolność magazynowania energii. Uzyskane wyniki potwierdzają postawioną hipotezę.
PL
W pracy zaproponowano kontynualne, termodynamiczne podejście do opisu fizyko-mechanicznych zjawisk oddziaływania agresywnych czynników środowiska zewnętrznego w warstwach powierzchniowych materiału porowatego (betonu) oraz zachodzących procesów dyfuzji i reakcji chemicznych. Beton rozpatruje się jako nasycony roztworem wodnym materiał porowaty. Przy opisie procesów w fazach wykorzystuje się koncepcje termodynamiki procesów nierównowagowych (teorii roztworów wieloskładnikowych), a dla otrzymania równań dla ciała w całości - metody uśrednienia przestrzennego teorii ośrodków wielofazowych.
EN
The thermodynamical approach has been proposed for description of physical and mechanical processes in subsurface layers of concrete through acting aggressive factors of the surroundings accompanying their diffusion and corresponding chemical reactions. Concrete is considered as two-phase porous material saturated by water solution. For the description of the phases the concept of thermodynamics of nonequilibrium processes (the theory of multicomponent solutions) is used, and methods of space averaging of the theory of multiphase media are applied for a description of whole body.
first rewind previous Strona / 1 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.