Among sound insulating materials used in the automotive industry, multilayer systems consisting of foams, nonwovens, mats, knitted fabrics or porous panels in different combinations are very popular. These materials can be replaced by fibre reinforced composites. These composites can be good sound absorbing materials even at low thickness. One way to increase sound absorption is to form a composite with an optimal structure and surface topography. In this work, the investigations concern the sound absorption by thermoplastic composites with surface asymmetry. The influence of surface asymmetry of thermoplastic composites on their sound absorption coefficient was studied. The first kind of asymmetry concerns the structure of the composite surface, i.e. plastic and fibrous structure. The second kind of asymmetry concerns the topography of the composite surface, i.e. the one side of the composite surface is smooth and on the opposite side it is characterized by some relief. The sound absorption coefficient was measured for different sample orientations to the sound wave to assess the significance of the surface asymmetry and to indicate a more favourable composite side from the sound absorption point of view. Generally, both the surface structure asymmetry and surface topography asymmetry influence the sound wave behaviour and consequently increase the compositesound absorption.
PL
Spośród materiałów tłumiących dźwięk stosowanych w przemyśle samochodowym bardzo popularne są układy warstwowe składające się z pianek, włóknin, mat, dzianin lub porowatych paneli w różnych kombinacjach. Materiały takie mogą być zastąpione przez kompozyty wzmacniane włóknami, które mogą wykazywać dużą absorpcję dźwięku nawet przy małej ich grubości. Jednym ze sposobów zwiększenia absorpcji dźwięku jest zapewnienie optymalnej struktury i topografii kompozytu. W pracy przedstawiono badania dotyczące absorpcji dźwięku przez kompozyty charakteryzujące się asymetrią powierzchniową. Badano wpływ asymetrii powierzchniowej kompozytu na współczynnik absorpcji dźwięku. Pierwszy rodzaj asymetrii dotyczył struktury powierzchni kompozytu, tj. struktury włóknistej oznaczonej jako „fibrous”, i struktury bardziej sprasowanej, oznaczonej jako „plastic”. Drugi rodzaj asymetrii dotyczył topografii powierzchni kompozytu, tj. jedna strona kompozytu była gładka, druga posiadała specjalnie nadany relief. Współczynnik absorpcji dźwięku był wyznaczany dla różnego ukierunkowania próbki kompozytu w stosunku do padającej fali dźwiękowej, tak by można było ocenić znaczenie asymetrii powierzchniowej i wskazać bardziej korzystną stronę kompozytu z punktu widzenia możliwości tłumienia dźwięku. Generalnie, zarówno asymetria struktury, jak i topografii powierzchni kompozytu wpływa na zachowanie się tłumionej fali dźwiękowej, a w konsekwencji na wzrost absorpcji dźwięku przez kompozyt.
PL
W artykule przedstawiono technologię produkcji kompozytów termo-elastoplastycznych poprzez jednoczesną dewulkanizację odpadów gumowych i ich reaktywne mieszanie z polimerem termoplastycznym za pomocą współbieżnej wytłaczarki dwuślimakowej zaprojektowanej i wykonanej w Instytucie IMPIB. Na podstawie przeprowadzonych prób dokonano optymalizacji parametrów procesu. Otrzymano kompozyty termoplastyczne dewulkanizatu EPDM/PP o szerokim spektrum twardości, niewymagające wulkanizacji, kształtowane w procesie wytłaczania metodami stosowanymi w przetwórstwie tworzyw sztucznych. Kompozyty mogą być poddawane granulacji i powtórnie przetwarzane. Materiał może być stosowany do produkcji detali dla przemysłu motoryzacyjnego, nawierzchni sportowych, elementów antywibracyjnych, konfekcji drogowej, rur i węży nawadniających.
