Preferencje help
Widoczny [Schowaj] Abstrakt
Liczba wyników
Powiadomienia systemowe
  • Sesja wygasła!

Znaleziono wyników: 4

Liczba wyników na stronie
first rewind previous Strona / 1 next fast forward last
Wyniki wyszukiwania
Wyszukiwano:
w słowach kluczowych:  lead content
help Sortuj według:

help Ogranicz wyniki do:
first rewind previous Strona / 1 next fast forward last
EN
Heavy metals are some of the environmental pollutants that have a serious impact on the environment. The analysis of hydromacrophytes growing in small rivers of the south of Kazakhstan with different contents of heavy metal salts revealed that the morphometric indicators of the same plant species differ significantly, depending on the level of total mineralization of the aquatic environment in different rivers of the Turkestan region. It has been established that two plant species can be used to bioindicate the content of lead ions in the aquatic environment: Azolla caroliniana Willd. and Veronica beccabunga L., which must be introduced into the tested aqueous solutions in the amount of 1.0 kg/m3 and 1.5–2.0 kg/m3, respectively, to fully cover the water column at different depths. The first morphological changes in plants, in the form of destruction of the structure of chloroplasts along the edges of unfolded leaves in A. caroliniana Willd. and slight withering of the lower underwater leaves in V. beccabunga L., occur already at a 1.5 mg/l Pb2+ content in water, and a further increase in the content of lead ions in water to 600.0–800.0 mg/l leads to the death of plants.
PL
W artykule podano wyniki doświadczeń laboratoryjnych ługowania ołowiu z koncentratu miedziowego za pomocą octanu amonu. Przebadano wpływ dodatku nadtlenku wodoru do roztworu ługującego na stopień ługowania ołowiu z koncentratu. Proces prowadzono przez 60 minut w temperaturze 293 K, stosując roztwory octanu amonowego o stężeniu 10% i 40% wagowych.
EN
This article presents results of laboratory experiments of leaching lead from copper concentrate with ammonium acetate. The effect of addition of hydrogen peroxide to the leaching solution on the rate of lead leaching from copper concentrate was studied. The process was carried out for 60 minutes at 293 K, in 10 and 40 percent (by weight) ammonium acetate solutions.
PL
W procesie flotacji ołów towarzyszący rudom miedzi przechodzi do koncentratów miedziowych. Jego obecność jest przyczyną trudności w dalszej przeróbce metalurgicznej. Badania prowadzone przez różne ośrodki naukowe w kraju zmierzają do opracowania sposobu obniżenia zawartości ołowiu we wspomnianych produktach. W prezentowanej pracy przedstawiono wyniki badań wykonanych na koncentracie miedzi z ZWR RUDNA. Próbka zawierała średnio ok. 30 % miedzi i 1,5 % ołowiu i charakteryzowała się bardzo drobnym uziarnieniem. Klasy poniżej 45 mikrometrów było ok. 62 %. Celem badań była ocena możliwości obniżenia zawartości ołowiu w koncentracie miedzi dwoma sposobami: na drodze obróbki chemicznej koncentratu za pomocą roztworu octanu amonu, poprzez wstępną obróbkę materiału za pomocą rozcieńczonego kwasu nieorganicznego lub gorącą wodą, a następnie flotacji. Stwierdzono, że w wyniku ługowania chemicznego octanem amonu można obniżyć zawartość ołowiu w koncentracie miedziowym z 1,5 % Pb do ok. 0,2 %. Równocześnie odbywa się ługowanie miedzi, której straty w koncentracie są dość duże. Wykazano, że najkorzystniejsze warunki otrzymuje się podczas ługowania surowej próbki z płukaniem placka filtracyjnego. Osiąga się wówczas obniżenie zawartości ołowiu do 0,6 %, przy minimalnej stracie miedzi, wynoszącej tylko 3,5 % Cu w roztworze w stosunku do próbki wyjściowej. W wyniku wstępnej obróbki powierzchniowej koncentratu za pomocą kwasu azotowego lub gorącej wody a następnie flotacji, otrzymano dwa produkty o zróżnicowanych zawartościach miedzi i ołowiu. Jeden o zawartości miedzi ok. 25 do 36 % i zawartości ołowiu ok. 1,7 %, przy wychodzie od 75 do 90 %. Drugi o obniżonej zawartości ołowiu od 0,8 do 1 % i zawartości miedzi ok. 13 do 16 %, przy wychodzie wahającym się od 25 do 10 %.
EN
Lead, accompanying copper ores, passes to copper concentrate during flotation of the ores. Its presence makes further metallurgical processing difficult. Research, done in various scientific centres in Poland, is aimed at developing a method to lower the content of lead in these products. This paper presents the results of research on a copper concentrate from the Rudna Processing Plant. The sample contained on average 30 % copper and 1.5 % lead and was very fine grained. As much as 62 % was in the - 45 micrometers grain class. The study aimed to assess the possibility of lowering lead content in copper concentrate by two methods: chemical treatment of the concentrate with an ammonium acetate solution, pre-treatment of the feed with diluted inorganic acid, or with hot water, followed by flotation. It was found that lead content in the concentrate could be reduced from 1.5 % to about 0.2 % by leaching with ammonium acetate. Copper was leached at the same time, which impoverished the concentrate. The best results were achieved by leaching the raw sample and washing the filter cake. By doing so, the lead content could be lowered to 0.6 % with minimum loss of copper - only 3.5 % in solution, regarding the initial sample. Surface pre-treatment of the concentrate with nitric acid or hot water, followed by flotation, resulted in two products with different copper and lead content. One of them contained 25-36 % copper and about 1.7 % lead, at yields ranging from 75 to 90 %. The other, with a lead content lowered to 0.8-1 %, contained 13-16 % copper, at yields ranging from 25-10%.
4
Content available remote A flotational-chemical method of reducing lead content in copper concentrate
EN
This paper presents the results of laboratory studies performed on copper concentrate sample containing about 30 percent Cu and about 1.55 percent Pb. The objective of the study was to demonstrate that by combining chemical treatment and flotation one can obtain a concentrate with reduced lead content. As a result of pre-treatment of the sample with a 10% (by weight) ammonium acetate solution and subsequent flotation in the presence of a collector added at a ratio of 10 g/Mg, the material can be separated into two products: - one obtained at a yield of37%, containing about 44% copper and about 0.9% lead - and one containing about 19% Cu and up to 1.6% Pb. Thus obtained products can be directed to different copper-recovery metallurgical processes.
PL
Artykuł przedstawia wyniki badań laboratoryjnych wykonane dla próbki koncentratu miedzi zawierającego około 30% Cu i około 1,55% Pb. Celem badań było wykazanie, że połączone metody obróbki chemicznej i flotacji mogą dać w wyniku produkt o obniżonej zawartości ołowiu w koncentracie. Wstępna obróbka chemiczna badanej próbki za pomocą octanu amonu o stężeniu 10% wag., a następnie flotacja w obecności zbieracza o stężeniu 10 g/Mg pozwala rozdzielić materiał na dwa produkty: - jeden o wychodzie około 37% i zawartości miedzi około 44%, a ołowiu około 0,9%; - drugi zawierający około 19% miedzi i około 1,6% ołowiu. Każdy z tak otrzymanych produktów może być kierowany do otrzymywania miedzi różnymi metodami metalurgicznymi.