EN
The casting workshop in Grzybiany, in Lower Silesia (SW Poland) is a valuable source of knowledge on the development of casting techniques in the 7 – 6 centuries BC. Abundant evidence found on the archaeological site points to cast manufacturing by means of precision casting in ceramic moulds (lost-wax molding). The workshop is the biggest collection of moulds for bracelet, necklace and other smaller decorative artefacts in Poland. The aim of the work is to conduct the research of the moulds and casts with the view of performing a computer reconstruction of the casting moulds from the Bronze and Early Iron Age, based on the Grzybiany finds. As part of the work, both the microscopic structure and defectoscopic analyses of the casting moulds were performed. Chemical composition of the casts was tested using the X-ray fluorescence spectroscopy method. Based on these results and using computer modelling methods, a geometric visualisation was performed, which is the bases for preparing the visualisation of the process of pouring liquid metal into the moulds, reconstructing both the technology and the alloys used.
EN
This work presents the research result of the temperature distribution and the microstructure in certain parts of the field-glass body frame casting made from silumin AlSi9 using the investment casting method in the ceramic mould. It was proved that the highest temperature of the silumin appears in the sprue in which the silumin is in the liquid-solid state, though the process of silumin crystallization in the casting is finished. It was stated that in certain elements of the casting the side opposite to the runner crystallizes and cools fastest. The differences in the rate of crystalline growth and cooling of certain casting elements cause different microstructure in them which can also influence the mechanic properties. It is necessary to state that the temperature of the initial heating of the ceramic mold equal to 60ºC guarantees obtaining of the castings without defects and of little porosity. Incomplete modification of the silumin with strontium causes silica precipitation to appear close to the spherical ones.
first rewind previous Strona / 1 next fast forward last
JavaScript jest wyłączony w Twojej przeglądarce internetowej. Włącz go, a następnie odśwież stronę, aby móc w pełni z niej korzystać.