EN
The present paper is related to technology of production of thermo-elastic composites through simultaneously devulcanization of rubber wastes and their reactive mixing with thermoplastic polymer in co-rotating twin-screw extruder. The prototype of machinery was designed and made at Institute for Engineering of Polymer Materials & Dyes. On the basis of conducted tries the process was optimized. Thermoplastic composites of EPDM devulcanizate with PP were obtained in a wide spectra of hardness. These composites do not require vulcanization and can be processed with methods commonly used for plastics. The composites can be regranulated and reused. Such materials can be exploited in production of automotive parts, sport surfaces, antivibration systems, road confection, pipes or tubes.
EN
The objective of this paper is to discuss effect of commingling parameter on characteristics of Glass/Polypropylene commingled hybrid yarns to get homogenous mix of matrix and reinforcement elements in the final yarn. A commingling machine developed to produce hybrid yarn using two techniques viz. mingling technique and hollow spindle wrapping technique using single machine is highlighted .The machine can run at speed upto 800 meters/min and for hybrid yarn it can go up to 200 meters/min. To study the effect of parameter three variable namely Air pressure, Overfeed and Take-up speed are take in to consideration and the Box-Behanken design is used for experimental setup. The hybrid yarn samples have been evaluated to investigate the influence of process variables the commingling characteristics of hybrid yarn viz. nip frequency; nip stability and nip regularity have also been studied. 'MINITAB' software is used for the analysis of test results. It was observed that effects of individual parameter as well as interaction effects are equally important in deciding final yarn quality. The structural analysis of hybrid yarn is done using SEM (Scanning electron microscope). To study the mixing behaviour of glass/polypropylene hybrid yarn three different methods have been used to prepare hybrid yarn viz. Friction spinning, hollow spindle wrapping, commingling. Its was clearly observed that commingled process gives better homogenous mixing of glass and polypropylene filaments compare to other two method. This yarn is used to make final laminate sample using hot press.
PL
Problem recyklingu odpadów tekstylnych stał się w ostatnich latach jednym z najczęściej podejmowanych tematów badań w czołowych zagranicznych ośrodkach naukowych, pracujących na rzecz włókiennictwa. Podjęte przez te placówki prace obejmują zagadnienia organizacyjne (logistyka zbiórki odpadów tekstylnych), recykling materiałowy z ukierunkowaniem na różne produkty utylizacji (np. kompozyty i laminaty).
PL
Jedną z najbardziej rozpowszechnionych światowych tendencji w dziedzinie otrzymywania kompozytów z tworzyw sztucznych jest napełnianie ich polimerami naturalnymi, co pozwala na uzyskiwanie kompozytów o zmienionych właściwościach i równocześnie biorozpadalnych. Szczególnie chodzi o wykorzystanie uciążliwych dla środowiska naturalnego odpadów, z równoczesnym ograniczeniem ilości używanych tworzyw termoplastycznych. W chwili obecnej do najczęściej stosowanych jako napełniacze polimerów naturalnych należą celuloza i skrobia. Badania prowadzone w Instytucie Chemii Przemysłowej wykazują, że jako napełniacz w kompozytach polimerowych można także stosować odpady z garbowania skóry.
EN
In this study, an elastic-plastic stress analysis is carried out on symmetric steel fiber reinforced high density polyethylene thermoplastic matrix laminated beams under a bending moment. The Bernoulli-Euler theory is used. The orientation angles are chosen as (90o/0o)2, (30o/-30o)2, (45o/-45o)2 and (60o/-60o)2. The composite material is assumed to be linearly hardening. The stress component 'sigma'x is to be maximum at the upper and lower surfaces in the elastic-plastic solution. The residual stress component 'sigma'x is found to be highest at the upper and lower surfaces. However, when the plastic region is further expanded the residual stress component 'sigma'x is found to be the highest at the elastic and plastic boundaries. The plastic flow is to be maximum at the upper and lower surfaces for the (30o/-30o)2 orientation. The transverse displacement is obtained to be highest at the free end for the (90o/0o)2 orientation.